> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0019839 A1
- Document ID: US20250019839A1
- Status: Published application
- Kind: A1
- Application number: 18/747,661
- Filed: 2024-06-19
- Published: 2025-01-16
- Earliest claimed: 2023-07-13
- Assignees: Wisconsin Alumni Research Foundation; Ohio State Innovation Foundation
- Applicants: Wisconsin Alumni Research Foundation; Ohio State Innovation Foundation
- Inventors: Xudong Wang; Yutao Dong; Dane Morgan; Jun Meng; Jinwoo Hwang; Mehrdad Abbasi Gharacheh
- Web page: https://patentgrep.com/patent/US20250019839A1

## CPC

- C25B 11/049: Photocatalysts
- C25B 1/55: Photoelectrolysis
- C25B 11/059: Silicon
- C25B 11/087: Photocatalytic compound
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

A post-ALD in-situ water treatment procedure is used to remove the ligand residues in amorphous TiO2 films coated on photoanode material to improve the film stoichiometry without introducing any additional crystallization. The processed amorphous TiO2 film showed drastically improved chemical stability, and thereby substantially elongated the lifetime of silicon-based photoanodes in alkaline electrolyte.

## Claims

### Claim 1

A method of removing precursor ligands and byproducts in a photoelectrode, the method comprising:
(a) performing an atomic layer deposition of an oxide onto a photoanode material including the steps of:
pulsing oxygen precursors onto a photoanode material surface;
purging the photoanode material surface with an inert gas;
pulsing metal precursors onto the photoanode material surface; and
purging the photoanode material surface with the inert gas
to deposit a thin film of oxide onto the photoanode material surface to produce a thin film matrix;
(b) performing a water treatment of the thin film matrix including the steps of:
pulsing the oxygen precursors onto the thin film matrix; and
purging the thin film matrix with the inert gas;
to reduce a ratio of precursor ligand to oxide from the thin film matrix.

### Claim 2 (depends on 1)

The method of claim 1 wherein the water treatment reduces the ratio of precursor ligand to oxide by at least 20%.

### Claim 3 (depends on 2)

The method of claim 2 wherein the water treatment reduces the ratio of precursor ligand to oxide by at least 25%.

### Claim 4 (depends on 1)

The method of claim 1 wherein the photoanode material is silicon.

### Claim 5 (depends on 1)

The method of claim 1 wherein the thin film of oxide is TiO2.

### Claim 6 (depends on 5)

The method of claim 5 wherein the metal precursors are TiCl4.

### Claim 7 (depends on 6)

The method of claim 6 wherein the precursor ligands are Cl ligands.

### Claim 8 (depends on 7)

The method of claim 7 wherein the inert gas is N2 or Ar.

### Claim 9 (depends on 1)

The method of claim 1 further comprising sputtering nickel (Ni) onto the thin film matrix.

### Claim 10 (depends on 1)

The method of claim 1 where the step of water pulsing has a duration of at least 2 hours.

### Claim 11 (depends on 10)

The method of claim 10 wherein the step of water pulsing onto the thin film matrix is pulsing a water pulse that is at least 0.5 second and the water pulse is repeated.

### Claim 12 (depends on 1)

The method of claim 1 wherein the step of inert gas purging has a duration of at least 5 hours.

### Claim 13 (depends on 12)

The method of claim 12 where the step of inert gas purging onto the thin film matrix is purging with an inert gas at least 0.5 second and the insert gas purging is repeated.

### Claim 14 (depends on 1)

The method of claim 1 wherein the temperature of the atomic layer deposition is at less than or equal to 80 degrees Celsius.

### Claim 15 (depends on 1)

The method of claim 1 wherein the temperature of the water treatment is at less than or equal to 80 degrees Celsius.

### Claim 16 (depends on 1)

The method of claim 1 wherein the thin film of oxide has a thickness that is less than 15 nm.

### Claim 17 (depends on 1)

The method of claim 1 wherein the thin film matrix has a thickness that is less than 40 nm.

### Claim 18 (depends on 1)

The method of claim 1 wherein the atomic layer deposition and water treatment are performed in a vacuum.

### Claim 19

A photoelectrode comprising:
a thin film of oxide deposited onto a photoanode material via atomic layer deposition using a metal precursor reacted with an oxygen precursor resulting in a precursor ligand;
wherein the precursor ligand to oxide ratio is less than 3%.

### Claim 20 (depends on 19)

The photoelectrode of claim 19 wherein the photoanode material is silicon and the thin film of oxide is TiO2.