# US 2025/0059307 A1 · Ethylene/1-Hexene Copolymer Having Improved Long-Term Physical Property Stability and Processibility

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0059307 A1
- Document ID: US20250059307A1
- Status: Published application
- Kind: A1
- Application number: 18/726,279
- Filed: 2023-03-07
- Published: 2025-02-20
- Earliest claimed: 2022-03-10
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Joongsoo Kim; Yutaek Sung; Ka Ram Sun; Jinyoung Lee; Hyojoon Lee; Yeonsoo Kim; So Dam Jeong; Min Hong Jeon
- Web page: https://patentgrep.com/patent/US20250059307A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- F16L 9/12: of plastics with or without reinforcement (F16L9/16 - F16L9/22 take precedence)
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F 2420/07: Heteroatom-substituted Cp, i.e. Cp or analog where at least one of the substituent of the Cp or analog ring is or contains a heteroatom
- C08F 2420/10: Heteroatom-substituted bridge, i.e. Cp or analog where the bridge linking the two Cps or analogs is substituted by at least one group that contains a heteroatom
- C08F 2500/07: High density, i.e. > 0.95 g/cm3
- C08F 2500/12: Melt flow index or melt flow ratio
- C08F 2500/31: Impact strength or impact resistance, e.g. Izod, Charpy or notched
- C08F 2800/20: as weight or mass percentages
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

Provided is an ethylene/1-hexene copolymer satisfying the following conditions, having excellent long-term stability and processability as well as pipe resistance to internal pressure, and being useful for manufacturing high-pressure heating pipes, PE-RT pipes or large-diameter pipes, a molecular weight distribution (Mw/Mn) is 8 to 12, a broad orthogonal co-monomer distribution (BOCD) is 1 to 2, an integral value in the region where Log M is 6 or more in a gel permeation chromatography GPC curve graph having an x-axis of log M and a y-axis of dw/dlogM is 3.0% or more of the total integral value, and a tie molecule fraction is 6.0% or more.

## Claims

### Claim 1

An ethylene/1-hexene copolymer satisfying the following conditions:
a molecular weight distribution (Mw/Mn) is 8 to 12,
(a broad orthogonal co-monomer distribution) (BOCD) is 1 to 2,
an integral value in a region where Log M is 6 or more in a gel permeation chromatography (GPC) curve graph having an x-axis of log M and a y-axis of dw/dlogM is 3.0% or more of a total integral value, wherein the log M is a a log value of a weight average molecular weight, and the dwt/dlog M is a molecular weight distribution, and
a tie molecule fraction is 6.0% or more.

### Claim 2 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
wherein the molecular weight distribution (Mw/Mn) is 10 to 11.8.

### Claim 3 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
wherein the BOCD is 1.04 to 1.8.

### Claim 4 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
wherein the integral value in the region where Log M is 6 or more in a GPC curve graph having an x-axis of log M and a y-axis of dw/dlogM is 3.03% or more of the total integral value.

### Claim 5 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
wherein the tie molecule fraction is 6.05% or more.

### Claim 6 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a density measured according to ASTM D 1505 is of 0.945 g/cm3 to 0.955 g/cm3.

### Claim 7 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a melt index (MI2.16) measured at 190° C. under a load of 2.16 kg according to ASTM D 1238 0.05 g/10 min to 0.25 g/10 min.

### Claim 8 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a high-load melt index (HLMI, MI21.6) measured at 190° C. under a load of 21.6 kg according to ASTM D 1238 is of 10 g/10 min to 18 g/10 min.

### Claim 9 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a melt flow rate ratio (MI21.6/MI2.16) measured at 190° C. according to ASTM D 1238 is of 85 to 120.

### Claim 10 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a characteristic stress measured according to ASTM D 638 is of 13 MPa to 14.5 MPa.

### Claim 11 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a resistance to internal pressure measured according to ISO 9080 of 10 MPa to 12 MPa.

