# US 2025/0062123 A1 · Treatments for thin films used in photolithography

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0062123 A1
- Document ID: US20250062123A1
- Status: Published application
- Kind: A1
- Application number: 18/235,249
- Filed: 2023-08-17
- Published: 2025-02-20
- Earliest claimed: 2023-08-17
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: SHASHANK SHARMA; KAI B. NG; NORMAN TAM; YUQI GUO; ANDY LO; HUIXIONG DAI; KHOI PHAN; CHIHAN HSU; MADHUR SACHAN; NASRIN KAZEM; ZHENXING HAN
- Web page: https://patentgrep.com/patent/US20250062123A1

## CPC

- H10P 76/2041: {Photolithographic processes}
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10P 50/696: {Process specially adapted to improve the resolution of the mask}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/204: {of organic photoresist masks}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments disclosed herein include a method of thermal treatment or radical species treatment of a photoresist a metal-oxide photoresist. In an embodiment, a method of patterning a metal-oxide photoresist, such as a Sn-based photoresist, includes depositing the metal-oxide photoresist over a substrate, exposing the metal-oxide photoresist with an extreme ultra-violet (EUV) exposure to form exposed regions and non-exposed regions, developing the exposed metal-oxide photoresist, and performing a thermal treatment and/or a radical species treatment of the metal-oxide photoresist.

## Claims

### Claim 1

A method of patterning a metal-oxide photoresist, comprising:
depositing the metal-oxide photoresist over a substrate;
exposing the metal-oxide photoresist with an extreme ultra-violet (EUV) exposure to form exposed regions and non-exposed regions;
developing the exposed metal-oxide photoresist; and
performing a thermal treatment of the metal-oxide photoresist.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermal treatment of the metal-oxide photoresist is performed following the depositing but prior to the exposing of the metal-oxide photoresist.

### Claim 3 (depends on 1)

The method of claim 1, wherein the thermal treatment of the metal-oxide photoresist is performed following the exposing but prior to the developing of the metal-oxide photoresist.

### Claim 4 (depends on 1)

The method of claim 1, wherein the thermal treatment of the metal-oxide photoresist is performed following the developing of the metal-oxide photoresist.

### Claim 5 (depends on 1)

The method of claim 1, wherein the thermal treatment is performed at temperature in the range of 60-400 degrees Celsius, at a pressure of 1 Torr to 760 Torr, for a duration in the range of 10 seconds to 10 minutes, and using one or a mixture of gases selected from the group consisting of N2, H2, O2, NH3, Ar and He.

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal-oxide photoresist is a positive tone photoresist.

### Claim 7 (depends on 1)

The method of claim 1, wherein the metal-oxide photoresist is a negative tone photoresist.

### Claim 8

A method of patterning a metal-oxide photoresist, comprising:
depositing the metal-oxide photoresist over a substrate;
exposing the metal-oxide photoresist with an extreme ultra-violet (EUV) exposure to form exposed regions and non-exposed regions;
developing the exposed metal-oxide photoresist; and
performing a radical species treatment of the metal-oxide photoresist.

### Claim 9 (depends on 8)

The method of claim 8, wherein the radical species treatment of the metal-oxide photoresist is performed following the depositing but prior to the exposing of the metal-oxide photoresist.

### Claim 10 (depends on 8)

The method of claim 8, wherein the radical species treatment of the metal-oxide photoresist is performed following the exposing but prior to the developing of the metal-oxide photoresist.

### Claim 11 (depends on 8)

The method of claim 8, wherein the radical species treatment of the metal-oxide photoresist is performed following the developing of the metal-oxide photoresist.

### Claim 12 (depends on 8)

The method of claim 8, wherein the radical species treatment is performed at temperature in the range of 60-400 degrees Celsius, at a pressure of 50 mTorr to 20 Torr, for a duration in the range of 10 seconds to 10 minutes, and using one or a mixture of gases selected from the group consisting of N2, H2, O2, NH3, Ar and He.

### Claim 13 (depends on 8)

The method of claim 8, wherein the radical species treatment is performed using an inductively coupled plasma (ICP) source, a remote plasma source, or a microwave plasma source.

### Claim 14 (depends on 8)

The method of claim 8, wherein the metal-oxide photoresist is a positive tone photoresist.

### Claim 15 (depends on 8)

The method of claim 8, wherein the metal-oxide photoresist is a negative tone photoresist.

### Claim 16

A method of patterning a metal-oxide photoresist, comprising:
depositing the metal-oxide photoresist over a substrate;
exposing the metal-oxide photoresist with an extreme ultra-violet (EUV) exposure to form exposed regions and non-exposed regions;
developing the exposed metal-oxide photoresist;
performing a thermal treatment of the metal-oxide photoresist; and
performing a radical species treatment of the metal-oxide photoresist.

### Claim 17 (depends on 16)

The method of claim 16, wherein the thermal treatment is performed prior to the radical species treatment.

### Claim 18 (depends on 16)

The method of claim 16, wherein the radical species treatment is performed prior to the thermal treatment.

### Claim 19 (depends on 16)

The method of claim 16, wherein the thermal treatment is performed at temperature in the range of 60-400 degrees Celsius, at a pressure of 1 Torr to 760 Torr, and for a duration in the range of 10 seconds to 60 minutes.

### Claim 20 (depends on 16)

The method of claim 16, wherein the radical species treatment is performed at temperature in the range of 60-400 degrees Celsius, at a pressure of 50 mTorr to 20 Torr, and for a duration in the range of 10 seconds to 10 minutes, and wherein the radical species treatment is performed using an inductively coupled plasma (ICP) source, a remote plasma source, or a microwave plasma source.