# US 2025/0031399 A1 · Barrier layers in semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0031399 A1
- Document ID: US20250031399A1
- Status: Published application
- Kind: A1
- Application number: 18/353,976
- Filed: 2023-07-18
- Published: 2025-01-23
- Earliest claimed: 2023-07-18
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Mu-Min Hung; Fan Hsuan Chien; Jyh-Nan Lin; Kai-Shiung Hsu; Tzu-Chien Cheng; Su-Yu Yeh
- Web page: https://patentgrep.com/patent/US20250031399A1

## CPC

- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/501: {FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 30/014: {of FETs having zero-dimensional [0D] or one-dimensional [1D] channels, e.g. quantum wire FETs, single-electron transistors [SET] or Coulomb blockade transistors}
- H10D 30/019: {of FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 30/43: having one-dimensional [1D] charge carrier gas channels, e.g. quantum wire FETs or transistors having 1D quantum-confined channels
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 30/6735: {having gates fully surrounding the channels, e.g. gate-all-around}
- H10D 30/6757: {characterised by the structure of the channel, e.g. transverse or longitudinal shape or doping profile (TFTs having channel structures for preventing kink or snapback effects H10D30/6708; TFTs having lightly-doped source or drain extensions H10D30/6715)}
- H10D 62/116: {adjoining the input or output regions of field-effect devices, e.g. adjoining source or drain regions}
- H10D 62/121: {oriented parallel to substrates}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A semiconductor device with a barrier layer between a gate structure and gate spacer layers, and a method of fabricating the same are disclosed. The a method includes forming a fin structure on a substrate, forming a polysilicon structure on the fin structure, performing a nitridation operation to form a barrier layer on the polysilicon structure and the fin structure, forming gate spacer layers on the barrier layer, forming a source/drain region in the fin structure and adjacent to the barrier layer, annealing the gate spacer layers, and replacing the polysilicon structure with a gate structure.

## Claims

### Claim 1

A method, comprising:
forming a fin structure on a substrate;
forming a polysilicon structure on the fin structure;
performing a nitridation process to form a nitride layer on sidewalls of the polysilicon structure;
forming a gate spacer on the nitride layer;
forming a source/drain region adjacent to the nitride layer and the polysilicon structure;
performing an annealing process to densify the gate spacer; and
replacing the polysilicon structure with a gate structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein performing the nitridation process comprises exposing the polysilicon structure to a nitrogen plasma.

### Claim 3 (depends on 1)

The method of claim 1, wherein performing the nitridation process comprises controlling parameters of the nitridation process to form the nitride layer with a thickness of about 2 Å to about 5 Å.

### Claim 4 (depends on 1)

The method of claim 1, wherein performing the nitridation process comprises exposing the polysilicon structure to a nitrogen plasma for a duration of about 1 sec to about 5 sec.

### Claim 5 (depends on 1)

The method of claim 1, wherein performing the nitridation process comprises forming a hydrogen-free silicon nitride layer on the sidewalls of the polysilicon structure.

### Claim 6 (depends on 1)

The method of claim 1, further comprising forming a thermal oxide layer on the fin structure, wherein performing the nitridation process comprises forming a portion of the nitride layer on a surface of the thermal oxide layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein performing the nitridation process comprises forming a horizontal portion of the nitride layer with a first thickness and a vertical portion of the nitride layer with a second thickness greater than the first thickness.

### Claim 8 (depends on 1)

The method of claim 1, wherein replacing the polysilicon structure with the gate structure comprises forming a high-k gate dielectric layer of the gate structure on a top surface and a sidewall of the nitride layer.

### Claim 9

A method, comprising:
forming a polysilicon structure on a substrate;
performing a nitridation process to form a barrier layer on the polysilicon structure;
forming a gate spacer on the barrier layer;
forming a source/drain region adjacent to the barrier layer;
performing an annealing process to densify the gate spacer;
adjusting a height of the barrier layer; and
replacing the polysilicon structure with a gate structure.

### Claim 10 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises exposing the polysilicon structure to a nitrogen plasma.

### Claim 11 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises forming the barrier layer with a thickness of about 2 Å to about 5 Å.

### Claim 12 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises exposing the polysilicon structure to a nitrogen plasma for a duration of about 1 sec to about 5 sec.

### Claim 13 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises forming a hydrogen-free silicon nitride layer on the polysilicon structure.

### Claim 14 (depends on 9)

The method of claim 9, wherein adjusting the height of the barrier layer comprises:
removing an upper portion of the polysilicon structure;
etching the barrier layer using a lower portion of the polysilicon structure as a masking layer.

### Claim 15 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises forming a horizontal portion of the barrier layer with a first thickness and a vertical portion of the barrier layer with a second thickness greater than the first thickness.

### Claim 16 (depends on 9)

The method of claim 9, wherein performing the nitridation process comprises forming the barrier layer with an L-shaped cross-sectional profile.

### Claim 17

A device, comprising:
a substrate;
a fin structure disposed on the substrate;
a gate structure disposed on the fin structure;
a hydrogen free nitride layer disposed on the fin structure and sidewalls of the gate structure;
a gate spacer layer on the hydrogen free nitride layer; and
a source/drain region disposed on the fin structure and adjacent to the hydrogen free nitride layer.

### Claim 18 (depends on 17)

The device of claim 17, wherein the hydrogen free nitride layer comprises a vertical portion on sidewalls of the gate structure and horizontal a portion on the fin structure, and wherein a thickness of the vertical portion is greater than a thickness of the horizontal portion by at least 10%.

### Claim 19 (depends on 17)

The device of claim 17, wherein a height of the hydrogen free nitride layer is substantially the same as a height of the gate spacer.

### Claim 20 (depends on 17)

The device of claim 17, wherein a ratio between a height of the hydrogen free nitride layer and a height of the gate spacer layer is between about 30% and about 50%.