### Claim 12 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a strain hardening modulus, which is a slope of a linear fitting value between a true strain 8 and 12 in a Hookean constitutive model curve after measuring a strain/stress curve under 80° C. and 20 mm/min in accordance with ISO 18488 to obtain a Neo-Hookean constitutive model curve having a x-axis of λ2−1/λ, and a y-axis of σtrue of 23 MPa to 25 MPa.

### Claim 13 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
which has a notch pipe test (NPT) result according to ISO 13479 of 1500 to 4000 hours.

### Claim 14 (depends on 1)

The ethylene/1-hexene copolymer of claim 1,
wherein a 1-hexene content in the ethylene/1-hexene copolymer is 3.0 wt % to 7.0 wt % based on a total weight of the ethylene/1-hexene copolymer.

### Claim 15 (depends on 1)

A method for preparing the ethylene/1-hexene copolymer according to claim 1, comprising copolymerizing ethylene and 1-hexene in a mono-modal polymerization process in the presence of a catalyst composition comprising a first metallocene compound represented by Chemical Formula 1 and a second metallocene compound represented by Chemical Formula 2 while introducing hydrogen gas,
wherein the first metallocene compound and the second metallocene compound are included in a molar ratio of 1:2 to 1:8:
(Cp1Ra)n(Cp2Rb)M1Z3-n1 [Chemical Formula 1]
in Chemical Formula 1,
M1 is a Group 4 transition metal;
each of Cp1 and Cp2 is independently cyclopentadienyl unsubstituted or substituted with C1-20 hydrocarbon;
Ra and Rb are the same as or different from each other, and are each independently hydrogen, C1-20 alkyl, C1-20 alkoxy, C2-20 alkoxyalkyl, C6-20 aryl, C6-20 aryloxy, C2-20 alkenyl, C7-40 alkylaryl, C7-40 arylalkyl, C8-40 arylalkenyl, C2-20 alkynyl, or substituted or unsubstituted C2-20 heteroaryl containing at least one N, O or S, provided that at least one of Ra or Rb is not hydrogen;
Z1 are each independently halogen, C1-20 alkyl, C2-20 alkenyl, C7-40 alkylaryl, C7-40 arylalkyl, C6-20 aryl, substituted or unsubstituted C1-20 alkylidene, substituted or unsubstituted amino, C2-20 alkylalkoxy, or C7-40 arylalkoxy; and
n is 1 or 0,
in Chemical Formula 2,
M2 is a Group 4 transition metal;
A is carbon, silicon, or germanium;
X1 and X2 are the same as or different from each other, and are each independently halogen, or C1-20 alkyl;
R1 to R4 are the same as or different from each other, and are each independently hydrogen, C1-20 alkyl, C2-20 alkenyl, C6-20 aryl, C7-20 alkylaryl, or C7-20 arylalkyl, or two or more substituents adjacent to each other of R1 to R4 are connected with each other to form a substituted or unsubstituted aliphatic ring, a substituted or unsubstituted aromatic ring, or a substituted or unsubstituted heteroaromatic ring containing at least one N, O or S;
R5 and R6 are the same as or different from each other, and are each independently C1-20 alkyl, C2-20 alkenyl, C6-30 aryl, or C2-20 alkoxyalkyl; and
R7 is C1-20 alkyl, C2-20 alkenyl, or C6-30 aryl.

### Claim 16 (depends on 15)

The method of claim 15,
wherein the first metallocene compound is represented by any one of the following structural formulae:

### Claim 17 (depends on 15)

The method of claim 15,
wherein the second metallocene compound is represented by any one of the following structural formulae:

### Claim 18 (depends on 15)

The method of claim 15,
wherein the mono-modal polymerization process is performed in a single loop slurry reactor.

### Claim 19 (depends on 15)

The method of claim 15,
wherein the 1-hexene is included in an amount of 4.0 wt % to 6.0 wt % based on a total weight of the ethylene in the copolymerization process.

### Claim 20 (depends on 1)

A pipe comprising the ethylene/1-hexene copolymer of claim 1.