# US 2025/0043469 A1 · Device And Process For Manufacturing Natural Fiber Filling Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0043469 A1
- Document ID: US20250043469A1
- Status: Published application
- Kind: A1
- Application number: 18/671,987
- Filed: 2024-05-22
- Published: 2025-02-06
- Earliest claimed: 2023-08-04
- Assignees: Nalexible(Beijing)Technology Co., Ltd
- Applicants: Nalexible(Beijing)Technology Co., Ltd
- Inventors: Zhibin Song
- Web page: https://patentgrep.com/patent/US20250043469A1

## CPC

- B27N 1/00: Pretreatment of moulding material
- D03D 15/217: natural from plants, e.g. cotton
- B27N 1/029: {Feeding; Proportioning; Controlling}
- B27N 3/02: from particles
- B27N 3/12: from fibres
- B27N 3/18: Auxiliary operations, e.g. preheating, humidifying, cutting-off
- B27N 3/203: {with heating or cooling means}
- D03D 15/283: synthetic polymer-based, e.g. polyamide or polyester fibres (cellulose-based artificial fibres D03D15/225)
- D03D 15/47: multicomponent, e.g. blended yarns or threads (multicomponent fibres or filaments D03D15/292)
- D03D 23/00: General weaving methods not special to the production of any particular woven fabric or the use of any particular loom; Weaves not provided for in any other single group
- D03D 25/005: {Three-dimensional woven fabrics}
- B29C 43/003: {characterised by the choice of material}
- B29C 43/006: {Pressing and sintering powders, granules or fibres}
- B29C 43/02: of articles of definite length, i.e. discrete articles {(B29C35/0227 takes precedence)}
- D10B 2201/01: Natural vegetable fibres
- D10B 2321/022: polypropylene
- D10B 2403/033: Three dimensional fabric, e.g. forming or comprising cavities in or protrusions from the basic planar configuration, or deviations from the cylindrical shape as generally imposed by the fabric forming process
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- D03D: WOVEN FABRICS; METHODS OF WEAVING; LOOMS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

Disclosed in the present invention is a device for manufacturing a natural fiber filling material, which includes a ground, a mixed fiber felt preparation machine, an open-type oil heating mold, a hydraulic press, a single-sided roller gluing machine, a cold press, a lower mold, a hydraulic cylinder, an upper mold, a control box, a heat dissipation mechanism and a lubricating mechanism. The present invention relates to a device for manufacturing a natural fiber filling material. The device has a function of quickly dissipating heat from the control box on the cold press and can lubricate the hydraulic cylinder on the cold press.

## Claims

### Claim 1

A device for manufacturing a natural fiber filling material, comprising a ground (1), a mixed fiber felt preparation machine (2), an open-type oil heating mold (3), a hydraulic press (4), a single-sided roller gluing machine (5), a cold press (6), a lower mold (7), a hydraulic cylinder (8), an upper mold (9), a control box (10), a heat dissipation mechanism (11) and a lubricating mechanism (12), wherein the mixed fiber felt preparation machine (2) is disposed on the ground (1), the open-type oil heating mold (3) is disposed on the ground (1), the hydraulic press (4) is disposed on the ground (1), the single-sided roller gluing machine (5) is disposed on the ground (1), the cold press (6) is disposed on the ground (1), the hydraulic press (4) is provided with the lower mold (7), the hydraulic cylinder (8) is disposed on the hydraulic press (4), a telescopic end of the hydraulic cylinder (8) is slidably connected with the hydraulic press (4), the telescopic end of the hydraulic cylinder (8) is fixedly connected with the upper mold (9), the hydraulic press (4) is provided with the control box (10), the control box (10) is provided with the heat dissipation mechanism (11), and the hydraulic press (4) is provided with the lubricating mechanism (12).

