# US 2025/0059089 A1 · Methods for carbon-capture within biochar

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0059089 A1
- Document ID: US20250059089A1
- Status: Published application
- Kind: A1
- Application number: 18/815,916
- Filed: 2024-08-27
- Published: 2025-02-20
- Earliest claimed: 2023-03-03
- Assignees: Washington State University
- Applicants: Washington State University
- Inventors: Xianming Shi; Zhipeng Li
- Web page: https://patentgrep.com/patent/US20250059089A1

## CPC

- B01D 53/62: Carbon oxides
- C04B 14/28: of calcium
- B01D 53/80: Semi-solid phase processes, i.e. by using slurries
- C04B 28/04: Portland cements
- B01D 2251/404: of calcium
- B01D 2253/102: Carbon
- B01D 2257/504: Carbon dioxide
- B01D 2259/4591: Construction elements containing cleaning material, e.g. catalysts
- Y02P 40/18: Carbon capture and storage [CCS]
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods for carbon-capture within a biochar are provided. The method includes mixing a biochar with an alkaline solution to form an intermediate mixture and exposing the intermediate mixture to a CO2 source so as to precipitate calcium carbonate onto and into the biochar to form a CO2-weathered biochar. In some cases, the method also includes injecting CO2 into alkaline wastewater to sequester/store CO2 which can then serve as mixing water for producing cementitious composites. This method may be used to upcycle three waste streams, and treated CO2-weathered biochar preserves compressive strength of resultant concrete when substituted for a portion of the pre-cure cement and aggregate components. Further, treated CO2-weathered recycled aggregate preserves mechanical strength of resultant concrete when substituted for a portion of aggregate.

## Claims

### Claim 1

A CO2-weathered biochar, comprising:
a biochar; and
calcium carbonate particles precipitated on or within the biochar, wherein a size of the calcium carbonate particles ranges from 1-5000 nanometers.

### Claim 2

A cementitious composite, comprising:
a biochar;
calcium carbonate particles precipitated on or within the biochar, wherein a size of the calcium carbonate particles ranges from 1-5000 nanometers;
cement; and
an aqueous solution.

### Claim 3 (depends on 2)

The cementitious composite of claim 2, wherein the biochar comprises particles having a size of 150 micrometers or less.

### Claim 4 (depends on 3)

The cementitious composite of claim 3, wherein the CO2-weathered biochar replaces 1% to 80% by mass of a dry pre-mix total quantity of the cement in the cementitious composite.

### Claim 5 (depends on 4)

The cementitious composite of claim 4, wherein the CO2-weathered biochar replaces 1% to 40% by mass of a dry pre-mix total quantity of the cement in the cementitious composite.

### Claim 6 (depends on 2)

The cementitious composite of claim 2, wherein the biochar comprises particles having a size of 1-150 micrometers.

### Claim 7 (depends on 6)

The cementitious composite of claim 6, wherein the cementitious composite further comprises aggregates and wherein the CO2-weathered biochar replaces 1% to 20% by mass of a dry pre-mix total quantity of the aggregates in the cementitious composite.

### Claim 8 (depends on 6)

The cementitious composite of claim 6, wherein the cementitious composite does not comprise any aggregates.

### Claim 9 (depends on 6)

The cementitious composite of claim 6, wherein the cementitious composite comprises recycled aggregate.

### Claim 10 (depends on 9)

The cementitious composite of claim 9, wherein the recycled aggregate is carbonated.

### Claim 11 (depends on 2)

The cementitious composite of claim 2, wherein a compressive strength of the cementitious composite is increased as compared to a corresponding cementitious composite without the CO2-weathered biochar.

### Claim 12 (depends on 2)

The cementitious composite of claim 2, wherein the cementitious composite is selected from the group consisting of concrete, paste, grout, mortar, and cement stabilized soil.

### Claim 13 (depends on 2)

The cementitious composite of claim 2, wherein the biochar is a surface-modified biochar.

### Claim 14 (depends on 2)

The cementitious composite of claim 2, wherein the cementitious composite further comprises a fiber material.

### Claim 15

A method for carbon capture within a cementitious composite, comprising:
mixing a biochar with an alkaline solution to form an intermediate mixture;
exposing the intermediate mixture to a CO2 source so as to precipitate calcium carbonate particles onto and into the biochar to form a CO2-weathered biochar, wherein a size of the calcium carbonate particles ranges from 1-5000 nanometers; and
mixing the CO2-weathered biochar with a cement and an aqueous solution to form the cementitious composite.

### Claim 16 (depends on 15)

The method of claim 15, wherein the cementitious composite comprises recycled aggregate and wherein the recycled aggregate is carbonated by
mixing the recycled aggregate with a second alkaline solution to form a second intermediate mixture; and
exposing the second intermediate mixture to a CO2 source so as to precipitate calcium carbonate onto and into the recycled aggregate to form a CO2-weathered recycled aggregate.

### Claim 17 (depends on 15)

The method of claim 15, wherein the biochar is carbonated.

### Claim 18 (depends on 15)

The method of claim 15, wherein the aqueous solution is a carbonated alkaline aqueous solution.

### Claim 19 (depends on 15)

The method of claim 15, further comprising pretreating the biochar with a solution containing nanomaterials before the biochar is mixed with the alkaline solution.

### Claim 20 (depends on 15)

The method of claim 15, further comprising pretreating the biochar with one or more oxidizing agents before the biochar is mixed with the alkaline solution.