# US 2025/0026886 A1 · Method for producing polyether nitrile

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0026886 A1
- Document ID: US20250026886A1
- Status: Published application
- Kind: A1
- Application number: 18/708,331
- Filed: 2022-10-26
- Published: 2025-01-23
- Earliest claimed: 2021-11-18
- Assignees: Honshu Chemical Industry Co., Ltd.; Daikin Industries, Ltd.
- Applicants: Honshu Chemical Industry Co., Ltd.; Daikin Industries, Ltd.
- Inventors: Akihiro HASHIKAWA; Tomoaki SHIMODA; Ryoto KANO; Yasuhiro NAKANO
- Web page: https://patentgrep.com/patent/US20250026886A1

## CPC

- C08G 65/4006: {(I) or (II) containing elements other than carbon, oxygen, hydrogen or halogen as leaving group (X)}
- C08G 65/4093: {characterised by the process or apparatus used}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A method for producing a polyether nitrile obtained by allowing an aromatic dihydroxy compound (I) and a dihalobenzonitrile compound (II) to undergo a polycondensation reaction in the presence of a basic compound (III) includes a first step of feeding a reaction raw material composed of the aromatic dihydroxy compound (I), the dihalobenzonitrile compound (II), and the basic compound (III) and a reaction solvent to a polycondensation reactor to perform a polycondensation reaction, a second step of taking out a polymer obtained by the polycondensation reaction from the polycondensation reactor, and a step (Step 3) of removing the polymer remaining in the polycondensation reactor and feeding the reaction solvent and the reaction raw material anew to the polycondensation reactor to perform a new polycondensation reaction. In the method, the melt flowability during molding is intended to be less likely to vary and decrease when the polyether nitrile is repeatedly produced.

## Claims

### Claim 1

A method for producing a polyether nitrile obtained by allowing an aromatic dihydroxy compound (I) and a dihalobenzonitrile compound (II) to undergo a polycondensation reaction in the presence of a basic compound (III), the method comprising:
a first step of feeding a reaction raw material composed of the aromatic dihydroxy compound (I), the dihalobenzonitrile compound (II), and the basic compound (III) and a reaction solvent to a polycondensation reactor to perform a polycondensation reaction;
a second step of taking out a polymer obtained by the polycondensation reaction from the polycondensation reactor; and
a third step of removing the polymer remaining in the polycondensation reactor and feeding the reaction solvent and the reaction raw material anew to the polycondensation reactor to perform a new polycondensation reaction.

### Claim 2 (depends on 1)

The method for producing a polyether nitrile according to claim 1, wherein the aromatic dihydroxy compound (I) is a compound represented by general formula (1) below, and the dihalobenzonitrile compound (II) is a compound represented by general formula (2) below:
HO—R—OH (1)
where R represents a divalent group represented by general formula (1a) below or general formula (1b) below;
where each R1 independently represents a linear or branched alkyl group having 1 to 6 carbon atoms, a cyclic alkyl group having 5 or 6 carbon atoms, or a phenyl group, each m independently represents an integer of 0 to 4, n represents 0 or 1, p and q each independently represent 0, 1, or 2, and each * represents a bonding position;
where R1 and m are as defined in general formula (1a), Y represents an oxygen atom, a sulfur atom, a sulfonyl group, a carbonyl group, an alkylidene group having 1 to 15 carbon atoms, a fluorine-containing alkylidene group having 2 to 15 carbon atoms, a cycloalkylidene group having 5 to 15 carbon atoms, a phenylmethylidene group, a phenylethylidene group, a phenylene group, or a fluorenylidene group, Z represents an oxygen atom, a sulfur atom, or non-bridging, each Ar independently represents an aryl group having 6 to 8 carbon atoms, and each * represents a bonding position;
where each X independently represents a halogen atom, and r represents an integer of 1 to 4.

### Claim 3 (depends on 2)

The method for producing a polyether nitrile according to claim 2, wherein R in the compound represented by general formula (1) is general formula (1a′) below or general formula (1a″) below, and r in the compound represented by general formula (2) is 1:
where R1, m, and * are as defined in general formula (1a);
where R1, m, and * are as defined in general formula (1a).

### Claim 4 (depends on 3)

The method for producing a polyether nitrile according to claim 3, wherein the compound represented by general formula (1) is at least one selected from hydroquinone, resorcin, and 4,4′-biphenol.

### Claim 5 (depends on 1)

The method for producing a polyether nitrile according to claim 1, wherein the basic compound (III) is an alkali metal compound.

### Claim 6 (depends on 1)

The production method according to claim 1, wherein a residual polymer amount after the polymer remaining in the reactor has been removed in Step 3 is 5000 ppm or less relative to a theoretical yield of a polymer obtainable from the reaction raw material fed into the reactor when the new polycondensation reaction is performed.

### Claim 7 (depends on 1)

The production method according to claim 1, further comprising a step (Step 4) of cleaning the polymer taken out from the polycondensation reactor in Step 2.

### Claim 8 (depends on 1)

The production method according to claim 1, wherein a resulting polyether nitrile has a reduced viscosity ηred of 1 or more and 5 or less.

### Claim 9 (depends on 1)

The production method according to claim 1, wherein the polycondensation reactor is a batch-type reactor.