# US 2025/0043034 A1 · Processes for Making Polyolefins with Composition Control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0043034 A1
- Document ID: US20250043034A1
- Status: Published application
- Kind: A1
- Application number: 18/717,173
- Filed: 2022-12-14
- Published: 2025-02-06
- Earliest claimed: 2021-12-17
- Applicants: ExxonMobil Technology and Engineering Company
- Inventors: Giriprasath Gururajan; Rong Ma; Narayanaswami Dharmarajan; Jean-Roch Schauder
- Web page: https://patentgrep.com/patent/US20250043034A1

## CPC

- C08F 2/01: characterised by special features of the polymerisation apparatus used
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/659: Component covered by group C08F4/64 containing a transition metal-carbon bond {(C08F4/64003 - C08F4/64196 take precedence)}
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F 2500/06: Comonomer distribution, e.g. normal, reverse or narrow
- C08F 2500/08: Low density, i.e. < 0.91 g/cm3
- C08F 2500/09: Long chain branches
- C08F 2500/12: Melt flow index or melt flow ratio
- C08F 2500/27: Amount of comonomer in wt% or mol%
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Processes for making olefin copolymers, particularly ethylene-based copolymers. A process for making an olefin copolymer can include introducing an olefin monomer, at least one other olefin comonomer, and a single type of catalyst system to a tubular reactor to produce an olefin copolymer containing: a) an absolute comonomer distribution (CD) slope 90 of about 2.0 to about 30.0, an absolute CD slope 75 of about 2.0 to about 30.0, an absolute CD slope 50 of about 2.0 to about 30.0, or an absolute CD slope 25 of about 2.0 to about 30.0; b) a first long chain branching index (g′(Mz)) of about 0.30 to about 1.0; and c) a second long chain branching index (g′(Mz+1)) of about 0.30 to about 1.0. The tubular reactor can include one or more plug flow components, one or more spiral heat exchangers, and/or a recycle pump.

## Claims

### Claim 1

A process for making an olefin copolymer, comprising:
introducing an olefin monomer, at least one other olefin comonomer, and a single type of catalyst system to a tubular reactor to produce an olefin copolymer comprising:
a) an absolute comonomer distribution (CD) slope 90 of about 2.0 to about 30.0, an absolute CD slope 75 of about 2.0 to about 30.0, an absolute CD slope 50 of about 2.0 to about 30.0, or an absolute CD slope 25 of about 2.0 to about 30.0;
b) a first long chain branching index (g′(Mz)) of about 0.30 to about 1.0; and
c) a second long chain branching index (g′(Mz+1)) of about 0.30 to about 1.0.

### Claim 2 (depends on 1)

The process of claim 1, wherein an absolute average of CD slope 50 and CD slope 75, an absolute average of CD slope 25 and CD slope 50, or an absolute average of CD slope 75 and CD slope 90 is about 1.5 to about 12.0 when MZ/MW is about 1.8 to 6.0.

### Claim 3 (depends on 1)

The process of claim 1, wherein the tubular reactor comprises a recycle pump.

### Claim 4 (depends on 1)

The process of claim 1, wherein the tubular reactor comprises a spiral heat exchanger.

### Claim 5 (depends on 1)

The process of claim 1, wherein the catalyst system includes a metallocene catalyst comprising a Group 4 organometallic compound comprising two ancillary monanionic ligands, each of which is independently substituted or unsubstituted, wherein the ligands are bonded by a covalent bridge comprising a substituted single Group 14 atom, the substitution on said Group 14 atom comprising aryl groups, at least one of which comprises at least one hydrocarbylsilyl substituent group.

### Claim 6 (depends on 5)

The process of claim 5, wherein the hydrocarbylsilyl substituent has the formula Rn″SiR′3-n, wherein each R′ is independently a Ct-C20 hydrocarbyl, hydrocarbylsilyl, hydrofluorocarbyl substituent, R″ is a Ct-C10 linking group between Si and the aryl group, and n=0 or 1.

### Claim 7 (depends on 1)

The process of claim 1, wherein the olefin monomer and the at least one other olefin comonomer are copolymerized using a continuous solution polymerization process.

