# US 2024/0417900 A1 · Nonwoven fabric having improved softness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0417900 A1
- Document ID: US20240417900A1
- Status: Published application
- Kind: A1
- Application number: 18/663,674
- Filed: 2024-05-14
- Published: 2024-12-19
- Earliest claimed: 2023-06-16
- Assignees: Fitesa Simpsonville, Inc.
- Applicants: Fitesa Simpsonville, Inc.
- Inventors: Thitaree KONGDATE; Jirawan JIRAPONG
- Web page: https://patentgrep.com/patent/US20240417900A1

## CPC

- D04H 1/4291: Olefin series
- A61F 13/15699: {Forming webs by bringing together several webs, e.g. by laminating or folding several webs, with or without additional treatment of the webs}
- A61L 15/225: {Mixtures of macromolecular compounds}
- A61L 15/42: Use of materials characterised by their function or physical properties (liquid bandages A61L26/00)
- D04H 1/4374: using different kinds of webs, e.g. by layering webs
- D04H 1/43828: {sheath-core}
- D04H 1/43838: {Ultrafine fibres, e.g. microfibres}
- D04H 1/559: the fibres being within layered webs
- D04H 1/56: in association with fibre formation, e.g. immediately following extrusion of staple fibres
- D04H 3/007: Addition polymers
- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- A61F 2013/15447: {Fibre dimension, e.g. denier or tex}
- A61F 2013/15959: {by spunbond technique}
- A61F 2013/15967: {by meltblown technique}
- A61F 2013/15991: {in making composite multi-layered product}
- D10B 2321/022: polypropylene
- D10B 2401/063: high strength
- D10B 2509/026: Absorbent pads; Tampons; Laundry; Towels
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

A nonwoven fabric having a plurality of fibers bonded to form a coherent web, the fibers are formed of a polymeric blend of a polypropylene resin and an elastomeric polyolefin, wherein the fabric exhibits a decrease in fiber fineness of at least 5% in comparison to an identically prepared nonwoven fabric that does not include the elastomeric polyolefin blended with the polypropylene resin.

## Claims

### Claim 1

A nonwoven fabric comprising a plurality of fibers bonded to form a coherent web, the fibers comprising a polymeric blend of a polypropylene resin and an elastomeric polyolefin, wherein the fabric exhibits a decrease in fiber fineness of at least 5% in comparison to an identically prepared nonwoven fabric that does not include the elastomeric polyolefin blended with the polypropylene resin.

### Claim 2 (depends on 1)

The nonwoven fabric according to claim 1, wherein polypropylene resin has a molecular weight ranging from any of 120,000 to 300,000 g/mol, a melting temperature from about 150° C. to about 175° C., and wherein the polypropylene resin comprises a Ziegler-Natta catalyzed polypropylene, a metallocene catalyzed polypropylene, or a blend thereof.

### Claim 3 (depends on 1)

The nonwoven fabric according to claim 1, wherein the elastomeric polypropylene is present in the polymer blend in an amount ranging from about 2 to 30 weight percent, based on the total weight of the polymer blend.

### Claim 4 (depends on 1)

The nonwoven fabric according to claim 1, wherein the elastomeric polyolefin is selected from the group consisting of a propylene-alpha-olefin copolymer and a low isotacticity polypropylene polymer.

### Claim 5 (depends on 4)

The nonwoven fabric of claim 4, wherein the low isotacticity polypropylene has the following properties:
an isotacticity: a meso pentad fraction [mmmm] of 20 to 70% by mol;
an average number molecular weight (Mw) of 10,000 to 200,000;
a melting temperature from about 60 to 120° C.; and
a melt flow rate (MFR) greater than 40 g/10 min.

### Claim 6 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric comprises fibers having an average fiber fineness ranging from about 0.8 to 1.6 Dtex.

### Claim 7 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric exhibits a percent decrease in fiber dtex from about 5 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and is drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 8 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric has a machine direction bending softness ranging from 30 to 50 mm and a cross direction bending softness ranging from 15 to 40 mm.

### Claim 9 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric has an average machine/cross direction bending softness ranging from 25 to 40 mm, and in particular, from about 28 to 38 mm.

