# US 2025/0041936 A1 · Silver powder, method of producing silver powder, and conductive paste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0041936 A1
- Document ID: US20250041936A1
- Status: Published application
- Kind: A1
- Application number: 18/715,737
- Filed: 2022-12-02
- Published: 2025-02-06
- Earliest claimed: 2021-12-06
- Assignees: Dowa Electronics Materials Co., Ltd.
- Applicants: DOWA Electronics Materials Co., Ltd.
- Inventors: Taro TORIGOE; Hiroaki KOUBU; Fumiya ABE; Minami KANASUGI
- Web page: https://patentgrep.com/patent/US20250041936A1

## CPC

- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- H01B 5/00: Non-insulated conductors or conductive bodies characterised by their form
- B22F 1/065: Spherical particles
- B22F 1/068: Flake-like particles
- B22F 1/10: Metallic powder containing lubricating or binding agents; Metallic powder containing organic material
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- B22F 1/14: Treatment of metallic powder (mixing with lubricating or binding agents or with organic material B22F1/10)
- B22F 1/145: Chemical treatment, e.g. passivation or decarburisation
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- C22C 1/0466: {Alloys based on noble metals}
- H01B 1/00: Conductors or conductive bodies characterised by the conductive materials; Selection of materials as conductors
- H01B 1/22: the conductive material comprising metals or alloys
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- B22F 1/09: {Mixtures of metallic powders}
- B22F 2009/042: {using a particular milling fluid}
- B22F 2009/043: {by ball milling}
- B22F 2301/255: Silver or gold
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided are a silver powder that can reduce line resistance and a method of producing the same. The silver powder has a diameter at a cumulative value of 50% of 3 μm or more and a ratio of particles of 10 μm or larger of 10% or less. The silver powder includes flake-like particles having a major axis of 6 μm or more and irregularly shaped particles having a major axis of less than 6 μm, an average aspect ratio that is a ratio of average major axis relative to average thickness of the flake-like particles is 8 or more, and a shape factor that is a ratio of area of a circle having average maximum length of the irregularly shaped particles as a diameter relative to average particle area of the irregularly shaped particles is 1.7 to 1.9. Ignition loss is 0.1 wt % to 0.4 wt %.

## Claims

### Claim at position 1

1-9. (canceled)

### Claim 10

A silver powder that in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument, has a diameter at a cumulative value of 50% of 3 μm or more and a ratio of particles of 10 μm or larger of 10% or less, wherein
with regards to particle shape observed by image analysis based on an SEM image,
the silver powder includes flake-like particles having a major axis of 6 μm or more and irregularly shaped particles having a major axis of less than 6 μm,
an average aspect ratio that is a ratio of an average major axis of the flake-like particles relative to an average thickness of the flake-like particles is 8 or more, and
a shape factor that is a ratio of an area of a circle having an average maximum length of the irregularly shaped particles as a diameter relative to an average particle area of the irregularly shaped particles is not less than 1.7 and not more than 1.9, and
the silver powder has an ignition loss of not less than 0.1 wt % and not more than 0.4 wt %.

### Claim 11 (depends on 10)

The silver powder according to claim 10, wherein, in the particle size distribution, a ratio of a value of a difference determined by subtracting a diameter at a cumulative value of 10% from a diameter at a cumulative value of 90% relative to the diameter at the cumulative value of 50% is 2 or more.

### Claim 12

A method of producing a silver powder comprising:
a reduction step of adding a reductant to a silver ammine complex aqueous solution to obtain a first liquid;
a surface treatment agent addition step of adding a surface treatment agent to the first liquid to obtain a second liquid;
a separation step of obtaining a first silver powder through separation from the second liquid and drying; and
a flaking step of stirring the first powder, a lubricant, and media inside of a vessel to obtain a second silver powder in which the first silver powder has undergone flattening, wherein
an additive amount of the surface treatment agent in the surface treatment agent addition step is not less than 0.05 wt % and not more than 0.15 wt % relative to weight of silver contained in the silver ammine complex aqueous solution,
a specific surface area diameter calculated from specific surface area determined by the BET method after the first silver powder is mixed with the lubricant is not less than 1.3 μm and not more than 2.0 μm,
a diameter at a cumulative value of 50% in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument after the first silver powder is mixed with the lubricant is not less than 1.5 times and not more than 3 times the specific surface area diameter, and
an additive amount of the lubricant in the flaking step and the additive amount of the surface treatment agent are, in total, not less than 0.1 wt % and not more than 0.4 wt % relative to weight of silver in the first silver powder.

### Claim 13 (depends on 12)

The method of producing a silver powder according to claim 12, wherein
with regards to particle shape of the second silver powder observed by image analysis based on an SEM image, a number of flake-like particles having a major axis that is not less than 4 times the specific surface area diameter of the first silver powder is not less than 1% and not more than 13% of a total number of particles serving as subjects in the image analysis, and
in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument, the second silver powder has a diameter at a cumulative value of 50% of 3 μm or more and a ratio of particles of 10 μm or larger of 10% or less.

### Claim 14 (depends on 12)

The method of producing a silver powder according to claim 12, wherein the additive amount of the lubricant is not less than 0.05 wt % and not more than 0.3 wt % relative to weight of the first silver powder.

### Claim 15 (depends on 12)

The method of producing a silver powder according to claim 12, wherein, in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument after the first silver powder is mixed with the lubricant, a ratio of particles of 10 μm or larger is 10% or less.

### Claim 16

A method of producing a silver powder comprising a flaking step of stirring a first silver powder that is coated with a surface treatment agent, a lubricant, and media inside of a vessel to obtain a second silver powder in which the first silver powder has undergone flattening, wherein
a specific surface area diameter calculated from specific surface area determined by the BET method after the first silver powder is mixed with the lubricant is not less than 1.3 μm and not more than 2.0 μm,
a diameter at a cumulative value of 50% in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument after the first silver powder is mixed with the lubricant is not less than 1.5 times and not more than 3 times the specific surface area diameter, and
an additive amount of the lubricant in the flaking step and an attached amount of the surface treatment agent are, in total, not less than 0.1 wt % and not more than 0.4 wt % relative to weight of silver in the first silver powder.

### Claim 17 (depends on 16)

The method of producing a silver powder according to claim 16, wherein
with regards to particle shape of the second silver powder observed by image analysis based on an SEM image, a number of flake-like particles having a major axis that is not less than 4 times the specific surface area diameter of the first silver powder is not less than 1% and not more than 13% of a total number of particles serving as subjects in the image analysis, and
in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument, the second silver powder has a diameter at a cumulative value of 50% of 3 μm or more and a ratio of particles of 10 μm or larger of 10% or less.

### Claim 18 (depends on 16)

The method of producing a silver powder according to claim 16, wherein the additive amount of the lubricant is not less than 0.05 wt % and not more than 0.3 wt % relative to weight of the first silver powder.

### Claim 19 (depends on 16)

The method of producing a silver powder according to claim 16, wherein, in a volume-based particle size distribution measured using a laser diffraction/scattering particle size distribution measurement instrument after the first silver powder is mixed with the lubricant, a ratio of particles of 10 μm or larger is 10% or less.

### Claim 20 (depends on 10)

A conductive paste comprising: the silver powder according to claim 10; a resin; and a solvent.

### Claim 21 (depends on 20)

The conductive paste according to claim 20, further comprising a spherical silver powder.

### Claim 22 (depends on 11)

A conductive paste comprising: the silver powder according to claim 11; a resin; and a solvent.

### Claim 23 (depends on 22)

The conductive paste according to claim 22, further comprising a spherical silver powder.