### Claim 8 (depends on 1)

The process of claim 1, further comprising introducing hydrogen to the reactor, wherein the olefin monomer is ethylene, and wherein the at least one other olefin comonomer comprises at least one C4 to C20 olefin.

### Claim 9 (depends on 8)

The process of claim 8, further comprising: calculating a weight average molecular weight (Mw) of the olefin copolymer using the following equation: (Mw)2.2=−2.1E+011+1.5E+9*T avg−2.7E+8*H2/C2+4.1E+10*C2 conc+3.4E+011*C8 conc−1.8E+9*T avg*C8 conc−1.9E+010*C2 conc*C8 conc, wherein Tavg is average reactor temperature, H2/C2 is a molar ratio of the hydrogen to the ethylene introduced to the reactor, C2 conc is the ethylene concentration in wt %, and C8 conc is the at least one other comonomer concentration in wt %, all weight percentages being based on the total weight of the solution introduced to the reactor; and controlling the Mw based on the calculated Mw.

### Claim 10 (depends on 8)

The process of claim 8, further comprising: calculating the CD slope 90 using the following equation: Sqrt(Slope 90)=+0.11−7.6E-003*H2/C2+0.5*C2 conc−0.2*C8 conc+0.20*Cement conc, wherein Tavg is average reactor temperature, H2/C2 is a molar ratio of the hydrogen to the ethylene introduced to the reactor, C2 conc is the ethylene concentration in wt %, C8 conc is the at least one other comonomer concentration in wt %, and Cement conc is cement concentration in wt %, all weight percentages being based on the total weight of the solution introduced to the reactor; and controlling the comonomer distribution based on the calculated CD slope 90.

### Claim 11 (depends on 8)

The process of claim 8, further comprising: calculating the CD slope 75 using the following equation: Sqrt(Slope 75)=+2.6-0.011*T avg−5.7E-003*H2/C2+0.13*C2 conc−0.06*C8 conc+0.10*Cement Conc, wherein Tavg is average reactor temperature, H2/C2 is a molar ratio of the hydrogen to the ethylene introduced to the reactor, C2 conc is the ethylene concentration in wt %, C8 conc is the at least one other comonomer concentration in wt %, and Cement conc is cement concentration in wt %, all weight percentages being based on the total weight of the solution introduced to the reactor; and controlling the comonomer distribution based on the calculated CD slope 75.

### Claim 12 (depends on 8)

The process of claim 8, further comprising: calculating the first long chain branching index using the following equation: g′-Mz=+0.89+1.47E-004*H2/C2+0.02*C2 conc−2.8E-003*C8 conc−2.8E-005*PRPM, wherein H2/C2 is a molar ratio of the hydrogen to the ethylene introduced to the reactor, C2 conc is the ethylene concentration in wt,%, C8 conc is the at least one other comonomer concentration in wt %, and PRPM is the pump speed in the reactor, all weight percentages being based on the total weight of the solution introduced to the reactor; and controlling the first long chain branching index based on the calculated first long chain branching index.

### Claim 13 (depends on 3)

The process of claim 3, wherein the olefin copolymer is produced at a cement concentration of about 2 wt % and to about 40 wt % and at a recycle ratio of about 3 to about 50.

### Claim 14 (depends on 1)

The process of claim 1, wherein the olefin copolymer has a MWD of about 2.0 to about 7.0.

### Claim 15 (depends on 1)

The process of claim 1, wherein the olefin copolymer has a melt index of about 0.1 dg/min to about 500.0 dg/min, as measured according to ASTM D1238 (190° C./2.16 kg).

### Claim 16 (depends on 1)

The process of claim 1, wherein the olefin copolymer has a melt index ratio (MI21.6/MI2.16) of about 20.0 to about 100.0, as measured according to ASTM D1238.

### Claim 17 (depends on 1)

The process of claim 1, wherein the olefin copolymer has a density of about 0.850 g/cc to about 0.920 g/cc, as measured according to ASTM D792.

### Claim 18 (depends on 1)

The process of claim 1, wherein the first long chain branching index is about 0.70 to about 0.97, and wherein the second long chain branching index is about 0.70 to about 0.97.