# US 2024/0425455 A1 · Method for selectively and continuously producing 2-methylpyridine and diphenylamine from aniline

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0425455 A1
- Document ID: US20240425455A1
- Status: Published application
- Kind: A1
- Application number: 18/705,968
- Filed: 2022-10-19
- Published: 2024-12-26
- Earliest claimed: 2021-10-31
- Assignees: China Petroleum & Chemical Corporation; Sinopec Dalian Research Institute of Petroleum and Petrochemicals Co., Ltd.
- Applicants: China Petroleum & Chemical Corporation; Sinopec Dalian Research Institute of Petroleum and Petrochemicals Co., Ltd.
- Inventors: Haomeng LI; Xiangyu ZHAO; Libo WANG; Wenbo QI; Zhenyu WANG; Lanpeng LI; Fubin AI
- Web page: https://patentgrep.com/patent/US20240425455A1

## CPC

- B01J 29/70: of types characterised by their specific structure not provided for in groups B01J29/08 - B01J29/65
- C07D 213/127: Preparation from compounds containing pyridine rings
- B01J 29/7007: {Zeolite Beta}
- C07C 209/02: by substitution of hydrogen atoms by amino groups
- C07D 213/16: containing only one pyridine ring
- C07C 2529/04: having base-exchange properties, e.g. crystalline zeolites, pillared clays
- Y02P 20/584: Recycling of catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to the field of fine chemical industry. Specifically disclosed are a method for synthesizing 2-methylpyridine from aniline, and a method for selectively and continuously producing 2-methylpyridine and diphenylamine from aniline. The method comprises: in a hydrogen-containing atmosphere, enabling aniline and a catalyst to undergo a contact reaction at a temperature of 100-400° C., wherein the catalyst is β zeolite carrying a metal component, and the metal component comprises an active metal component selected from at least one of W, Mo, Ni, and Co; controlling the temperature of the contact reaction to be 100-240° C. to obtain a product mainly consisting of 2-methylpyridine; and controlling the temperature of the contact reaction to be 260-400° C. to obtain a product mainly consisting of diphenylamine.

## Claims

### Claim 1

A method for selectively and continuously producing 2-methylpyridine and diphenylamine from aniline, the method comprises: in a hydrogen-containing atmosphere, enabling an aniline and a catalyst to undergo a contact reaction at a temperature of 100-400° C., wherein the catalyst is a β zeolite carrying a metal component, and the metal component comprises an active metal component selected from at least one of W, Mo, Ni, and Co; controlling the temperature of the contact reaction to be 100-240° C. to obtain a product mainly consisting of 2-methylpyridine, and controlling the temperature of the contact reaction to be 260-400° C. to obtain a product mainly consisting of diphenylamine.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the active metal component in terms of metal element is contained in an amount of 0.5-5 wt. %, based on the total amount of the catalyst.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the metal component further comprises an auxiliary metal component selected from at least one of Li, Na, K, Mg, and Ca, the auxiliary metal component in terms of an oxidation state is contained in an amount of 0-6.5 wt. %, based on the total amount of the catalyst;
and/or, the active metal component in terms of metal element is contained in an amount of 0.5-3 wt. %, based on the total amount of the catalyst.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the catalyst further comprises an alumina binder, the catalyst comprises 50-85 wt. % of a β zeolite, 0.5-5 wt. % of an active metal component in terms of metal element, 0-6.5 wt. % of an auxiliary metal component in terms of oxidation state, and 10-45 wt. % of an alumina binder, based on the total amount of the catalyst;
and/or, the metal component further comprises an auxiliary metal component selected from at least one of Li, Na, K, Mg, and Ca, the auxiliary metal component in terms of an oxidation state is contained in an amount of 0.5-5.5 wt. %, based on the total amount of the catalyst.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the catalyst comprises 60-85 wt. % of a β zeolite, 0.5-3 wt. % of an active metal component in terms of the metal element, 0.5-5.5 wt. % of an auxiliary metal component in terms of oxidation state, and 15-34.5 wt. % of an alumina binder, based on the total amount of the catalyst.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the pressure of the contact reaction is within a range of 1.5-4 MPa, the contact reaction is carried out under a hydrogen atmosphere.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the contact reaction is performed under the circumstance without introducing ammonia gas.