### Claim 10 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric fibers were drawn and attenuated at a cabin greater than 4,200 Pa., and wherein the nonwoven fabric exhibits:
a. a percent decrease in machine direction bending softness that is from about 20 to 40%, and in particular, from about 25 to 35%, and more particularly, from about 26 to 32% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers are drawn and attenuated at a cabin pressure of less than 4,200 Pa,
and
b. a percent decrease in machine/cross direction bending softness that is from about 20 to 40%, and in particular, from about 20 to 35%, and more particularly, from about 22 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers are drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 11 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric fibers were drawn and attenuated at a cabin greater than 4,200 Pa., and wherein the nonwoven fabric exhibits one or more of the following characteristics:
a) an average fiber fineness ranging from about 0.8 to 1.6 dtex, and in particular, from about 0.9 to 1.4. and more particularly, from about 1.2 to 1.35 dtex;
b) the nonwoven fabric exhibits a percent decrease in fiber dtex from about 5 to 60%, such as a percent decrease of 15 to 50%, in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
c) the nonwoven fabric exhibits a machine direction bending softness ranging from 30 to 50 mm direction and a cross direction bending softness ranging from 15 to 40 mm;
d) the nonwoven fabric exhibits a machine direction softness of less than one or more of 50 mm, 48 mm, 46 mm, 44 mm, 42 mm, 40 mm, and 38 mm, 36 mm, 34 mm, 32 mm, and 30 mm, and a cross direction softness less than one or more of 44 mm, 42 mm, 40 mm, 38 mm, 36 mm, 34 mm, 32 mm, 30 mm, 28 mm, 26 mm, 24 mm, 22 mm, and 20 mm;
e) a machine direction softness of at least one or more of 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, 42 mm, 46 mm, and 48 mm, and a cross direction softness of at least one or more of 20 mm, least 24 mm, 26 mm, 28 mm, 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, 42 mm, 44 mm, 46 mm, 48 mm, and 50 mm;
f) an average machine/cross direction bending softness ranging from 25 to 40 mm, and in particular, from about 28 to 38 mm, such as an average machine/cross direction bending softness of at least one or more of 20 mm, 22 mm, 24 mm, 26 mm, 28 mm, 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, and wherein the average machine/cross direction bending softness is less than one or more of 40 mm, 38 mm, 36 mm, 34 mm, 32 mm, 30 mm, 28 mm, 26 mm, 24 mm, 22 mm, and 20 mm.
g) a percent decrease in machine direction bending softness that is from about 20 to 40%, and in particular, from about 25 to 35%, and more particularly, from about 26 to 32% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
h) an average percent decrease in machine/cross direction bending softness that is from about 20 to 40%, and in particular, from about 20 to 35%, and more particularly, from about 22 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
i) an average percent decrease in machine/cross direction bending softness that is at least one or more of 12%, 14%, 16%, 18%, 20%, 22%, 24%, 26%, 28%, 30%, 32%, 34%, 36%, 38% and 40% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
j) an average percent decrease in machine/cross direction bending softness that is less than one or more of 40%, 38%, 36%, 34%, 32%, 30%, 28%, 26%, 24%, 22%, 20%, 18%, 16%, 14% and 12% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
k) an increase in MD and CD tensile strengths ranging from about 2 to 15% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa; and
l) an increase in percent elongation in one or more of machine or cross direction ranging from about 5 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 12 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric has an increase in MD and CD tensile strengths ranging from about 2 to 15% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the filaments were drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 13 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric has an increase in percent elongations in one or more of machine or cross direction ranging from about 5 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the filaments were drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 14 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric has the following:
an average fiber fineness ranging from about 0.8 to 1.6 dtex, and in particular, from about 0.9 to 1.4, and more particularly, from about 1.2 to 1.35 dtex;
a percent decrease in fiber dtex from about 5 to 30%, such as a percent decrease of 15 to 25%, in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the filaments were drawn and attenuated at a cabin pressure of less than 4,200 Pa; and
a machine direction bending softness ranging from 30 to 50 mm direction and a cross direction bending softness ranging from 15 to 40 mm.

### Claim 15 (depends on 1)

The nonwoven fabric according to claim 1, wherein the nonwoven fabric comprises a spunbond layer.

### Claim 16 (depends on 1)

An absorbent article comprising the nonwoven fabric according to claim 1.

### Claim 17

Method of preparing a bonded nonwoven fabric comprising:
melt blending a first polypropylene resin and an elastomeric polyolefin to form a molten or semi-molten polymer stream of a polymer blend;
introducing the polymer stream into a spinning beam;
extruding the polymer stream from the spinning beam to form fibers;
subjecting the formed fibers to a cabin pressure greater than 4,200 Pa to draw and attenuate the fibers; and
collecting the fibers on a collection surface to form a nonwoven web, wherein the fibers exhibit an average fiber fineness ranging from about 0.8 to 1.6 dtex, and in particular, from about 0.9 to 1.4. and more particularly, from about 1.2 to 1.35 dtex, and the nonwoven fabric exhibits a percent decrease in fiber dtex from about 5 to 30%, such as a percent decrease of 15 to 25%, in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the cabin pressure ranges from about 4,500 to 7,500 Pa, and in particular, from about 5,500 to 7,500 Pa.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the elastomeric polyolefin comprises a propylene-alpha-olefin copolymer or a low isotacticity polypropylene polymer.

