# US 2025/0027223 A1 · Electrodeposition of molybdenum disulfide dry film lubricant coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0027223 A1
- Document ID: US20250027223A1
- Status: Published application
- Kind: A1
- Application number: 18/354,298
- Filed: 2023-07-18
- Published: 2025-01-23
- Earliest claimed: 2023-07-18
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Adam Paul Rabe; Jacob Alexander Rabe; Matthew G. Keast; Zhe Li
- Web page: https://patentgrep.com/patent/US20250027223A1

## CPC

- C25D 9/06: by anodic processes
- C25D 7/10: Bearings
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method of forming a lubricant coating, a method of coating a bearing surface with a lubricant coating, and a vehicle including a bearing including a lubricant coating. A substrate, such as a bearing, including a surface and an electrode are immersed in an electrolyte bath. The electrolyte bath includes an aqueous electrolyte solution including sodium metabisulfite (Na2S2O5), sodium molybdate (Na2MoO4·2H2O), a pH modifier, an anionic surfactant, and water. A first pulsed direct current is applied through the aqueous electrolyte solution using a direct current power supply and a molybdenum disulfide (MoS2) layer is formed on the surface of the substrate.

## Claims

### Claim 1

A method of forming a lubricant coating, comprising:
immersing a substrate including a surface and an electrode in an electrolyte bath, wherein the electrolyte bath includes an aqueous electrolyte solution including sodium metabisulfite (Na2S2O5), sodium molybdate (Na2MoO4·2H2O), a pH modifier, an anionic surfactant, and water;
applying a first pulsed direct current through the aqueous electrolyte solution using a direct current power supply, wherein the polarity of the first pulsed direct current causes the substrate to provide an anode and the electrode to provide a cathode; and
forming a molybdenum disulfide (MoS2) layer on the surface of the substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising applying the first pulsed direct current at a peak current density in the range of 5 milliamps per square centimeter (mA/cm{circumflex over ( )}2) to 50 mA/cm{circumflex over ( )}2 for a time period of 5 minutes to twenty minutes, wherein the pulses cycle in the range of 1 second to 4 second and have a duty cycle in the range of 25 percent to 50 percent of the cycle.

### Claim 3 (depends on 2)

The method of claim 2, further comprising preparing the aqueous electrolyte solution by combining the sodium metabisulfite (Na2S2O5) in the range of 5 percent and 15 percent by weight of the total weight of the aqueous electrolyte solution, the sodium molybdate (Na2MoO4·2H2O) in the range of 3 percent and 10 percent by weight of the total weight of the aqueous electrolyte solution, the pH modifier, and the anionic surfactant with the water.

### Claim 4 (depends on 3)

The method of claim 3, further comprising combining the pH modifier to the aqueous electrolyte solution and adjusting the pH of the aqueous electrolyte solution to a pH in the range of 4.0 to 7.0.

### Claim 5 (depends on 4)

The method of claim 4, further comprising combining citric acid as the pH modifier.

### Claim 6 (depends on 5)

The method of claim 5, further comprising combining the anionic surfactant in the range of 5 percent and 15 percent by weight of the total weight of the aqueous electrolyte solution.

### Claim 7 (depends on 2)

The method of claim 2, further comprising applying a second pulsed direct current through the aqueous electrolyte solution, wherein the polarity causes electrode to provide the anode and the substrate to provide the cathode; and forming a black oxide (Fe3O4) layer on the surface of the substrate prior to applying the first pulsed direct current.

### Claim 8 (depends on 7)

The method of claim 7, wherein applying the second pulsed direct current comprises applying the second pulsed direct current at a peak current density in the range of 5 milliamps per square centimeter (mA/cm{circumflex over ( )}2) to 25 mA/cm{circumflex over ( )}2 for a time period of one minute to five minutes, wherein the pulses cycle in the range of 1 second to 4 seconds and have a duty cycle in the range of 25 percent to 50 percent of the cycle.

### Claim 9 (depends on 8)

The method of claim 8, wherein the molybdenum disulfide (MoS2) layer is in the range of 0.01 micrometer and 4 micrometers in thickness and the black oxide (Fe3O4) layer is in the range of 0.1 micrometer to 3 micrometers in thickness.