### Claim 2 (depends on 1)

The device for manufacturing the natural fiber filling material according to claim 1, wherein the heat dissipation mechanism (11) comprises ventilation holes (111), an air inlet hole (112), a mounting housing (113), a semiconductor refrigeration sheet (114), a motor I (115), a bevel gear I (116), fan blades (117), a mounting disk (118), a filter screen (119), a mounting rod (1191), a rotating shaft (1192), a bevel gear II (11921), ejection plates (1193), a scraper (1194) and an elastic air bag (1195), the ventilation holes (111) are formed in the control box (10), the air inlet hole (112) is formed in the control box (10), the control box (10) is fixedly connected with the mounting housing (113), the semiconductor refrigeration sheet (114) is fixedly mounted in the mounting housing (113), a cold end of the semiconductor refrigeration sheet (114) is located inside the mounting housing (113), a hot end of the semiconductor refrigeration sheet (114) is located outside the mounting housing (113), the motor I (115) is fixedly mounted in the mounting housing (113), an outer side of an output end of the motor I (115) is fixedly sleeved with the bevel gear I (116), the output end of the motor I (115) is fixedly connected with the fan blades (117), the mounting disk (118) is fixedly connected in the mounting housing (113), the filter screen (119) is fixedly connected in the mounting disk (118), the mounting rod (1191) is fixedly connected in the mounting housing (113), the rotating shaft (1192) is mounted in the mounting rod (1191) through a bearing, the rotating shaft (1192) is rotatably connected with the mounting disk (118), the ejection plates (1193) are slidably connected in the rotating shaft (1192), the ejection plates (1193) are fixedly connected with the scraper (1194), and the scraper (1194) is slidably connected with the filter screen (119) and the mounting disk (118).

### Claim 3 (depends on 2)

The device for manufacturing the natural fiber filling material according to claim 2, wherein an outer side of the rotating shaft (1192) is fixedly sleeved with the bevel gear II (11921), and the bevel gear II (11921) is meshed with the bevel gear I (116).

### Claim 4 (depends on 2)

The device for manufacturing the natural fiber filling material according to claim 2, wherein the elastic air bag (1195) is bonded to the scraper (1194), and the other end of the elastic air bag (1195) is bonded to the rotating shaft (1192).

### Claim 5 (depends on 2)

The device for manufacturing the natural fiber filling material according to claim 2, wherein a plurality of fan blades (117) are provided, and the plurality of fan blades (117) are arranged in an annular array on the output end of the motor I (115).

### Claim 6 (depends on 1)

The device for manufacturing the natural fiber filling material according to claim 1, wherein the lubricating mechanism (12) comprises a flow guide pipe (121), an oil storage barrel (122), a sealing ball (123), a supporting shaft (124), a rotating end (125), a belt pulley I (126), a mounting plate (127), a motor II (128), a belt pulley II (129), a belt (1291), clamping holes (1292), an elastic block (1293) and a clamping ball (1294), the flow guide pipe (121) is fixedly connected in the hydraulic press (4), the hydraulic press (4) is fixedly connected with the oil storage barrel (122), the sealing ball (123) is rotatably connected in the oil storage barrel (122), the supporting shaft (124) is fixedly connected with the sealing ball (123), the supporting shaft (124) is rotatably connected with the oil storage barrel (122), the rotating end (125) is fixedly connected with the sealing ball (123), the rotating end (125) is rotatably connected with the oil storage barrel (122), an outer side of the rotating end (125) is fixedly sleeved with the belt pulley I (126), the mounting plate (127) is fixedly connected in the oil storage barrel (122), the motor II (128) is fixedly mounted on the mounting plate (127), an output shaft of the motor II (128) is rotatably connected with the mounting plate (127), an outer side of the output shaft of the motor II (128) is fixedly sleeved with the belt pulley II (129), the belt pulley II (129) and the belt pulley I (126) are jointly sleeved with the belt (1291), the clamping holes (1292) are formed in the output shaft of the motor II (128), the elastic block (1293) is bonded in the oil storage barrel (122), the clamping ball (1294) is bonded in the elastic block (1293), and the clamping ball (1294) is slidably connected with the clamping hole (1292).

### Claim 7 (depends on 6)

The device for manufacturing the natural fiber filling material according to claim 6, wherein a plurality of clamping holes (1292) are formed, and the plurality of clamping holes (1292) are arranged in an annular array on the output shaft of the motor II (128).