### Claim 20 (depends on 17)

The method according to claim 17, wherein the nonwoven fabric exhibits one or more of the following characteristics:
a) an average fiber fineness ranging from about 0.8 to 1.6 dtex, and in particular, from about 0.9 to 1.4. and more particularly, from about 1.2 to 1.35 dtex;
b) a percent decrease in fiber dtex from about 5 to 60%, such as a percent decrease of 15 to 25%, in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
c) a machine direction bending softness ranging from 30 to 50 mm and a cross direction bending softness ranging from 15 to 40 mm;
d) a machine direction bending softness of less than one or more of mm, 50 mm, 48 mm, 46 mm, 44 mm, 42 mm, 40 mm, and 38 mm, 36 mm, 34 mm, 32 mm, and 30 mm, and a cross direction softness less than one or more of 44 mm, 42 mm, 40 mm, 38 mm, 36 mm, 34 mm, 32 mm, 30 mm, 28 mm, 26 mm, 24 mm, 22 mm, and 20 mm;
e) a machine direction softness of at least one or more of 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, 42 mm, 46 mm, and 48 mm, and a cross direction softness of at least one or more of 20 mm, least 24 mm, 26 mm, 28 mm, 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, 42 mm, 44 mm, 46 mm 48 mm, and 50 mm;
f) an average machine/cross direction bending softness ranging from 25 to 40 mm, and in particular, from about 28 to 38 mm, such as an average machine/cross direction bending softness of at least one or more of 20 mm, 22 mm, 24 mm, 26 mm, 28 mm, 30 mm, 32 mm, 34 mm, 36 mm, 38 mm, and 40 mm, and wherein the average machine/cross direction bending softness is less than one or more of 40 mm, 38 mm, 36 mm, 34 mm, 32 mm, 30 mm, 28 mm, 26 mm, 24 mm, 22 mm, and 20 mm.
g) a percent decrease in machine direction bending softness that is from about 20 to 40%, and in particular, from about 25 to 35%, and more particularly, from about 26 to 32% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
h) an average percent decrease in machine/cross direction bending softness that is from about 20 to 40%, and in particular, from about 20 to 35%, and more particularly, from about 22 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
i) an average percent decrease in machine/cross direction bending softness that is at least one or more of 12%, 14%, 16%, 18%, 20%, 22%, 24%, 26%, 28%, 30%, 32%, 34%, 36%, 38% and 40% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
j) an average percent decrease in machine/cross direction bending softness that is less than one or more of 40%, 38%, 36%, 34%, 32%, 30%, 28%, 26%, 24%, 22%, 20%, 18%, 16%, 14% and 12% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa;
k) an increase in MD and CD tensile strengths ranging from about 2 to 15% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa; and
l) an increase in percent elongation in one or more of machine or cross direction ranging from about 5 to 30% in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the fibers were drawn and attenuated at a cabin pressure of less than 4,200 Pa.

### Claim 21 (depends on 17)

The method according to claim 17, wherein the nonwoven fabric has the following:
an average fiber fineness ranging from about 0.8 to 1.6 dtex, and in particular, from about 0.9 to 1.4. and more particularly, from about 1.2 to 1.35 dtex;
a percent decrease in fiber dtex from about 5 to 360%, such as a percent decrease of 15 to 25%, in comparison to an identically prepared fabric with the exception that the identically prepared fabric does not include the elastomeric polyolefin and in which the filaments were drawn and attenuated at a cabin pressure of less than 4,200 Pa; and
a machine direction bending softness ranging from 30 to 50 mm direction and a cross direction bending softness ranging from 15 to 40 mm, such as a machine direction bending softness ranging from 35 to 45 mm direction and a cross direction bending softness ranging from 25 to 40 mm.

### Claim 22 (depends on 17)

The method according to claim 17, further comprising a step of depositing a second fabric layer over the nonwoven web, and wherein the second fabric layer is selected from the group of meltblown layer; carded fabric layer, spunbond layer, resin bonded layer, airlaid fabric layer, and a spunlace layer.

### Claim 23 (depends on 17)

The method according to claim 17, further comprising a step of thermal bonding the nonwoven web.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the step of thermal bonding the nonwoven web comprises calender bonding the nonwoven web with an engraved roll having raised bonding points configured and arranged to impart a bonding pattern on a surface of the nonwoven web, the bonding pattern having a percent bonded area from about 9.6 to 14%, an average individual bond surface area from about 0.10 to 0.25 mm2, and an average bond point packing value from about 4 to 7.25 mm−1.