# US 2025/0027187 A1 · Aluminum alloy for impact extruded containers and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0027187 A1
- Document ID: US20250027187A1
- Status: Published application
- Kind: A1
- Application number: 18/908,497
- Filed: 2024-10-07
- Published: 2025-01-23
- Earliest claimed: 2019-06-28
- Assignees: Ball Corporation
- Applicants: Ball Corporation
- Inventors: John L. Siles; Samuel Melancon; Stanley Platek; Anthony Chatey
- Web page: https://patentgrep.com/patent/US20250027187A1

## CPC

- C22C 21/00: Alloys based on aluminium
- B21C 23/18: by impact extrusion
- B21C 23/186: {by backward extrusion}
- B65D 1/0207: {characterised by material, e.g. composition, physical features}
- C22C 21/08: with silicon
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

Novel aluminum alloys are provided for use in an impact extrusion manufacturing process to create shaped containers and other articles of manufacture. In one embodiment blends of recycled scrap aluminum are used in conjunction with relatively pure aluminum to create novel compositions which may be formed and shaped in an environmentally friendly process. Other embodiments include methods for manufacturing a slug material comprising mixtures of aluminum alloys for use in the impact extraction process, a container manufactured using the aluminum alloy in an impact extrusion process, and the container, wherein the material of the container is the aluminum alloy.

## Claims

### Claim 1

An aluminum alloy for use in an impact extrusion process to form a metallic container which is configured to receive an end closure, the aluminum alloy comprising:
at least 97.56 wt. % Al;
between about 0.07 wt. % Si and about 0.18 wt. % Si;
between about 0.22 wt. % Fe and about 0.44 wt. % Fe;
between about 0.22 wt. % Mn and about 0.65 wt. % Mn;
between about 0.06 wt. % Mg and about 0.20 wt. % Mg;
between about 0.02 wt. % Ti and about 0.05 wt. % Ti; and
a balance comprising at least one of Zn, Cr and impurities.

### Claim 2 (depends on 1)

The aluminum alloy of claim 1, further comprising:
at most 0.17 wt. % Mg;
between about 0.02 wt. % Zn and about 0.04 wt. % Zn; and
between about 0.02 wt. % Cr and about 0.04 wt. % Cr.

### Claim 3 (depends on 2)

The aluminum alloy of claim 2, further comprising between about 0.03 wt. % Cu and about 0.18 wt. % Cu.

### Claim 4 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy is formed from between 40 wt. % and 90 wt. % of a first aluminum and between 10 wt. % and 60 wt. % of a second aluminum.

### Claim 5 (depends on 4)

The aluminum alloy of claim 4, wherein the first aluminum is selected from a first group consisting of AA1050, AA1070 or P1020A.

### Claim 6 (depends on 4)

The aluminum alloy of claim 4, wherein the second aluminum is selected from a second group consisting of AA3104, AA3004, AA3105, AA3003 or AA3103.

### Claim 7 (depends on 4)

The aluminum alloy of claim 4, further comprising a titanium boride added to a melt of the first aluminum and the second aluminum to alter a grain structure of the aluminum alloy.

### Claim 8 (depends on 1)

The aluminum alloy of claim 1, wherein a hardness of a sample of the aluminum alloy is between 52.4 HB and 68.8 HB.

### Claim 9 (depends on 1)

The aluminum alloy of claim 1, wherein a yield strength of a sample of the aluminum alloy with a thickness of 5.5 mm is between 20.7 MPa and 55.2 MPa.

### Claim 10 (depends on 1)

The aluminum alloy of claim 1, further comprising between about 0.02 wt. % Zn and about 0.04 wt. % Zn.

### Claim 11 (depends on 10)

The aluminum alloy of claim 10, further comprising between about 0.02 wt. % Cr and about 0.04 wt. % Cr.

### Claim 12 (depends on 11)

The aluminum alloy of claim 11, further comprising at least about 0.03 wt. % Cu.

### Claim 13 (depends on 1)

The aluminum alloy of claim 1, further comprising at least about 0.03 wt. % Cu.

### Claim 14 (depends on 1)

The aluminum alloy of claim 1, further comprising between 0.015 wt. % Cu and about 0.2 wt. % Cu.

### Claim 15 (depends on 1)

The aluminum alloy of claim 1, wherein a tensile strength of a sample of the aluminum alloy with a thickness of 5.5 mm is between 96.5 MPa and 144.8 MPa, and wherein an elongation percent of a sample of the aluminum alloy with a thickness of 5.5 mm is between 30% and 42%.

### Claim 16

A method to produce a slug formed from an aluminum alloy, the slug configured for use in an impact extrusion process to form a metallic container which is configured to receive an end closure, comprising:
forming an aluminum alloy which comprises:
at least 97.56 wt. % Al;
between about 0.07 wt. % Si and about 0.18 wt. % Si;
between about 0.22 wt. % Fe and about 0.44 wt. % Fe;
between about 0.22 wt. % Mn and about 0.65 wt. % Mn;
between about 0.06 wt. % Mg and about 0.20 wt. % Mg;
between about 0.02 wt. % Ti and about 0.05 wt. % Ti; and
a balance comprising at least one of Zn, Cr and impurities; and
forming the slug from the aluminum alloy, wherein a thickness of the slug is between 3.81 millimeters (mm) and 14.0 mm, and a diameter or width of the slug is between 20.3 mm and 88.9 mm.

### Claim 17 (depends on 16)

The method of claim 16, further comprising combining between 40 wt. % and 90 wt. % of a first aluminum alloy and between 10 wt. % and 60 wt. % of a second aluminum alloy to form the aluminum alloy.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
melting the first aluminum alloy and the second aluminum alloy to form a melt; and
adding titanium boride to the melt to alter a grain structure of the aluminum alloy, wherein the first aluminum alloy is selected from a first group consisting of AA1050, AA1070 or P1020A, and wherein the second aluminum alloy is selected from a second group consisting of AA3104, AA3004, AA3105, AA3003 or AA3103.

### Claim 19

A method for producing a metallic container which is configured to receive an end closure in an impact extrusion process from a slug formed from an aluminum alloy, comprising:
providing the slug formed of the aluminum alloy, wherein the aluminum alloy comprises:
at least 97.56 wt. % Al;
between about 0.07 wt. % Si and about 0.18 wt. % Si;
between about 0.22 wt. % Fe and about 0.44 wt. % Fe;
between about 0.22 wt. % Mn and about 0.65 wt. % Mn;
between about 0.06 wt. % Mg and about 0.20 wt. % Mg;
between about 0.02 wt. % Ti and about 0.05 wt. % Ti; and
a balance comprising at least one of Zn, Cr and impurities; and
wherein a thickness of the slug is between 3.81 millimeters (mm) and 14.0 mm, and a diameter or width of the slug is between 20.3 mm and 88.9 mm.

### Claim 20 (depends on 19)

The method of claim 19, wherein the aluminum alloy is formed by combining between 40 wt. % and 90 wt. % of a first aluminum alloy and between 10 wt. % and 60 wt. % of a second aluminum alloy.