### Claim 10 (depends on 1)

The method of claim 1, further comprising preparing the aqueous electrolyte solution by combining the sodium metabisulfite (Na2S2O5) present in the range of 8 and 12 percent by weight of the total weight of the aqueous electrolyte solution, the sodium molybdate (Na2MoO4·2H2O) present in the range of 3 percent and 7 percent by weight of the total weight of the aqueous electrolyte solution, citric acid as the pH modifier present in the range of 1 percent and 3 percent by weight of the total weight of the aqueous electrolyte solution, TEEPOL 601 S as the anionic surfactant present in the range of 8 percent and 12 percent by weight of the total weight of the solution, and the water.

### Claim 11 (depends on 1)

The method of claim 1, wherein immersing the substrate comprises immersing at least one surface of a bearing.

### Claim 12 (depends on 11)

The method of claim 11, wherein the bearing is a ball bearing.

### Claim 13 (depends on 11)

The method of claim 11, wherein the bearing is a journal bearing.

### Claim 14

A method of coating a bearing surface with a lubricant coating, comprising:
immersing a bearing including a surface and an electrode in an electrolyte bath, wherein the electrolyte bath includes an aqueous electrolyte solution including sodium metabisulfite (Na2S2O5), sodium molybdate (Na2MoO4·2H2O), a pH modifier, an anionic surfactant, and water;
applying a first pulsed direct current through the aqueous electrolyte solution using a direct current power supply, wherein the polarity of the current causes the bearing to provide an anode and the electrode to provide a cathode; and
forming a molybdenum disulfide (MoS2) layer on the surface of the bearing.

### Claim 15 (depends on 14)

The method of claim 14, further comprising applying the first pulsed direct current at a peak current density in the range of 5 milliamps per square centimeter (mA/cm{circumflex over ( )}2) to 50 mA/cm{circumflex over ( )}2 for a time period of 5 minutes to twenty minutes, wherein the pulses cycle in the range of 1 second to 4 second and have a duty cycle in the range of 25 percent to 50 percent of the cycle.

### Claim 16 (depends on 14)

The method of claim 14, further comprising applying a second pulsed direct current through the aqueous electrolyte solution, wherein the polarity causes electrode to provide the anode and the bearing to provide the cathode; and forming a black oxide (Fe3O4) layer on the surface of the bearing prior to applying the first pulsed direct current.

### Claim 17 (depends on 16)

The method of claim 16, wherein applying the second pulsed direct current comprises applying the second pulsed direct current at a peak current density in the range of 5 milliamps per square centimeter (mA/cm{circumflex over ( )}2) to 25 mA/cm{circumflex over ( )}2 for a time period of 1 minute to five minutes, wherein the pulses cycle in the range of 1 second to 4 seconds and have a duty cycle in the range of 25 percent to 50 percent of the cycle.

### Claim 18 (depends on 14)

The method of claim 14, further comprising preparing the aqueous electrolyte solution by combining the sodium metabisulfite (Na2S2O5) present in the range of 5 percent and 15 percent by weight of the total weight of the aqueous electrolyte solution, the sodium molybdate (Na2MoO4·2H2O) present in the range of 3 percent and 10 percent by weight of the total weight of the aqueous electrolyte solution, citric acid as the pH modifier present in the range of 1 percent and 3 percent by weight of the total weight of the aqueous electrolyte solution, TEEPOL 601 S as the anionic surfactant present in the range of 5 percent and 15 percent by weight of the total weight of the solution, and the water.

### Claim 19

A vehicle comprising:
an electric drive unit including a battery, a power electronic module connected to the battery, an electric motor connected to the power electronic module, and a transmission connected to the electric motor;
an inverter included in the power electronic module;
a motor shaft connected to the electric motor;
a bearing rotatably supporting the motor shaft, wherein the bearing includes a surface; and
a coating including a molybdenum disulfide (MoS2) layer disposed on the surface, wherein the molybdenum disulfide (MoS2) layer is in the range of 0.1 micrometer and 4 micrometers in thickness.

### Claim 20 (depends on 19)

The vehicle of claim 19, wherein the coating further comprises a black oxide (Fe3O4) layer contacting the surface of the bearing and the molybdenum disulfide (MoS2) layer contacts the black oxide (Fe3O4) layer, wherein the black oxide (Fe3O4) layer is in the range of 0.1 micrometers to 3 micrometers in thickness.