# US 2025/0058379 A1 · Method of preparing iridium nanocrystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0058379 A1
- Document ID: US20250058379A1
- Status: Published application
- Kind: A1
- Application number: 18/938,081
- Filed: 2024-11-05
- Published: 2025-02-20
- Earliest claimed: 2022-12-13
- Assignees: PetroChina Company Limited
- Applicants: PetroChina Company Limited
- Inventors: Yanfei WANG; Yinglong YU; Chenyi SHAO; Chuan LONG; Qinfeng ZHAO; Jingjing WANG; Yeheng HE; Qingxun LI
- Web page: https://patentgrep.com/patent/US20250058379A1

## CPC

- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 1/054: Nanosized particles
- B22F 1/07: Metallic powder characterised by particles having a nanoscale microstructure (nanosized particles B22F1/054)
- B22F 9/002: {amorphous or microcrystalline}
- C25B 11/081: the element being a noble metal
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 28/04: from liquids
- C30B 29/02: Elements
- B22F 2009/245: {Reduction reaction in an Ionic Liquid [IL]}
- B22F 2201/10: Inert gases
- B22F 2301/25: Noble metals, i.e. Ag Au, Ir, Os, Pd, Pt, Rh, Ru
- B22F 2998/10: Processes characterised by the sequence of their steps
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C25B 1/04: by electrolysis of water
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

The present application provides a preparation method for iridium nanocrystal, including the following steps: mixing an iridium salt, an alcohol solvent and a centrifugal waste liquid to form a mixed solution, and adding an alkali solution in an inert atmosphere for a heating reaction. After centrifugation, an iridium nanocrystal is obtained. The centrifugal waste liquid is a waste liquid produced in the pre-synthesis process of iridium nanocrystal. The preparation method can shorten the reaction time, and the obtained iridium nanocrystal has the advantages of high yield and low cost.

## Claims

### Claim 1

A preparation method for an iridium nanocrystal, comprising the following steps:
mixing an iridium salt, an alcohol solvent and a centrifugal waste liquid to form a mixed solution, and adding an alkali solution in an inert atmosphere for a heating reaction, centrifuging to obtaining an iridium nanocrystal, wherein the heating reaction is performed under a condition of a temperature of 140-220° C. and a time not exceeding 6 h; a volume of the centrifugal waste liquid is 10-50% of a volume of the mixed solution; and the centrifugal waste liquid is a waste liquid produced by a pre-synthesis process of the iridium nanocrystal.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in the inert atmosphere, the mixed solution is heated to 120-220° C. and then the alkali solution is added.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the heating reaction has a time of 1-5 h.

### Claim 4 (depends on 2)

The preparation method according to claim 2, wherein the heating reaction has a time of 1-5 h.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the heating reaction has a time of 1.5-2 h.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein the volume of the centrifugal waste liquid is 15-40% of the volume of the mixed solution.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein a mass content of the iridium salt in the mixed solution is 0.02%-0.1%.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein an average particle size of the iridium nanocrystal is 5-60 nm.

### Claim 9 (depends on 1)

The preparation method according to claim 1, wherein the centrifugal waste liquid is a waste liquid produced by a primary synthesis process of the iridium nanocrystal.

### Claim 10 (depends on 1)

The preparation method according to claim 1, wherein the iridium salt includes at least one of iridium trichloride, iridium tetrachloride, chloroiridic acid and iridium acetate.

### Claim 11 (depends on 1)

The preparation method according to claim 1, wherein the alkali solution contains an alkaline compound, and a molar ratio of the alkaline compound to the iridium salt is (0.1-1):1.

### Claim 12 (depends on 1)

The preparation method according to claim 1, wherein a molar ratio of the alcohol solvent to the iridium salt is (8000-14000):1.

### Claim 13 (depends on 1)

The preparation method according to claim 1, wherein the mixed solution also contains an organic ligand; and the organic ligand comprises at least one of ethylenediamine, polyacrylamide, citric acid and malic acid.

### Claim 14 (depends on 1)

The preparation method according to claim 1, wherein a molar ratio of the organic ligand to the iridium salt is (0.05-5):1.