# US 2025/0051227 A1 · METHOD FOR PRODUCING CALCINED PRODUCT COMPRISING gamma-2CaOSiO2

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0051227 A1
- Document ID: US20250051227A1
- Status: Published application
- Kind: A1
- Application number: 18/698,154
- Filed: 2022-10-07
- Published: 2025-02-13
- Earliest claimed: 2021-10-13
- Assignees: Tokuyama Corporation
- Applicants: Tokuyama Corporation
- Inventors: Masami OTA
- Web page: https://patentgrep.com/patent/US20250051227A1

## CPC

- C01B 33/24: Alkaline-earth metal silicates
- C04B 7/434: {Preheating with addition of fuel, e.g. calcining}
- C04B 7/3453: {Belite cements, e.g. self-disintegrating cements based on dicalciumsilicate}
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

By preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2 O3 after heating at 1000° C. of 5.0 mass % or less, and calcining at a calcination temperature of 1350° C. to 1600° C., it is possible to efficiently use waste materials as a part of raw materials, and to obtain a calcined product that comprises almost an equivalent amount of γ-2CaO·SiO2 as conventional can be obtained.

## Claims

### Claim 1

A method of producing a calcined product comprising γ-2CaO·SiO2, the method comprising preparing a raw material mixture comprising CaO raw material, SiO2 raw material and waste material, and having a content of Al2 O3 after heating at 1000° C. of 5.0 mass % or less, and calcining at a calcination temperature of 1350° C. to 1600° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the waste material is at least one waste material selected from coal ash, blast furnace slag, concrete sludge, waste concrete, incineration fly ash, and municipal waste incineration ash.

### Claim 3 (depends on 1, 2)

The method according to claim 1 or 2, wherein the raw material mixture is a raw material mixture which total content of Al2O3 and Fe2O3 after heating at 1000° C. is 5.0 mass % or more.

### Claim 4 (depends on 1, 2)