# US 2025/0014791 A1 · Method of producing magnetic powder, magnetic material for magnetic field amplification, and magnetic material for hyper-high frequency absorption

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0014791 A1
- Document ID: US20250014791A1
- Status: Published application
- Kind: A1
- Application number: 18/712,397
- Filed: 2022-11-09
- Published: 2025-01-09
- Earliest claimed: 2021-11-22
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Jun AKAMATSU; Satoshi ABE; Masahiro ABE; Kenta IWAI; Satoshi YAMANAKA; Shuichi TADA; Nobuyoshi IMAOKA
- Web page: https://patentgrep.com/patent/US20250014791A1

## CPC

- H01F 1/0552: {with a protective layer}
- B22F 1/145: Chemical treatment, e.g. passivation or decarburisation
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- C22C 38/001: {containing N}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C23C 22/42: containing also phosphates
- H01F 1/059: and Va elements, e.g. Sm2Fe17N2
- H01F 1/061: {with a protective layer}
- H01F 1/083: {in a bonding agent}
- B22F 2301/355: Rare Earth - Fe intermetallic alloys
- C22C 2202/02: Magnetic
- H05K 9/0075: {Magnetic shielding materials}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A method of producing a magnetic powder includes performing a phosphorus treatment to obtain a phosphorus compound and a rare earth-iron-nitrogen-based magnetic powder, the phosphorus treatment including adding an inorganic acid to a slurry containing: a rare earth-iron-nitrogen-based magnetic powder containing R, Fe, and N, where R represents at least one of rare earth elements selected from the group consisting of Y, Ce, Pr, Nd, Gd, Tb, Dy, Ho, Er, Tm, Lu, and Sm, and if R contains Sm, Sm constitutes less than 50 atm % of a total R atomic content; water; and a phosphorus-containing substance.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method of producing a magnetic powder, the method comprising:
performing a phosphorus treatment to obtain a phosphorus compound and a rare earth-iron-nitrogen-based magnetic powder, the phosphorus treatment comprising
adding an inorganic acid to a slurry comprising:
a rare earth-iron-nitrogen-based magnetic powder containing R, Fe, and N, where R represents at least one selected from the group consisting of Y, Ce, Pr, Nd, Gd, Tb, Dy, Ho, Er, Tm, Lu, and Sm, and if R contains Sm, Sm constitutes less than 50 atm % of a total R atomic content;
water; and
a phosphorus-containing substance.

### Claim 16 (depends on 15)

The method of producing a magnetic powder according to claim 15,
wherein, in the phosphorus treatment, the inorganic acid is added to adjust a pH of the slurry to at least 1 but not higher than 4.5.

### Claim 17 (depends on 15)

The method of producing a magnetic powder according to claim 15,
wherein a phosphorus content in the resulting phosphorus compound and rare earth-iron-nitrogen-based magnetic powder is at least 0.02% by mass but not higher than 4% by mass.

### Claim 18 (depends on 15)

The method of producing a magnetic powder according to claim 15, wherein the method comprises, after performing the phosphorus treatment, performing an oxidation comprising heat-treating the resulting phosphorus compound and rare earth-iron-nitrogen-based magnetic powder in an oxygen-containing atmosphere.

### Claim 19 (depends on 15)

The method of producing a magnetic powder according to claim 15,
wherein the phosphorus compound covers a surface of the rare earth-iron-nitrogen-based magnetic powder, and
wherein the phosphorus compound has an R-rich region with a higher atomic concentration of R than an atomic concentration of R in the rare earth-iron-nitrogen-based magnetic powder.

### Claim 20 (depends on 19)

The method of producing a magnetic powder according to claim 19,
wherein the atomic concentration of R in the R-rich region is at least 1 time an atomic concentration of Fe in the R-rich region.

### Claim 21

A magnetic material for magnetic field amplification, comprising:
a phosphorus compound; and
a rare earth-iron-nitrogen-based magnetic powder containing R, Fe, and N, where R represents at least one selected from the group consisting of Y, Ce, Pr, Nd, Gd, Tb, Dy, Ho, Er, Tm, Lu, and Sm, and if R contains Sm, Sm constitutes less than 50 atm % of a total R atomic content.

### Claim 22 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21,
wherein a ratio of a real part of a relative permeability of the magnetic material at 20 MHz to a real part of a relative permeability of the magnetic material at 2 MHz is at least 0.8 but not higher than 1.1.

### Claim 23 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21,
wherein a ratio of a real part to an imaginary part of a relative permeability of the magnetic material at 20 MHz is at least 3 but not higher than 10000.

### Claim 24 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21,
wherein the phosphorus compound covers a surface of the rare earth-iron-nitrogen-based magnetic powder.

### Claim 25 (depends on 24)

The magnetic material for magnetic field amplification according to claim 24,
wherein the phosphorus compound has an R-rich region with a higher atomic concentration of R than an atomic concentration of R in the rare earth-iron-nitrogen-based magnetic powder.

### Claim 26 (depends on 25)

The magnetic material for magnetic field amplification according to claim 25,
wherein the atomic concentration of R in the R-rich region is at least 1 time the atomic concentration of Fe in the R-rich region.

### Claim 27 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21,
wherein a phosphorus content with respect to a total amount of the phosphorus compound and the rare earth-iron-nitrogen-based magnetic powder is at least 0.02% by mass but not higher than 4% by mass.

### Claim 28 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21 configured to be used for wireless power transfer.

### Claim 29 (depends on 21)

The magnetic material for magnetic field amplification according to claim 21, further comprising a resin.

### Claim 30

A magnetic material for hyper-high frequency absorption, comprising:
a phosphorus compound; and
a rare earth-iron-nitrogen-based magnetic powder containing R, Fe, and N, where R represents at least one selected from the group consisting of Y, Ce, Pr, Nd, Gd, Tb, Dy, Ho, Er, Tm, Lu, and Sm, and if R contains Sm, Sm constitutes less than 50 atm % of a total R atomic content.

### Claim 31 (depends on 30)

The magnetic material for hyper-high frequency absorption according to claim 30,
wherein an imaginary part of a relative permeability of the magnetic material at 0.11 THz is at least 0.02.

### Claim 32 (depends on 30)

The magnetic material for hyper-high frequency absorption according to claim 30,
wherein a ratio of an imaginary part of a relative permeability of the magnetic material at 0.11 THz to an imaginary part of a relative permeability of the magnetic material at 10 GHz is at least 0.03.

### Claim 33 (depends on 30)

The magnetic material for hyper-high frequency absorption according to claim 30,
wherein the phosphorus compound covers a surface of the rare earth-iron-nitrogen-based magnetic powder, and
wherein the phosphorus compound has an R-rich region with a higher atomic concentration of R than an atomic concentration of R in the rare earth-iron-nitrogen-based magnetic powder.

### Claim 34 (depends on 33)

The magnetic material for hyper-high frequency absorption according to claim 33,
wherein the atomic concentration of R in the R-rich region is at least 1 time an atomic concentration of Fe in the R-rich region.