# US 2025/0042819 A1 · Zirconia sintered body, zirconia powder, and method for producing zirconia sintered body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0042819 A1
- Document ID: US20250042819A1
- Status: Published application
- Kind: A1
- Application number: 18/717,261
- Filed: 2023-03-03
- Published: 2025-02-06
- Earliest claimed: 2022-03-11
- Assignees: Daiichi Kigenso Kagaku Kogyo Co., Ltd.
- Applicants: Daiichi Kigenso Kagaku Kogyo Co., Ltd.
- Inventors: Keisuke FUJITA; Masayuki TAKAI
- Web page: https://patentgrep.com/patent/US20250042819A1

## CPC

- C04B 35/486: Fine ceramics
- C01G 25/02: Oxides
- C01G 25/06: Sulfates
- C04B 35/4885: {with aluminium oxide}
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/62685: {characterised by the order of addition of constituents or additives}
- C04B 35/6455: {Hot isostatic pressing}
- C01P 2002/52: containing elements as dopants
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/12: Surface area
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3213: Strontium oxides or oxide-forming salts thereof
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3227: Lanthanum oxide or oxide-forming salts thereof
- C04B 2235/3246: Stabilised zirconias, e.g. YSZ or cerium stabilised zirconia
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/6567: Treatment time
- C04B 2235/668: Pressureless sintering
- C04B 2235/765: Tetragonal symmetry
- C04B 2235/77: Density
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B 2235/9669: Resistance against chemicals, e.g. against molten glass or molten salts
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Disclosed herein is a zirconia sintered body containing stabilized zirconia containing zirconia and a stabilizer, wherein the stabilizer contains an oxide of yttrium and an oxide of M, the M is at least one selected from the group consisting of Ca, Ba, Sr, Dy, Tb, Gd, Eu, Sm, Nd, Pr, and La, a content of the stabilizer in the stabilized zirconia is 1.7 mol % or more and 2.6 mol % or less in terms of oxide, a molar ratio between the oxide of M and the oxide of yttrium [(oxide of M)/(oxide of yttrium)] is 0.05 or more and 1.5 or less, and a crystal grain diameter is 0.20 μm or less.

## Claims

### Claim 1

A zirconia sintered body comprising stabilized zirconia containing zirconia and a stabilizer, wherein
the stabilizer contains an oxide of yttrium and an oxide of M,
the M is at least one selected from the group consisting of Ca, Ba, Sr, Dy, Tb, Gd, Eu, Sm, Nd, Pr, and La,
a content of the stabilizer in the stabilized zirconia is 1.7 mol % or more and 2.6 mol % or less in terms of oxide,
a molar ratio between the oxide of M and the oxide of yttrium [(oxide of M)/(oxide of yttrium)] is 0.05 or more and 1.5 or less, and
a crystal grain diameter is 0.20 μm or less.

### Claim 2 (depends on 1)

The zirconia sintered body according to claim 1, wherein the M is at least one selected from the group consisting of Ca, Dy, Tb, Nd, and La.

### Claim 3 (depends on 1)

The zirconia sintered body according to claim 1, wherein a content of the oxide of M in the stabilized zirconia is 0.1 mol % or more and 1.3 mol % or less.

### Claim 4 (depends on 1)

The zirconia sintered body according to claim 1, wherein a ratio of a tetragonal fraction after thermal treatment at 300° C. for 1 hour relative to a tetragonal fraction before thermal treatment is 70% or more.

### Claim 5 (depends on 1)

The zirconia sintered body according to claim 1, wherein a ratio of a tetragonal fraction after hydrothermal treatment at 134° C. and 3 atmospheres for 40 hours relative to a tetragonal fraction before hydrothermal treatment is 70% or more.

### Claim 6 (depends on 1)

The zirconia sintered body according to claim 1, which has a toughness value of 5 MPa·m0.5 or more as measured by IF method.

### Claim 7 (depends on 1)

The zirconia sintered body according to claim 1, which has a three-point bending strength of 80 kgf/mm2 or more and 150 kgf/mm2 or less.

### Claim 8

A zirconia powder comprising
stabilized zirconia containing zirconia and a stabilizer, wherein
the stabilizer contains an oxide of yttrium and an oxide of M,
the M is at least one selected from the group consisting of Ca, Ba, Sr, Dy, Tb, Gd, Eu, Sm, Nd, Pr, and La,
a content of the stabilizer in the stabilized zirconia is 1.7 mol % or more and 2.6 mol % or less in terms of oxide, and
a molar ratio between the oxide of M and the oxide of yttrium [(oxide of M)/(oxide of yttrium)] is 0.05 or more and 1.5 or less.

### Claim 9 (depends on 8)

The zirconia powder according to claim 8, wherein the M is at least one selected from the group consisting of Ca, Dy, Tb, Nd, and La.

### Claim 10 (depends on 8)

The zirconia powder according to claim 8, wherein a content of the oxide of M is 0.1 mol % or more and 1.3 mol % or less relative to an entire amount of the stabilized zirconia.

### Claim 11 (depends on 8)

The zirconia powder according to claim 8, which has a specific surface area of 15 m2/g or more and 50 m2/g or less.

### Claim 12 (depends on 8)

The zirconia powder according to claim 8, which has a particle diameter D50 of 0.1 μm or more and less than 1.0 μm.

### Claim 13 (depends on 8)

The zirconia powder according to claim 8, which has the following <Characteristic 1> when molded at a molding pressure of 2 t/cm2 by cold isostatic pressing and then heated at 1250° C. for 2 hours:
<Characteristic 1>
a ratio of a tetragonal fraction after thermal treatment at 300° C. for 1 hour relative to a tetragonal fraction before thermal treatment is 70% or more.

### Claim 14 (depends on 8)

The zirconia powder according to claim 8, which has the following <Characteristic 2> when molded at a molding pressure of 2 t/cm2 by cold isostatic pressing and then heated at 1250° C. for 2 hours:
<Characteristic 2>
a ratio of a tetragonal fraction after hydrothermal treatment at 134° C. and 3 atmospheres for 40 hours relative to a tetragonal fraction before hydrothermal treatment is 70% or more.

### Claim 15 (depends on 8)

The zirconia powder according to claim 8, which has the following <Characteristic 3> when molded at a molding pressure of 2 t/cm2 by cold isostatic pressing and then heated at 1250° C. for 2 hours:
<Characteristic 3>
a toughness value as measured by IF method is 5 MPa·m0.5 or more.

### Claim 16 (depends on 8)

The zirconia powder according to claim 8, which has the following <Characteristic 4> when molded at a molding pressure of 2 t/cm2 by cold isostatic pressing and then heated at 1250° C. for 2 hours:
<Characteristic 4>
a three-point bending strength is 80 kgf/mm2 or more and 150 kgf/mm2 or less.

### Claim 17 (depends on 8)

A method for producing a zirconia sintered body, the method comprising:
step X in which the zirconia powder according to claim 8 is molded to obtain a molded body; and
step Y in which after step X, the molded body is sintered under conditions of 1200° C. or higher and 1350° C. or lower and 1 hour or more and 5 hours or less.