# US 2024/0417258 A1 · Method, product and system for cogenerating ferric phosphate through nitrophosphate fertilizer device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0417258 A1
- Document ID: US20240417258A1
- Status: Published application
- Kind: A1
- Application number: 18/209,343
- Filed: 2023-06-13
- Published: 2024-12-19
- Earliest claimed: 2022-06-20
- Assignees: Guizhou Batian Ecotypic Engineering Co., Ltd.; Shenzhen Batian Ecotypic Engineering Co.,Ltd.
- Applicants: Guizhou Batian Ecotypic Engineering Co., Ltd.; Shenzhen Batian Ecotypic Engineering Co., Ltd.
- Inventors: Deming HUANG; Guojun ZHAO; Faan LIU; Jin FANG; Shiying HUANG; Jing CHENG; Lingyun ZHANG; Junqiang FENG; Jianqing HUA
- Web page: https://patentgrep.com/patent/US20240417258A1

## CPC

- C01B 25/375: {of iron}
- C01F 11/44: Concentrating; Crystallisating; Dehydrating; Preventing the absorption of moisture or caking
- C01F 11/46: Sulfates (dehydration of gypsum {for the production of calcium sulfate cements} C04B11/02)
- C05B 11/00: Fertilisers produced by wet-treating or leaching raw materials either with acids in such amounts and concentrations as to yield solutions followed by neutralisation, or with alkaline lyes
- C05B 11/06: using nitric acid (nitrophosphates)
- C05B 17/00: Other phosphatic fertilisers, e.g. soft rock phosphates, bone meal
- C05D 9/02: containing trace elements
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C05B: PHOSPHATIC FERTILISERS
- C05D: INORGANIC FERTILISERS NOT COVERED BY SUBCLASSES C05B, C05C; FERTILISERS PRODUCING CARBON DIOXIDE

## Abstract

The present disclosure discloses a method, product, and system for cogenerating ferric phosphate through a nitrophosphate fertilizer device. The method comprises the steps of: acid-hydrolyzing phosphate rock with a nitric acid, and separating acid-insoluble substances to obtain an acid-hydrolyzed solution; freezing-crystallizing the acid-hydrolyzed solution, and carrying out solid-liquid separation to obtain a first solution; adding a solution containing sulfate ions to the first solution for reaction to obtain a second solution; subjecting the second solution to a denitrification to obtain a third solution; adding ammonia to the third solution for neutralization, and carrying out solid-liquid separation to obtain an ammonium phosphate solution, and adding an iron source to the ammonium phosphate solution for reaction to prepare a ferric phosphate. The present disclosure utilizes phosphate rock raw material to prepare a high-purity ferric phosphate, and by-product can be directly used for fertilizer preparation or as independent product, without waste.

## Claims

### Claim 1

A method for cogenerating ferric phosphate through a nitrophosphate fertilizer device, comprising the following steps of:
acid-hydrolyzing phosphate rock or phosphate concentrate with a nitric acid, and separating acid-insoluble substances to obtain an acid-hydrolyzed solution;
freezing-crystallizing the acid-hydrolyzed solution, and then carrying out solid-liquid separation to obtain a first solution;
adding a solution containing sulfate ions to the first solution for reaction, and then carrying out solid-liquid separation to obtain a second solution A; and/or adding a sulfuric acid to the first solution for reaction, and then carrying out solid-liquid separation to obtain a second solution B;
subjecting the second solution A and/or the second solution B to a denitrification to obtain a third solution A and/or a third solution B;
adding ammonia to the third solution A for neutralization, and then carrying out solid-liquid separation to obtain an ammonium phosphate solution, and then adding an iron source to the ammonium phosphate solution for reaction to prepare ferric phosphate;
and/or, subjecting the third solution B to a pre-treatment and extraction by using an extractant to obtain an extract phase, and then subjecting the extract phase to a post-treatment and back-extraction to obtain a phosphoric acid solution, and then reacting the phosphoric acid solution with an iron source to obtain ferric phosphate.

### Claim 2 (depends on 1)

The method for cogenerating ferric phosphate through the nitrophosphate fertilizer device according to claim 1, wherein the iron source comprises at least one of iron salts, ferrous salts, or elemental iron, and the solution containing sulfate ions is at least one of a sulfuric acid solution or an ammonium sulfate solution.

### Claim 3 (depends on 1)

The method for cogenerating ferric phosphate through the nitrophosphate fertilizer device according to claim 1, wherein the pH value of the reaction system is controlled between 4 and 6 during the reaction of the iron source with the ammonium phosphate solution, and wherein the pH value of the reaction system is controlled between 4 and 6 during the reaction of the iron source with the phosphoric acid solution.

### Claim 4 (depends on 1)

The method for cogenerating ferric phosphate through the nitrophosphate fertilizer device according to claim 1, wherein the concentration of the nitrate ions in the third solution A and the third solution B is below 0.1%; more preferably, the concentration of the nitrate ions in the third solution is below 0.05%; more preferably, the concentration of the nitrate ions in the third solution is below 0.01%.

### Claim 5 (depends on 1)

The method for cogenerating ferric phosphate through the nitrophosphate fertilizer device according to claim 1, wherein in the step of subjecting the third solution B to the extraction by using the extractant, the volume ratio of the extractant to the third solution B is 0.5-5:1.

### Claim 6 (depends on 1)

The method for cogenerating ferric phosphate through the nitrophosphate fertilizer device according to claim 1, wherein the ammonia comprises at least one of ammonia gas, liquid ammonia, or aqueous ammonia.

### Claim 7 (depends on 1)

A ferric phosphate product prepared by a method for cogenerating ferric phosphate through a nitrophosphate fertilizer device according to claim 1.

### Claim 8

A system for cogenerating ferric phosphate through a nitrophosphate fertilizer device, comprising:
an acid hydrolysis tank for an acid hydrolysis reaction of phosphate rock with a nitric acid;
a first solid-liquid separation device for solid-liquid separating the acid-hydrolyzed slurry after acid hydrolysis to obtain an acid-hydrolyzed solution;
a freezing-crystallization device for freezing-crystallizing the acid-hydrolyzed solution;
a second solid-liquid separation device for solid-liquid separating the acid-hydrolyzed solution obtained from the freezing-crystallization device to obtain a first solution;
a decalcification reaction device for reacting of the first solution with a solution containing sulfate ions;
a third solid-liquid separation device for solid-liquid separating product from the decalcification reaction to obtain a second solution;
a denitrification device for evaporating the second solution to remove nitrate ions, in order to obtain a third solution;
an extraction device for subjecting the third solution to a pre-treatment and extraction by using an extractant to obtain an extract phase;
a back-extraction device for subjecting the extract phase to a post-treatment and back-extraction to obtain phosphoric acid solution;
a ferric phosphate reaction device for reacting the phosphoric acid solution or the ammonium phosphate solution with an iron source to generate ferric phosphate;
and/or, a neutralization device and a fourth solid-liquid separation device, wherein the neutralization device is configured for the a neutralization reaction of the third solution with ammonium to obtain a neutralization reaction solution, and wherein the fourth solid-liquid separation device is configured for the solid-liquid separating the solution from the neutralization reaction to obtain an ammonium phosphate solution.