# US 2025/0059362 A1 · Soft polyolefin composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0059362 A1
- Document ID: US20250059362A1
- Status: Published application
- Kind: A1
- Application number: 18/720,986
- Filed: 2022-12-12
- Published: 2025-02-20
- Earliest claimed: 2021-12-23
- Assignees: Basell Poliolefine Italia S.r.l.
- Applicants: Basell Poliolefine Italia S.r.l.
- Inventors: Michele Grazzi; Monica Galvan
- Web page: https://patentgrep.com/patent/US20250059362A1

## CPC

- C08L 23/12: Polypropene
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- C08L 23/20: having four to nine carbon atoms
- C08L 2203/16: used for films
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polyolefin composition made from or containing (I) 75-95 wt % of a thermoplastic polyolefin made from or containing (A) 18-30 wt % of a propylene copolymer with 1.0-6.0 wt. % of CH2═CHR comonomer, having a melt flow rate (MFR) ranging from 30 to 60 g/10 min; and (B) 70-82 wt % of a propylene copolymer with 20-35 wt. % of CH2═CHR comonomer, and optionally a diene, wherein the thermoplastic polyolefin has i) a xylene soluble fraction equal to or greater than 70 wt. %; and ii) a MFR from 0.2 to 15.0 g/10 min, and (II) 5-25 wt % of a polybutene component, having a flexural modulus equal to or lower than 60 MPa and made from or containing a butene-1 copolymer with ethylene and optionally a comonomer of formula CH2═CHR1, wherein the copolymer having i) up to and including 20 wt % of ethylene-or comonomer-derived units; and ii) Mw/Mn equal to or lower than 3.

## Claims

### Claim 1

A polyolefin composition comprising:
(I) 75-95% by weight of a thermoplastic polyolefin comprising:
(A) 18-30% by weight of a copolymer of propylene with from 1.0 to 6.0% by weight of a comonomer of formula CH2═CHR, where R is H or a linear or branched C2-C8 alkyl, based on the weight of (A), and having a melt flow rate (MFR(A)), measured according to ISO 1133 (230° C., 2.16 kg), ranging from 30 to 60 g/10 min; and
(B) 70-82% by weight of a copolymer of propylene with from 20 to 35% by weight of a comonomer of formula CH2═CHR, and optionally a diene, where R is H or a linear or branched C2-C8 alkyl, based on the weight of (B),
wherein the thermoplastic polyolefin has
i) an amount of fraction soluble in xylene at 25° C. (XS(I)) equal to or greater than 70% by weight, based on the total weight of (A)+(B); and
ii) a melt flow rate (MFR(I)), measured according to ISO 1133 (230° C., 2.16 kg) from 0.2 to 15.0 g/10 min, and
wherein the amounts of (A) and (B) are based on the total weight of (A)+(B); and
(II) 5-25% by weight of a polybutene component,
having a flexural modulus equal to or lower than 60 MPa, measured according to the method ISO 178:2019 and
comprising a copolymer of butene-1 with ethylene and optionally a comonomer of formula CH2═CHR1, where R1 is methyl or a linear or branched C3-C8 alkyl,
wherein the copolymer of butene-1 having
iii) up to and including 20% by weight of units deriving from ethylene and optionally the comonomer, based on the weight of (II); and
ii) a molecular weight distribution Mw/Mn equal to or lower than 3;
wherein the amounts of (I) and (II) are based on the total weight of (I)+(II).

### Claim 2 (depends on 1)

The polyolefin composition of claim 1 comprising from 80 to 90% by weight of the thermoplastic polyolefin (I) and from 10 to 20% by weight of the polybutene component (II), wherein the amounts of (I) and (II) are based on the total weight of (I)+(II).

### Claim 3 (depends on 1)

The polyolefin composition of claim 1, wherein the comonomers CH2═CHR of components (A) and (B) of the thermoplastic polyolefin (I) are independently selected from the group consisting of ethylene, butene-1, hexene-1, 4-methy-pentene-1, octene-1 and combinations thereof.

### Claim 4 (depends on 1)

The polyolefin composition according to claim 1, wherein the thermoplastic polyolefin (I) has an amount of fraction soluble in xylene at 25° C. (XS(I)) ranging from 70 to 90% by weight, based on the weight of the thermoplastic polyolefin (I).

### Claim 5 (depends on 1)

The polyolefin composition according to claim 1, wherein the fraction soluble in xylene at 25° C. of the thermoplastic polyolefin (I) has an intrinsic viscosity XSIV(I) ranging from 2.5 to 4.5 dl/g.

### Claim 6 (depends on 1)

The polyolefin composition according to claim 1, wherein the thermoplastic polyolefin (I) has a melt flow rate MFR(I), measured according to ISO 1133 (230° C., 2.16 kg), ranging from 0.2 to 5.0 g/10 min.

### Claim 7 (depends on 1)

The polyolefin composition according to claim 1, wherein the propylene copolymer (A) has a melt flow rate (MFR(A)), measured according to ISO 1133 (230° C., 2.16 kg), ranging from 35 to 50 g/10 min.

### Claim 8 (depends on 1)

The polyolefin composition according to claim 1, wherein the copolymer of butene-1 of the polybutene component (II) is a copolymer of butene-1 and ethylene having from 5 to 10% by weight of units deriving from ethylene, based on the weight of polybutene component (II).

### Claim 9 (depends on 1)

The polyolefin composition according to claim 1, wherein the polybutene component (II) has a flexural modulus equal to or lower than 60 MPa, measured according to the method ISO 178:2019.

### Claim 10 (depends on 1)

The polyolefin composition according to claim 1, wherein the polybutene component (II) has at least one of the following properties:
a shore A value equal to or lower than 90, measured according to the method ISO 868 on compression-molded specimens; or
a compression set equal to or lower than 50%, measured on compression-molded specimens according to the method ASTM D395 at 23° C. and 25% deformation.

### Claim 11 (depends on 1)

A shaped article comprising the polyolefin composition according to claim 1.

### Claim 12 (depends on 11)

The shaped article according to claim 11, wherein the article is a film or sheet.

### Claim 13 (depends on 12)

The shaped article according to claim 12, comprising a layer X and a layer Y adhered to a surface of the layer X, wherein the layer X comprises the polyolefin composition and the layer Y comprises a plastic material selected from the group consisting of propylene homopolymers, propylene copolymers, polyethylene, polyethylene terephthalate, and combinations thereof.

### Claim 14 (depends on 12)

The shaped article according to claim 12, wherein the film or sheet is a layer of a single-ply roofing sheet or membrane.

### Claim 15 (depends on 12)

The shaped article according to claim 12, wherein the film or sheet is a layer of a geomembrane.