### Claim 8 (depends on 1)

The method according to claim 1, when a product mainly consisting of 2-methylpyridine is obtained, the temperature of the contact reaction is within the range of 160-240° C., the pressure of the contact reaction is within the range of 1.5-3 MPa; or
when a product mainly consisting of diphenylamine is obtained, the temperature of the contact reaction is within the range of 280-360° C., the pressure of the contact reaction is within the range of 1.5-3 MPa.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the aniline is reacted through a fixed bed reactor containing the catalyst;
and/or, when a product mainly consisting of 2-methylpyridine is obtained, the liquid hourly mass space velocity of the aniline is within the range of 0.5-3 h−1.
and/or, when a product mainly consisting of diphenylamine is obtained, the liquid hourly mass space velocity of the aniline is within the range of 0.3-1.5 h−1.

### Claim 10

A method for synthesizing 2-methylpyridine from aniline, wherein the method comprises carrying out a contact reaction between an aniline and a catalyst under a hydrogen-containing atmosphere and a condition for isomeric rearrangement reaction, the catalyst is a β zeolite carrying a metal component comprising an active metal component selected from at least one of W, Mo, Ni, and Co, and the temperature of the contact reaction is within the range of 100-240° C.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the active metal component in terms of metal element is contained in an amount of 0.5-5 wt. %, based on the total amount of the catalyst.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the metal component further comprises an auxiliary metal component selected from at least one of Li, Na, K, Mg, and Ca, the auxiliary metal component in terms of an oxidation state is contained in an amount of 0-6.5 wt. %, based on the total amount of the catalyst;
and/or, the active metal component in terms of metal element is contained in an amount of 0.5-3 wt. %, based on the total amount of the catalyst.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the catalyst further comprises an alumina binder, the catalyst comprises 50-85 wt. % of a β zeolite, 0.5-5 wt. % of an active metal component in terms of metal element, 0-6.5 wt. % of an auxiliary metal component in terms of oxidation state, and 10-45 wt. % of an alumina binder, based on the total amount of the catalyst.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the catalyst comprises 60-85 wt. % of a β zeolite, 0.5-3 wt. % of an active metal component in terms of reduced state, 0.5-5.5 wt. % of an auxiliary metal component in terms of oxidation state, and 15-34.5 wt. % of an alumina binder, based on the total amount of the catalyst.

### Claim 15 (depends on 10)

The method according to claim 10, wherein the contact reaction is performed under the circumstance without introducing ammonia gas.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the contact reaction is carried out intermittently, the temperature of the contact reaction is within the range of 130-180° C., the pressure of the contact reaction is within the range of 2-4 MPa, the reaction time is within the range of 4-8 h; or
the contact reaction is carried out continuously, the temperature of the contact reaction is within the range of 160-240° C., the pressure of the contact reaction is within the range of 1.5-3 MPa.

### Claim 17 (depends on 10)

The method according to claim 10, wherein the aniline is reacted through a fixed bed reactor containing the catalyst;
and/or, the contact reaction is carried out intermittently, the used amount of the catalyst accounts for 1-4 wt. % of the used amount of the aniline;
and/or, the contact reaction is carried out continuously, the liquid hourly mass space velocity of the aniline is within the range of 0.5-3 h−1.

### Claim 18 (depends on 10)

The method according to claim 10, wherein the aniline is fed from the bottom of the fixed bed reactor and passes through a catalyst bed.

### Claim 19 (depends on 9)

The method according to claim 9, wherein the aniline is fed from the bottom of the fixed bed reactor and passes through a catalyst bed.