# US 2024/0425627 A1 · Hdpe intermediate bulk container resin using advanced chrome catalyst by polyethylene gas phase technology

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0425627 A1
- Document ID: US20240425627A1
- Status: Published application
- Kind: A1
- Application number: 18/700,450
- Filed: 2022-10-14
- Published: 2024-12-26
- Earliest claimed: 2021-10-15
- Assignees: Univation Technologies, LLC
- Applicants: Univation Technologies, LLC
- Inventors: Elva L. Lugo; Mengmeng Li; Cliff R. Mure; Taylor L. Crammer; Francois Alexandre
- Web page: https://patentgrep.com/patent/US20240425627A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- B29C 49/0005: {characterised by the material}
- B29C 49/04: Extrusion blow-moulding
- C08F 2/34: Polymerisation in gaseous state
- C08F 4/69: Chromium, molybdenum, tungsten or compounds thereof
- B29K 2023/08: {Copolymers of ethylene (B29K2023/16 takes precedence)}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

According to one embodiment, a process for producing unimodal ethylene/α-olefin copolymer, the process comprising contacting ethylene and, optionally, one or more (C3-C12)α-olefin comonomers with a catalyst system in a gas-phase polymerization reactor, wherein the catalyst system comprises a chromium-based catalyst; wherein the unimodal ethylene copolymer comprises: a density from 0.942 g/cm3 to 0.950 g/cm3 according to ASTM D792-13; a flow index (I21) from 5.5 to 7.5 dg/min, when measured according to ASTM D1238 at 190° C. and a 21.6 kg load; a strain hardening modulus of 40 to 50 MPa; and a molecular weight distribution (MWD) as determined by a conventional gel permeation chromatography method or absolute gel permeation chromatography.

## Claims

### Claim 1

A process for producing unimodal ethylene/α-olefin copolymer, the process comprising contacting ethylene and, optionally, one or more (C3-C12)α-olefin comonomers with a catalyst system in a gas-phase polymerization reactor, wherein the catalyst system comprises a chromium-based catalyst;
wherein the unimodal ethylene copolymer comprises:
a density from 0.942 g/cm3 to 0.950 g/cm3 according to ASTM D792-13;
a flow index (I21) from 5.5 to 7.5 dg/min, when measured according to ASTM D1238 at 190° C. and a 21.6 kg load;
a strain hardening modulus of 40 to 50 MPa; and
a GPCabs molecular weight distribution (MWD), as measured by the weight average molecular weight (Mw) divided by the molecular number (Mn) (Mw/Mn), that is from 24 to 29 as determined by an absolute gel permeation chromatography method (GPCabs).

### Claim 2 (depends on 1)

The process of claim 1, wherein:
the density is in the range of 0.943-0.949 g/cm3; and
the melt flow index (I21) is from 5.5 to 7.2 dg/min.

### Claim 3 (depends on 1)

The process of claim 1, wherein the unimodal ethylene/α-olefin copolymer has a melt viscosity ratio (V0.1/V100) at 190° C. from 50 to 70, where V0.1 is the viscosity of the unimodal ethylene/α-olefin copolymer at 190° C. at a frequency of 0.1 radians/second, and V100 is the viscosity of the unimodal ethylene/α-olefin copolymer at 190° C. at a frequency of 100 radians/second.

### Claim 4 (depends on 1)

The process of claim 1, wherein the GPCabs molecular weight distribution (MWD) is from 25 to 28.

### Claim 5 (depends on 1)

The process of claim 1, wherein the unimodal ethylene/α-olefin copolymer has a viscosity (V0.1) at 190° C. at a frequency of 0.1 radians/second greater than or equal to 130,000 pascal-seconds.

### Claim 6 (depends on 1)

The process of claim 1, wherein the (C3-C12)α-olefin comonomer is 1-hexene.

### Claim 7

An unimodal ethylene/α-olefin copolymer comprising polymerized units derived from ethylene, wherein the unimodal ethylene/α-olefin copolymer comprises:
a density from 0.942 g/cm3 to 0.950 g/cm3 according to ASTM D792-13;
a flow index (I21) from 5.5 to 7.5 dg/min, when measured according to ASTM D1238 at 190° C. and a 21.6 kg load;
Charpy impact strength of 6.5 to 8.5 kilojoules per meter square (kJ/m2), measured at −40° C. according to ISO 179;
a stain hardening modulus of 41 to 45 MPa; and
a GPCabs molecular weight distribution (MWD), as measured by the weight average molecular weight (Mw) divided by the GPCabs molecular number (Mn) (Mw/Mn), that is from 24 to 29 as determined by an absolute gel permeation chromatography method (GPCabs).

### Claim 8 (depends on 7)

The unimodal ethylene/α-olefin copolymer of claim 7, wherein the density is in the range of 0.943-0.949 g/cm3.

### Claim 9 (depends on 7)

The unimodal ethylene/α-olefin copolymer of claim 7, wherein the melt flow index (I21) is from 5.5 to 7.2 dg/min.

### Claim 10 (depends on 7)

The unimodal ethylene/α-olefin copolymer of claim 7, wherein the unimodal ethylene/α-olefin copolymer has a melt viscosity ratio (V0.1/V100) at 190° C. is from 50 to 70, where V0.1 is the viscosity of the unimodal ethylene/α-olefin copolymer at 190° C. at a frequency of 0.1 radians/second, and V100 is the viscosity of the unimodal ethylene/α-olefin copolymer at 190° C. at a frequency of 100 radians/second.

### Claim 11 (depends on 7)

The unimodal ethylene/α-olefin copolymer of claim 7, wherein the GPCabs molecular weight distribution (MWD) (Mw/Mn), is from 25 to 28.

### Claim 12 (depends on 7)

The unimodal ethylene/α-olefin copolymer of claim 7, wherein the unimodal ethylene/α-olefin further comprises a environmental stress cracking resistance of greater than 1000 hours.

### Claim 13 (depends on 7)

An article comprising the unimodal ethylene/α-olefin copolymer of claim 7.

### Claim 14 (depends on 7)

A process of blow molding a unimodal ethylene/α-olefin copolymer into a blow-molded article, the process comprising:
melting the unimodal ethylene/α-olefin copolymer according to claim 7 to produce a melt thereof;
extruding the melt into a mold to form a shape; and
injecting a gas into the mold so as to create a cavity within the shape.