# US 2025/0059663 A1 · Method of aluminum-scandium alloy production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0059663 A1
- Document ID: US20250059663A1
- Status: Published application
- Kind: A1
- Application number: 18/623,827
- Filed: 2024-04-01
- Published: 2025-02-20
- Earliest claimed: 2018-03-15
- Assignees: Fea Materials LLC
- Applicants: Fea Materials LLC
- Inventors: Adam Clayton POWELL; Matthew R. EARLAM; Salvador A. BARRIGA; Richard SALVUCCI; Brian HUNT
- Web page: https://patentgrep.com/patent/US20250059663A1

## CPC

- C25C 3/36: Alloys obtained by cathodic reduction of all their ions
- C22C 21/00: Alloys based on aluminium
- C25C 7/02: Electrodes (consumable anodes for the refining the metals C25C1/00 - C25C5/00); Connections thereof
- C25C 7/06: Operating or servicing
- Y02P 10/25: Process efficiency
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed methods relate to producing an aluminum-scandium (Al—Sc) alloy. A method can include providing an electrolyte bath comprising a first portion of at least one of ScF3 or AlF3 and a first portion of at least one of LiF, NaF, or KF; providing a cathode in electrical contact with the electrolyte bath; providing an anode in electrical contact with the electrolyte bath; adding a first portion of Sc2O3 into the electrolyte bath; reacting an aluminum ion with the cathode; applying an electric current to the cathode, thereby reacting a scandium ion with the cathode to produce the Al—Sc alloy.

## Claims

### Claim 1

A method of producing an aluminum-scandium (Al—Sc) alloy, comprising:
(a) providing an electrolyte bath comprising a first portion of at least one of ScF3 or AlF3 and a first portion of at least one of LiF, NaF, or KF;
(b) providing a cathode in electrical contact with the electrolyte bath, wherein the cathode comprises aluminum;
(c) providing an anode in electrical contact with the electrolyte bath;
(d) adding a first portion of Sc2O3 into the electrolyte bath;
(e) reacting an aluminum ion with the cathode; and
(f) applying an electric current to the cathode, thereby reacting a scandium ion with the cathode to produce the Al—Sc alloy, wherein after reacting the scandium ion with the cathode:
the electrolyte bath comprises ScF3, AlF3, and at least one of LiF, NaF, or KF, and
the cathode comprises the aluminum and scandium.

### Claim 2 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy comprises between about 5-12 weight % scandium.

### Claim 3 (depends on 1)

The method of claim 1, wherein the Al—Sc alloy comprises between about 8-12 weight % scandium.

### Claim 4 (depends on 1)

The method of claim 1, wherein at least a portion of the aluminum and the scandium in the cathode is a liquid.

### Claim 5 (depends on 1)

The method of claim 1, wherein the electric current to the cathode has a current density of about 0.2-1.0 A/cm2.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
maintaining a predetermined molar ratio of the scandium ion to the aluminum ion of about 0:1 to about 2:1, wherein the predetermined ratio is maintained by controlling the electric current to the cathode.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
maintaining a predetermined molar ratio of an oxygen ion to a fluoride ion of about 1:20 to about 1:250, wherein the predetermined ratio of the oxygen ion to the fluoride ion is maintained by:
controlling the electric current, or
adding a second portion of Sc2O3 into the electrolyte bath.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
maintaining a predetermined molar ratio of a lithium ion to the scandium ion and the aluminum ion of about 0.5:1 to about 4:1, wherein the predetermined molar ratio is maintained by adding a second portion of LiF.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
maintaining a predetermined molar ratio of a sodium ion to the scandium ion and the aluminum ion of about 0.5:1 to about 6:1, wherein the predetermined molar ratio is maintained by adding a second portion of NaF.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
maintaining a predetermined molar ratio of a potassium ion to the scandium ion and the aluminum ion of about 0.5:1 to about 6:1, wherein the predetermined molar ratio is maintained by adding a second portion of KF.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
adding a second portion of Sc2O3, AlF3, and a second portion of at least one of LiF, NaF, or KF into the electrolyte bath.

### Claim 12 (depends on 11)

The method of claim 11, wherein the second portion of Sc2O3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 17-38 weight % ScF3, about 15-28 weight % AlF3, about 43-55 weight % NaF, and about 1-5 weight % Sc2O3.

### Claim 13 (depends on 11)

The method of claim 11, wherein the second portion of Sc2O3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 22-45 wt % ScF3, about 18-33 wt % AlF3, about 31-43 wt % LiF, and about 1-6 wt % Sc2O3.

### Claim 14 (depends on 11)

The method of claim 11, wherein the second portion of Sc2O3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 14-32 wt % ScF3, about 12-24 wt % AlF3, about 51-63 wt % KF, and about 1-5 wt % Sc2O3.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
adding a second portion of Sc2O3, ScF3, AlF3, and a second portion of at least one of LiF, NaF, or KF into the electrolyte bath.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second portion of Sc2O3, ScF3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 17-38 weight % ScF3, about 15-28 weight % AlF3, about 43-55 weight % NaF, and about 1-5 weight % Sc2O3.

### Claim 17 (depends on 15)

The method of claim 15, wherein the second portion of Sc2O3, ScF3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 22-45 wt % ScF3, about 18-33 wt % AlF3, about 31-43 wt % LiF, and about 1-6 wt % Sc2O3.

### Claim 18 (depends on 15)

The method of claim 15, wherein the second portion of Sc2O3, ScF3, AlF3, and the second portion of at least one of LiF, NaF, or KF are added such that the electrolyte bath comprises about 14-32 wt % ScF3, about 12-24 wt % AlF3, about 51-63 wt % KF, and about 1-5 wt % Sc2O3.