# US 2025/0027218 A1 · Diamond laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0027218 A1
- Document ID: US20250027218A1
- Status: Published application
- Kind: A1
- Application number: 18/707,496
- Filed: 2022-11-02
- Published: 2025-01-23
- Earliest claimed: 2021-11-05
- Assignees: Daicel Corporation; National University Corporation Kanazawa University
- Applicants: Daicel Corporation; National University Corporation Kanazawa University
- Inventors: Norio TOKUDA; Satoshi YAMASAKI; Hitoshi ASAKAWA; Tsubasa MATSUMOTO; Shinji NAGAMATSU; Tatsuya NAKANO; Taro YOSHIKAWA
- Web page: https://patentgrep.com/patent/US20250027218A1

## CPC

- C01B 32/25: Diamond
- C25B 11/043: Carbon, e.g. diamond or graphene
- C01B 32/40: Carbon monoxide
- C25B 9/50: Cells or assemblies of cells comprising photoelectrodes; Assemblies of constructional parts thereof
- C25B 11/052: Electrodes comprising one or more electrocatalytic coatings on a substrate
- C25B 11/065: Carbon
- C25B 11/083: Diamond
- C25B 11/087: Photocatalytic compound
- C25B 1/23: Carbon monoxide or syngas
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

Provided is a diamond laminate that exhibits an excellent electron emission capability and can form an electrode reaction field with an excellent reducing property. The laminate of the present disclosure includes an electron excitation layer (1) having a diamond crystal structure in which some carbon atoms are substituted with nitrogen atoms, and a conductive layer (2) having a diamond crystal structure in which some carbon atoms are substituted with boron atoms. The nitrogen atom concentration in the layer (1) is preferably 5×1018 atoms/cm3 or greater, and the boron atom concentration in the layer (2) is preferably 1×1019 atoms/cm3 or greater. The thickness of the layer (1) is preferably from 1 nm to 100 μm, and the thickness of the layer (2) is preferably 1 μm or greater.

## Claims

### Claim 1

A laminate comprising:
an electron excitation layer (1) having a diamond crystal structure in which some carbon atoms are substituted with nitrogen atoms; and
a conductive layer (2) having a diamond crystal structure in which some carbon atoms are substituted with boron atoms.

### Claim 2 (depends on 1)

The laminate according to claim 1, wherein a nitrogen atom concentration in the electron excitation layer (1) is 5×1018 atoms/cm3 or greater, and a boron atom concentration in the conductive layer (2) is 1×1019 atoms/cm3 or greater.

### Claim 3 (depends on 1)

The laminate according to claim 1, wherein the electron excitation layer (1) has a thickness from 1 nm to 100 μm, and the conductive layer (2) has a thickness of 1 μm or greater.

### Claim 4 (depends on 1)

A method for producing a laminate, the method comprising laminating an electron excitation layer (1) having a diamond crystal structure in which some carbon atoms are substituted with nitrogen atoms, and a conductive layer (2) having a diamond crystal structure in which some carbon atoms are substituted with boron atoms, to obtain the laminate described in claim 1.

### Claim 5 (depends on 1)

An electrode comprising the laminate described in claim 1.

### Claim 6 (depends on 5)

The electrode according to claim 5, wherein the electrode is a visible light-responsive reduction electrode.

### Claim 7 (depends on 5)

An electrolytic reaction apparatus comprising the electrode described in claim 5.

### Claim 8 (depends on 5)

A method for producing carbon monoxide, the method comprising reducing, under irradiation with visible light, carbon dioxide on the electrode described in claim 5 to obtain carbon monoxide.

### Claim 9 (depends on 1)

The laminate according to claim 1, wherein a nitrogen atom concentration in the electron excitation layer (1) is 5×1018 atoms/cm3 or greater.

### Claim 10 (depends on 1)

The laminate according to claim 1, wherein a boron atom concentration in the conductive layer (2) is 1×1019 atoms/cm3 or greater.

### Claim 11 (depends on 1)

The laminate according to claim 1, wherein a nitrogen atom concentration in a portion from a surface of the electron excitation layer (1) to a depth of 30 nm is 1×1019 atoms/cm3 or greater.

### Claim 12 (depends on 1)

The laminate according to claim 1, wherein a concentration of heteroatoms other than boron atoms and nitrogen atoms in the electron excitation layer (1) is 1×1018 atoms/cm3 or less.

### Claim 13 (depends on 1)

The laminate according to claim 1, wherein a surface layer portion of the electron excitation layer (1) is hydrogen-terminated.

### Claim 14 (depends on 1)

The laminate according to claim 1, wherein a nitrogen atom concentration in the conductive layer (2) is 1×1018 atoms/cm3 or less.

### Claim 15 (depends on 1)

The laminate according to claim 1, wherein the laminate has a thickness from 1010 nm to 500 μm.

### Claim 16 (depends on 1)

The laminate according to claim 1, wherein a total weight of the electron excitation layer (1) and the conductive layer (2) accounts for 70 wt. % or more of a total weight of the laminate.

### Claim 17 (depends on 4)

The method for producing the laminate according to claim 4, the method further comprising:
1: fixing nitrogen-containing diamond particles on a substrate; and
2: forming, through a vapor phase growth method, a boron-doped diamond crystal structure on the substrate having the particles fixed thereon.

### Claim 18 (depends on 4)

The method for producing a laminate according to claim 4, the method further comprising:
1: fixing nitrogen-containing diamond particles on a substrate;
2: forming, through a vapor phase growth method, a boron-doped diamond crystal structure on the substrate having the particles fixed thereon;
3: removing the substrate; and
4: subjecting a surface exposed by removing the substrate to a hydrogenation treatment.

### Claim 19 (depends on 17)

The method for producing a laminate according to claim 17, wherein the step 1 comprises the following I and II:
I: applying, onto a substrate having a positive or negative charge, a paint comprising nitrogen-containing diamond particles having a positive or negative charge, the charge thereof being opposite the charge of the substrate, and then fixing the nitrogen-containing diamond particles on the substrate; and
II: applying, onto the fixed nitrogen-containing diamond particles, a paint comprising nitrogen-containing diamond particles having a positive or negative charge, the charge thereof being opposite the charge of the fixed nitrogen-containing diamond particles, and laminating the nitrogen-containing diamond particles having the opposite charge onto the fixed nitrogen-containing diamond particles.

### Claim 20 (depends on 17)

The method for producing a laminate according to claim 17, wherein the step 1 comprises the following I and II′:
I: applying, onto a substrate having a positive or negative charge, a paint comprising nitrogen-containing diamond particles having a positive or negative charge, the charge thereof being opposite the charge of the substrate, and then fixing the nitrogen-containing diamond particles on the substrate; and
II′: applying, onto the fixed nitrogen-containing diamond particles, a paint comprising nitrogen-containing diamond particles having a positive or negative charge, the charge thereof being opposite the charge of the fixed nitrogen-containing diamond particles, the nitrogen-containing diamond particles having a zeta potential amplitude of 40 mV or greater, and laminating the nitrogen-containing diamond particles having the opposite charge onto the fixed nitrogen-containing diamond particles.