# US 2025/0001498 A1 · Preparation method of rare earth permanent magnetic material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0001498 A1
- Document ID: US20250001498A1
- Status: Published application
- Kind: A1
- Application number: 18/274,460
- Filed: 2023-03-13
- Published: 2025-01-02
- Earliest claimed: 2023-03-09
- Assignees: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences
- Applicants: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences
- Inventors: Bo Zhou; Lei Liu; Yingli Sun; Yong Ding; Aru Yan
- Web page: https://patentgrep.com/patent/US20250001498A1

## CPC

- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- B22F 3/16: in successive or repeated steps
- B22F 9/023: {Hydrogen absorption}
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 1/0433: {Nickel- or cobalt-based alloys}
- C22C 19/07: based on cobalt
- C22C 30/02: containing copper
- C22C 33/0257: {characterised by the range of the alloying elements}
- C22C 33/04: by melting
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/06: containing aluminium
- C22C 38/10: containing cobalt
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- H01F 1/0577: {sintered}
- H01F 1/059: and Va elements, e.g. Sm2Fe17N2
- B22F 2003/241: {Chemical after-treatment on the surface}
- B22F 2003/248: {Thermal after-treatment}
- B22F 2009/044: {by jet milling}
- B22F 2201/016: NH3
- B22F 2201/02: Nitrogen
- B22F 2201/11: Argon
- B22F 2202/03: Treatment under cryogenic or supercritical conditions
- B22F 2202/05: Use of magnetic field
- B22F 2301/155: Rare Earth - Co or -Ni intermetallic alloys
- B22F 2301/355: Rare Earth - Fe intermetallic alloys
- B22F 2301/40: Intermetallics other than rare earth-Co or -Ni or -Fe intermetallic alloys
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 2202/02: Magnetic
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A preparation method of a rare earth permanent magnetic material comprises one or more times of cryogenic treatment and tempering treatment. When the preparation method comprises one time of cryogenic treatment and tempering treatment, the cryogenic treatment is performed between sintering treatment and the tempering treatment, or is performed after the tempering treatment. When the preparation method comprises two or more times of cryogenic treatment and tempering treatment, at least one time of cryogenic treatment is performed between sintering treatment and the tempering treatment, and at least one time of cryogenic treatment is performed after the tempering treatment. The preparation method can refine and homogenize the structure and realize quick and convenient treatment, and can effectively improve the mechanical performance of the rare earth permanent magnetic material and maintain good magnetic performance.

## Claims

### Claim 1

A preparation method of a rare earth permanent magnetic material, comprising one or more times of cryogenic treatment and tempering treatment.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the preparation method comprises one time of cryogenic treatment and tempering treatment, and the cryogenic treatment is performed between sintering treatment and the tempering treatment, or the cryogenic treatment is performed after the tempering treatment.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the preparation method comprises two or more times of cryogenic treatment and tempering treatment, at least one time of cryogenic treatment is performed between sintering treatment and the tempering treatment, and at least one time of cryogenic treatment is performed after the tempering treatment.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the preparation method comprises two times of cryogenic treatment and tempering treatment, primary cryogenic treatment is performed after sintering treatment, then the tempering treatment is performed, and then, secondary cryogenic treatment is performed.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the preparation method comprises three times of cryogenic treatment and tempering treatment.

### Claim 6 (depends on 5)

The preparation method according to claim 5, wherein primary cryogenic treatment is performed after sintering treatment, then the tempering treatment is performed, then secondary cryogenic treatment is performed, and then, ternary cryogenic treatment is performed;
or, primary cryogenic treatment is performed after sintering treatment, then secondary cryogenic treatment is performed, then the tempering treatment is performed, and then, ternary cryogenic treatment is performed.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the rare earth permanent magnetic material comprises one of an R2Fe14B series rare earth permanent magnetic material alloy, a SmCo5 series rare earth permanent magnetic material alloy, a Sm2Co17 series rare earth permanent magnetic material alloy, a Sm2Fe17Nx series rare earth permanent magnetic material alloy, and a 1:12 type rare earth permanent magnetic material alloy.

### Claim 8 (depends on 2)

The preparation method according to claim 2, wherein the preparation method comprises: raw material preparation, melting, pulverizing, oriented green compacting, the sintering treatment, the cryogenic treatment, and the tempering treatment;
or, the preparation method comprises: raw material preparation, melting, pulverizing, oriented green compacting, the sintering treatment, the tempering treatment, and the cryogenic treatment.

### Claim 9 (depends on 4)

The preparation method according to claim 4, wherein the preparation method comprises: raw material preparation, melting, pulverizing, oriented green compacting, the sintering treatment, the primary cryogenic treatment, the tempering treatment, and the secondary cryogenic treatment.

### Claim 10 (depends on 5)

The preparation method according to claim 5, wherein the preparation method comprises: raw material preparation, melting, pulverizing, oriented green compacting, sintering treatment, primary cryogenic treatment, the tempering treatment, secondary cryogenic treatment, and ternary cryogenic treatment;
or, the preparation method comprises: raw material preparation, melting, pulverizing, oriented green compacting, sintering treatment, primary cryogenic treatment, secondary cryogenic treatment, the tempering treatment, and ternary cryogenic treatment.

### Claim 11 (depends on 1)

The preparation method according to claim 1, wherein the step of cryogenic treatment comprises: placing a green body in a cryogenic treatment system, performing cryogenic treatment when the temperature is decreased to a cryogenic treatment temperature, and then taking the green body out of the cryogenic treatment system;
or, the step of cryogenic treatment comprises: directly placing a green body in liquid nitrogen for cryogenic treatment, and then taking the green body out of the liquid nitrogen.

### Claim 12 (depends on 1)

The preparation method according to claim 1, wherein a cryogenic treatment temperature is lower than or equal to −130° C., and/or a cryogenic treatment time is 1-500 min.

### Claim 13 (depends on 1)

The preparation method according to claim 1, wherein a cryogenic treatment temperature is lower than or equal to −160° C., and/or a cryogenic treatment time is 10-400 min.

### Claim 14 (depends on 1)

The preparation method according to claim 1, wherein a cryogenic treatment temperature is lower than or equal to −190° C., and/or a cryogenic treatment time is 20-300 min.

### Claim 15 (depends on 1)

The preparation method according to claim 1, wherein the tempering treatment is one of tempering diffusion treatment, aging treatment and nitrogen treatment.

### Claim 16 (depends on 15)

The preparation method according to claim 15, wherein the tempering diffusion treatment comprises: performing primary tempering at 800-950° C. for 2-6 h, and then decreasing the temperature to 400-650° C. at a rate of 0.3-1.3° C./min to perform secondary tempering for 2-6 h;
the aging treatment comprises: maintaining the green body at 800-950° C. for 10-25 h, then decreasing the temperature to 400-550° C. at a rate of 0.3-1.3° C./min, and maintaining the green body at 400-550° C. for 2-12 h;
the nitrogen treatment comprises: maintaining the green body at 400-650° C. for 1-20 h under a nitrogen and/or ammonia atmosphere.

### Claim 17 (depends on 1)

A rare earth permanent magnetic material, being prepared by the preparation method for a rare earth permanent magnetic material according to claim 1.