# US 2024/0417266 A1 · Process for manufacturing a silicon carbide coated body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0417266 A1
- Document ID: US20240417266A1
- Status: Published application
- Kind: A1
- Application number: 18/813,502
- Filed: 2024-08-23
- Published: 2024-12-19
- Earliest claimed: 2017-12-27
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Peter J. GUERCIO; Paul WESTPHAL; Kirk Allen FISHER
- Web page: https://patentgrep.com/patent/US20240417266A1

## CPC

- C01B 32/318: characterised by the starting materials
- C23C 16/0209: {by heating}
- C01B 32/336: characterised by gaseous activating agents
- C01B 32/372: Coating; Grafting; Microencapsulation
- C04B 35/522: {Graphite (C04B35/536 takes precedence)}
- C04B 41/009: {characterised by the material treated}
- C04B 41/5059: {Silicon carbide}
- C04B 41/87: Ceramics
- C23C 16/0227: {by cleaning or etching}
- C23C 16/325: {Silicon carbide}
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2006/10: Solid density
- C01P 2006/16: Pore diameter
- C01P 2006/80: Compositional purity
- C04B 2235/6584: at an oxygen percentage below that of air
- C04B 2235/663: Oxidative annealing
- C04B 2235/72: Products characterised by the absence or the low content of specific components, e.g. alkali metal free alumina ceramics
- C04B 2235/724: Halogenide content
- C04B 2235/77: Density
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present invention relates to a new process for manufacturing a silicon carbide (SiC) coated body by depositing SiC in a chemical vapor deposition method using dimethyldichlorosilane (DMS) as the silane source on a graphite substrate. A further aspect of the present invention relates to the new silicon carbide coated body, which can be obtained by the new process of the present invention, and to the use thereof for manufacturing articles for high temperature applications, susceptors and reactors, semiconductor materials, and wafer.

## Claims

### Claim 1

A method of manufacturing an activated graphite substrate with a modified surface porosity, comprising:
i) positioning a porous graphite substrate in a process chamber, the porous graphite substrate having an open porosity comprising pores with a surface pore diameter of less than 30 μm;
ii) purging the porous graphite substrate with nitrogen;
iii) heating the porous graphite substrate in the process chamber to a first temperature; and
iv) continuing purging with nitrogen in the process chamber and heating the porous graphite substrate to a second temperature.

### Claim 2 (depends on 1)

The method of claim 1, further comprising annealing the porous graphite substrate at a third temperature after purging the porous graphite substrate with nitrogen and heating of the porous graphite substrate to the second temperature until the process chamber reaches a first oxygen content.

### Claim 3 (depends on 1)

The method of claim 1, further comprising directly subjecting the porous graphite substrate to a chemical vapor deposition treatment after continuing purging with nitrogen in the process chamber and heating of the porous graphite substrate to the second temperature, without cleaning the porous graphite substrate before the chemical vapor deposition treatment.

### Claim 4 (depends on 1)

The method of claim 1, wherein before heating the porous graphite substrate in the process chamber to the first temperature, nitrogen is flowed in the process chamber until an oxygen content in the process chamber is 3.0%.

### Claim 5 (depends on 1)

The method of claim 1, wherein after heating the porous graphite substrate in the process chamber to the first temperature, heating is continued until an oxygen content is reduced to 0.3% or less, wherein the first temperature is at least 1000° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the porous graphite substrate, prior to being placed in the process chamber, has a chlorine content of at least 20.00 ppb by weight, wherein said chlorine content is present in the graphite substrate being 50 μm or more below a surface.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first temperature and the second temperature are between 1000 and 1500° C., and wherein the porous graphite substrate has a modified surface porosity comprising pores with an average pore diameter of >10 μm at a surface of the activated graphite substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein after continuing purging with nitrogen in the process chamber and heating of the porous graphite substrate to the second temperature, the pores of the porous graphite substrate have an average pore diameter which is enlarged compared to the pores thereof prior to being placed in the process chamber, wherein the second temperature is more than 1000° C., a first oxygen content is less than 0.5%, and the porous graphite substrate having a first average grain size less than 0.05 mm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the porous graphite substrate has a total amount of impurities of 10.00 ppm or less by weight.

