# US 2024/0425756 A1 · Polymeric flame retardant synergist and the method of producing it and its formulation for polyamides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0425756 A1
- Document ID: US20240425756A1
- Status: Published application
- Kind: A1
- Application number: 18/708,316
- Filed: 2022-11-17
- Published: 2024-12-26
- Earliest claimed: 2021-11-23
- Assignees: Agency for Science, Technology and Research
- Applicants: Agency for Science, Technology and Research
- Inventors: Jun Hua Kong; Songlin Liu; Qi Feng Lim; Qun Ye; Warintorn Thitsartarn; Chaobin He
- Web page: https://patentgrep.com/patent/US20240425756A1

## CPC

- C09K 21/14: Macromolecular materials
- C08G 12/30: with substituted triazines
- C08G 12/34: and acyclic or carbocyclic compounds
- C08G 12/40: Chemically modified polycondensates
- C08L 23/06: Polyethylene
- C08L 77/00: Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain (of polyhydrazides C08L79/06; of polyamideimides or polyamide acids C08L79/08); Compositions of derivatives of such polymers
- C08L 77/02: Polyamides derived from omega-amino carboxylic acids or from lactams thereof (C08L77/10 takes precedence)
- C08L 2201/02: Flame or fire retardant/resistant
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A flame retardant synergist including a repeating unit including a backbone represented by a formula of: where moiety A is derived from a substituted triazine having at least two amino groups, and where moiety B is derived from a dialdehyde having a terminal aldehyde. Furthermore, moiety A and moiety B are bonded via a —C—N— linkage formed from having one of the at least two amino groups reacted with the terminal aldehyde, where n ranges from 5 to 1000. Additionally, one or more side units extend from the backbone, where the one or more side units are derived from 9,10-dihydro-9-oxa-10-phosphaphenanthrene 10-oxide or a derivative thereof. Furthermore, a flame retardant polymer composite that includes a polymer, the flame retardant synergist, and a flame retardant additive, is disclosed herein. Methods of forming the flame retardant synergist and the flame retardant polymer composite are further disclosed herein.

## Claims

### Claim 1

A flame retardant synergist comprising:
a repeating unit comprising:
a backbone represented by a formula of:
wherein moiety A is derived from a substituted triazine having at least two amino groups;
wherein moiety B is derived from a dialdehyde having a terminal aldehyde;
wherein moiety A and moiety B are bonded via a —C—N— linkage formed from having one of the at least two amino groups reacted with the terminal aldehyde;
wherein n ranges from 5 to 1000; and
one or more side units extending from the backbone, wherein the one or more side units are derived from 9,10-dihydro-9-oxa-10-phosphaphenanthrene 10-oxide or a derivative thereof.

### Claim 2 (depends on 1)

The flame retardant synergist of claim 1, wherein the flame retardant synergist is absent of a halogen and a halide.

### Claim 3 (depends on 1)

The flame retardant synergist of claim 1, wherein the substituted triazine is:
wherein R is selected from the group consisting of hydrogen, C1-6alkyl, —CH═CH2,

### Claim 4 (depends on 1)

The flame retardant synergist of claim 1, wherein the dialdehyde is:
wherein X is selected from the group consisting of a bond, —(CH2)m—, —(CH2)2—NH—(CH2)4—NH—(CH2)2—,
and
wherein m ranges from 1 to 10.

### Claim 5 (depends on 1)

The flame retardant synergist of claim 1, wherein the one or more side units are derived from

### Claim 6 (depends on 1)

The flame retardant synergist of claim 1, wherein the flame retardant synergist comprises:
wherein n ranges from 5 to 1000.

### Claim 7 (depends on 1)

A method of forming the flame retardant synergist of claim 1, the method comprising:
dissolving a substituted triazine and a dialdehyde in a mixture of organic solvents, wherein the substituted triazine has at least two amino groups and the dialdehyde has a terminal aldehyde to form a first reaction mixture; and
mixing 9,10-dihydro-9-oxa-10-phosphaphenanthrene 10-oxide or a derivative thereof with the first reaction mixture.

### Claim 8 (depends on 7)

The method of claim 7, wherein the mixture of organic solvents comprises an alcohol and dimethylacetamide.

### Claim 9 (depends on 7)

The method of claim 7, wherein the dissolving and/or the mixing is carried out at a temperature of 80° C. to 150° C.

### Claim 10 (depends on 7)

The method of claim 7, wherein the dissolving is carried out for a duration of more than 12 hours.

### Claim 11 (depends on 7)

The method of claim 7, wherein the mixing is carried out for a duration of at least 48 hours.

### Claim 12 (depends on 1)

A flame retardant polymer composite comprising:
a polymer;
the flame retardant synergist of claim 1; and
a flame retardant additive.

### Claim 13 (depends on 12)

The flame retardant polymer composite of claim 12, wherein the polymer is a thermoplastic.

### Claim 14 (depends on 12)

The flame retardant polymer composite of claim 12, wherein the thermoplastic comprises a polyamide or a polyethylene.

### Claim 15 (depends on 12)

The flame retardant polymer composite of claim 12, further comprising a char forming agent and/or a blowing agent.

### Claim 16 (depends on 1, 12)

A method of producing the flame retardant polymer composite of claim 12, the method comprising:
mixing the flame retardant synergist of claim 1 with a flame retardant agent to form a pre-mix; and
compounding the pre-mix with a polymer to form the flame retardant polymer composite.

### Claim 17 (depends on 16)

The method of claim 16, wherein the flame retardant synergist and the flame retardant agent are mixed in weight ratio of 1:3 to 1:4.

### Claim 18 (depends on 16)

The method of claim 16, wherein the loading of the flame retardant synergist and the flame retardant additive in the flame retardant polymer composite is less than 12.5 wt %.