Abstract
An aqueous dispersion including a binder resin, a nonionic surfactant, and a wax component, wherein the content of the nonionic surfactant is 0.1 to 200 parts by mass based on 100 parts by mass of the binder resin, and 2 parts by mass or more based on 100 parts by mass of the wax component.
Claims23
An aqueous dispersion, comprising:
- a binder resin;
- a nonionic surfactant;
- and
- a wax component,
- wherein a content of the nonionic surfactant is 0.1 to 200 parts by mass based on 100 parts by mass of the binder resin, and 2 parts by mass or more based on 100 parts by mass of the wax component.
2 more elements
An aqueous dispersion, comprising:
- a binder resin;
- a surfactant;
- and
- a wax component,
- wherein the surfactant comprises at least one selected from the group consisting of a sucrose fatty acid ester and a sorbitan fatty acid ester, and
- a content of the surfactant is 0.1 to 200 parts by mass based on 100 parts by mass of the binder resin, and 2 parts by mass or more based on 100 parts by mass of the wax component.
3 more elements
A film, comprising:
- a binder resin;
- a nonionic surfactant;
- and
- a wax component,
- wherein a content of the nonionic surfactant is 0.1 to 200 parts by mass based on 100 parts by mass of the binder resin, and 2 parts by mass or more based on 100 parts by mass of the wax component.
2 more elements
A film, comprising:
- a binder resin;
- a surfactant;
- and
- a wax component,
- wherein the surfactant comprises at least one selected from the group consisting of a sucrose fatty acid ester and a sorbitan fatty acid ester, and
- a content of the surfactant is 0.1 to 200 parts by mass based on 100 parts by mass of the binder resin, and 2 parts by mass or more based on 100 parts by mass of the wax component.
3 more elements
A film, comprising:
- a binder resin;
- a nonionic surfactant;
- and
- a wax component,
- wherein the film comprises a phase (X) having birefringence.
2 more elements
A film, comprising:
- a binder resin;
- a nonionic surfactant;
- and
- a wax component,
- wherein a surface of the film has a surface roughness Ra of 10 to 100 nm as measured by a scanning probe microscope method.