### Claim 10

A method of processing a porous graphite substrate, comprising:
i) positioning a porous graphite substrate in a process chamber;
ii) purging the porous graphite substrate with nitrogen;
iii) heating the porous graphite substrate in the process chamber to a first temperature; and
iv) continuing purging with nitrogen in the process chamber and heating the porous graphite substrate to a second temperature;
heating of the porous graphite substrate to a third temperature greater than the second temperature and initiating purging with chlorine gas to form a chlorine atmosphere; and
heating the porous graphite substrate in the chlorine atmosphere to a fourth temperature of greater than the third temperature.

### Claim 11 (depends on 10)

The method of claim 10, wherein the porous graphite substrate has an open porosity comprising pores with a surface pore diameter of less than 30 μm and the porous graphite substrate has a total amount of impurities of 10.00 ppm or less by weight, and wherein the porous graphite substrate has a first average grain size.

### Claim 12 (depends on 10)

The method of claim 10, wherein after continuing purging with nitrogen in the process chamber and heating of the porous graphite substrate to the second temperature, the porous graphite substrate having a modified average pore diameter which is enlarged compared to an average pore diameter prior to being placed in the process chamber.

### Claim 13 (depends on 10)

The method of claim 10, wherein the porous graphite substrate, prior to being placed in the process chamber, has a chlorine content of at least 20.00 ppb by weight, wherein said chlorine content is present in the porous graphite substrate being 50 μm or more below a surface of the porous graphite substrate.

### Claim 14

A silicon carbide coated body used in a process chamber, comprising:
a graphite substrate comprising pores having an average pore diameter of >10 μm at a surface of the graphite substrate a surface; and
a silicon carbide layer on a surface of the graphite substrate,, the silicon carbide layer extending into the pores relative to the surface.

### Claim 15 (depends on 14)

The silicon carbide coated body used in a process chamber of claim 14, wherein the graphite substrate has a chlorine content of at least 20.00 ppb by weight, wherein said chlorine content is present in the graphite substrate being more than 50 μm below an outer surface thereof.

### Claim 16 (depends on 14)

The silicon carbide coated body used in a process chamber of claim 14, the graphite substrate having modified pores and unmodified pores, the modified pores having a diameter of two to eight times a diameter of the unmodified pores.

### Claim 17 (depends on 14)

The silicon carbide coated body used in a process chamber of claim 14, wherein the graphite substrate a first average grain size is from about 0.015 mm to about 0.04 mm.

### Claim 18 (depends on 14)

The silicon carbide coated body used in a process chamber of claim 14, wherein the graphite substrate has a density of 1.50 g/cm3 to 1.75 g/cm3.

### Claim 19 (depends on 14)

The silicon carbide coated body used in a process chamber of claim 14, wherein the graphite substrate comprises one or more of the following elements in an amount of:
calcium being less than 50.00 ppb by weight,
magnesium being less than 50.00 ppb by weight,
aluminum being less than 50.00 ppb by weight,
titanium being less than 10.00 ppb by weight,
chromium being less than 100.00 ppb by weight,
manganese being less than 10.00 ppb by weight,
copper being less than 50.00 ppb by weight,
iron being less than 10.00 ppb by weight,
cobalt being less than 10.00 ppb by weight,
nickel being less than 10.00 ppb by weight,
zinc being less than 50.00 ppb by weight, or
molybdenum being less than 150.00 ppb by weight.

### Claim 20 (depends on 15)

The silicon carbide coated body used in a process chamber of claim 15, wherein the silicon carbide layer is derived from dimethyldichlorosilane, and the silicon carbide layer comprises substantially tetrahedral crystalline silicon carbide tendrils having a length of at least 50 μm.