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

A use method of the device for manufacturing the natural fiber filling material according to any one of claims 1-7, wherein the use method specifically comprises:
step one: preparing wood fiber, hemp fiber and polypropylene fiber into filaments, wherein a mass ratio of wood fiber to hemp fiber to polypropylene fiber is (1-3):(3-5):(3-5); under the action of the mixed fiber felt preparation machine (2), opening, premixing, mixing and separating, carding, crossing, lapping, pre-needling, finish-needling and cutting off the obtained filamentous fiber so as to be woven into mixed fiber felt, and putting the mixed fiber felt into the open-type oil heating mold (3) and heating the mixed fiber felt in the open-type oil heating mold (3) at a temperature of 200-240° C. for 1-2 minutes;
step two: then, taking out the mixed fiber felt in a soft state and putting the mixed fiber felt into the lower mold (7), keeping the mixed fiber felt in the mold under a pressure of 20-25 Mpa from the hydraulic press (4) for 2-3 minutes, and taking out a molded natural fiber substrate;
step three: in this process, through the arrangement of the control box (10), possibly performing the following operations: controlling and using the hydraulic cylinder (8); in order to ensure that electronic elements in the control box (10) operate at a normal temperature, starting the semiconductor refrigeration sheet (114) to cool air; starting the motor I (115) to drive the output end to rotate, so as to drive the fan blades (117) to rotate and blow the air, for the purpose of accelerating circulation of cold air and improving a heat dissipation effect of the control box (10); filtering out dust in the air under the action of the filter screen (119); driving the bevel gear I (116) to rotate when the motor I (115) drives the output end to rotate; under a meshing relationship, allowing the bevel gear I (116) to be forced to drive the bevel gear II (11921) to rotate, further to drive the rotating shaft (1192) to rotate, further to cause the ejection plates (1193) to drive the scraper (1194) to slide along a surface of the filter screen (119), so as to clean the dust attached to the filter screen (119) and avoid the blockage of the filter screen (119); and when the scraper (1194) is worn and thinned after long-time use, pushing, under the deformation of the elastic air bag (1195), the scraper (1194) to be in contact with the filter screen (119) to ensure a cleaning effect of the scraper (1194);
step four: starting the motor II (128) to drive the output shaft to rotate, so as to drive the belt pulley II (129) to rotate, and then drive the belt (1291) to drive, and finally drive the belt pulley I (126) to rotate; driving the rotating end (125) to rotate by the belt pulley I (126) under a force to drive the sealing ball (123) to deflect, so that a through hole formed in the sealing ball (123) rotates, and then the oil storage barrel (122) is in a circulating state, wherein during this process, the clamping hole (1292) is forced to squeeze the clamping ball (1294), the clamping ball (1294) is forced to push the elastic block (1293) to deform and finally the clamping ball (1294) is separated from the clamping hole (1292), the clamping ball (1294) slides along a surface of the output shaft of the motor II (128) under the action of force, when the clamping ball (1294) slides into the next clamping hole (1292), the elastic block (1293) recovers deformation thereof to push the clamping ball (1294) into the clamping hole (1292) to limit the output shaft of the motor II (128), further to accurately control a rotation position of the sealing ball (123) and finally cause lubricating oil to flow through the flow guide pipe (121) into the hydraulic press (4), so that the lubricating oil is in contact with the telescopic end of the hydraulic cylinder (8) to lubricate the hydraulic cylinder (8); and
step five: then putting the natural fiber substrate into the open-type oil heating mold (3) again, taking out the mixed fiber felt in the soft state and putting the mixed fiber felt into the lower mold (7), keeping the mixed fiber felt in the lower mold (7) under a pressure of 315-500 T from the hydraulic press (4) for 8-10 seconds, taking out a molded natural fiber core material for later use, passing two plate sheets through the single-sided roller gluing machine (5) for gluing for later use, putting the core material between the two plate sheets, putting the core material and the two plate sheets in the cold press (6) for laminating for 1-2 minutes, and taking out a molded natural fiber plate.