# US 2025/0019852 A1 · Method of controlling properties of electrolytic copper foil and manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0019852 A1
- Document ID: US20250019852A1
- Status: Published application
- Kind: A1
- Application number: 18/548,195
- Filed: 2023-03-30
- Published: 2025-01-16
- Earliest claimed: 2022-05-11
- Assignees: Korea Zinc Co., Ltd.; Kzam Corporation
- Applicants: Korea Zinc Co., Ltd.; KZAM Corporation
- Inventors: Jeong Hwan KIM; Sae Kwon HEO; Gyun HU
- Web page: https://patentgrep.com/patent/US20250019852A1

## CPC

- C25D 1/04: Wires; Strips; Foils
- C25D 3/38: of copper
- C25D 5/00: Electroplating characterised by the process; Pretreatment or after-treatment of workpieces
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- Y02E 60/10: Energy storage using batteries
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of controlling physical properties of an electrolytic copper foil according to one embodiment of the present invention includes: controlling the physical properties of the electrolytic copper foil including elongation, tensile strength and roughness by regulating a surface glossiness of the electrolytic copper foil through addition of a surface glossiness agent. The surface glossiness is regulated within a range of 35 to 400 GU (60°).

## Claims

### Claim 1

A method of controlling physical properties of an electrolytic copper foil, comprising:
controlling the physical properties of the electrolytic copper foil including elongation, tensile strength and roughness by regulating a surface glossiness of the electrolytic copper foil through addition of a surface glossiness agent,
wherein the surface glossiness is within a range of 35 to 400 GU (60°).

### Claim 2 (depends on 1)

The method of claim 1, wherein the elongation is regulated according to the following Equation 1 by regulating the surface glossiness:
E
=
-
3.15
×
10
-
5
×
G
2
+
0.006
×
G
+
7.19
Equation
⁢
1
where G represents the surface glossiness (GU (60°)), and E represents the elongation (%).

### Claim 3 (depends on 1)

The method of claim 1, wherein the tensile strength is regulated according to the following Equation 2 by regulating the surface glossiness:
T
=
1.25
×
10
-
4
×
G
2
-
0.104
×
G
+
49.8
Equation
⁢
2
where G represents the surface glossiness (GU (60°)) and T represents the tensile strength (kgf/mm2).

### Claim 4 (depends on 1)

The method of claim 1, wherein the roughness is regulated according to the following Equation 3 by regulating the surface glossiness:
R
=
7.59
×
10
-
6
×
G
2
-
0.005
×
G
+
1.8
Equation
⁢
3
where G represents the surface glossiness (GU (60°)) and R represents the roughness (μm).

### Claim 5 (depends on 3)

The method of claim 3, wherein the roughness is regulated according to the following Equation 3 by regulating the surface glossiness:
R
=
7.59
×
10
-
6
×
G
2
-
0.005
×
G
+
1.8
Equation
⁢
3
where G represents the surface glossiness (GU (60°)) and R represents the roughness (μm).

### Claim 6 (depends on 1)

The method of claim 1, wherein the surface glossiness agent includes at least one of thiophosphoric acid-tris-(ω-sulfopropyl)ester trisodium salt, 3-mercapto-1-propanesulfonic acid (MPS), bis-(3-sulfopropyl)-disulfide disodium salt (SPS), and thioglycolic acid, which are sulfonic acids (compounds containing sulfur atoms), or metal salts thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein a concentration of the surface glossiness agent is 12 to 40 ppm.

### Claim 8 (depends on 7)

The method of claim 7, wherein a concentration of the surface glossiness agent is 18 to 28 ppm.

### Claim 9 (depends on 1)

A method for manufacturing an electrolytic copper foil, comprising:
dissolving copper ions in sulfate ions to prepare an electrolyte and adding at least one of an elongation agent for maintaining and improving elongation and a tensile strength agent for maintaining and improving tensile strength to the electrolyte;
controlling the physical properties of the electrolytic copper foil according to the method of claim 1 by adding a surface glossiness agent for improving surface glossiness; and
forming the electrolytic copper foil by supplying an electric current while supplying the electrolyte containing additives to a foil manufacturing machine in which a positive plate and a negative electrode rotating drum are spaced apart from each other.

### Claim 10 (depends on 9)

The method of claim 9, wherein a concentration of copper ions in the electrolyte is 70 g/L to 100 g/L, and a concentration of sulfate ions is 80 g/L to 150 g/L.

### Claim 11 (depends on 9)

The method of claim 9, wherein the elongation agent includes at least one of carboxymethylcellulose, polyethylene glycol, hydroxyethyl cellulose (HEC), octane diol-bis-polyalkylene glycol ether, and polyglycerin, which are nonionic water-soluble polymers.

### Claim 12 (depends on 9)

The method of claim 9, wherein the tensile strength agent includes at least one of diethylthiourea, ethylenethiourea, acetylenethiourea, 2-thiouracil, which are thiourea-based compounds or compounds in which a thiol group is linked to a nitrogen-containing hetero ring, 2-mercapto-5-benzoimidazole sulfonic acid sodium salt, sodium 3-(5-mercapto-1-tetrazolyl)benzene sulfonate, and 2-mercapto benzothiazole.

### Claim 13 (depends on 9)

The method of claim 9, wherein the surface glossiness agent includes at least one of thiophosphoric acid-tris-(co-sulfopropyl)ester trisodium salt, 3-mercapto-1-propanesulfonic acid (MPS), bis-(3-sulfopropyl)-disulfide disodium salt (SPS), and thioglycolic acid, which are sulfonic acids (compounds containing sulfur atoms), or metal salts thereof.

### Claim 14 (depends on 9)

The method of claim 9, wherein a concentration of the surface glossiness agent is 12 to 40 ppm.

### Claim 15 (depends on 14)

The method of claim 14, wherein a concentration of the surface glossiness agent is 18 to 28 ppm.