# US 2024/0410043 A1 · Fine-Grain Tin-Phosphor Bronze Alloy Strip and A Preparation Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0410043 A1
- Document ID: US20240410043A1
- Status: Published application
- Kind: A1
- Application number: 18/666,665
- Filed: 2024-05-16
- Published: 2024-12-12
- Earliest claimed: 2023-06-08
- Assignees: Chinalco Research Institute of Science and Technology Co., Ltd; China Copper Industry Co., Ltd
- Applicants: Chinalco Research Institute of Science and Technology Co., Ltd; China Copper Industry Co., Ltd
- Inventors: Huafen LOU; Zhongping CHEN; Chaojian XIANG; Yongda MO; Hu WANG; Miaomiao WANG
- Web page: https://patentgrep.com/patent/US20240410043A1

## CPC

- C22F 1/08: of copper or alloys based thereon
- B22D 11/004: {Copper alloys}
- B22D 11/045: for horizontal casting (B22D11/049 - B22D11/059 take precedence)
- C22C 9/02: with tin as the next major constituent
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The disclosure provides a fine-grain tin-phosphor bronze alloy strip and a preparation method thereof. The fine-grain tin-phosphor bronze alloy strip comprises the following elements in percentage by mass: 4.0-10 wt % of Sn, 0.01-0.3 wt % of P and the balance of Cu and inevitable impurity elements, the average grain size of the tin-phosphor bronze alloy strip is 1-3 μm, the grain size is in normal distribution, and the standard deviation of the grain size is 0.9 μm or below; the proportion of the total low-ΣCSL grain boundary in the tin-phosphor bronze alloy strip in the whole grain boundary is 66-74%, and in the total low-ΣCSL grain boundary, the ratio range of (Σ9+Σ27)/Σ3 is 0.12-0.23:1. The fine-grain tin-phosphor bronze alloy strip of this disclosure enables a finished strip can have the tensile strength and the excellent bending performance at the same time.

## Claims

### Claim 1

A fine-grain tin-phosphor bronze alloy strip comprising the following elements in percentage by mass: 4.0-10 wt % of Sn, 0.01-0.3 wt % of P and the balance of Cu and inevitable impurity elements, wherein, the average grain size of the tin-phosphor bronze alloy strip is 1-3 μm, the grain size is in normal distribution, and the standard deviation of the grain size is 0.9 μm or below; the proportion of the total low-ΣCSL grain boundary in the tin-phosphor bronze alloy strip in the whole grain boundary is 66-74%, and in the total low-ΣCSL grain boundary, the ratio range of (Σ9+Σ27)/Σ3 is 0.12-0.23:1.

### Claim 2 (depends on 1)

The fine-grain tin-phosphor bronze alloy strip according to claim 1, wherein, in the total low-ΣCSL grain boundary, the length fraction of the Σ3 grain boundary is 56-60%, the length fraction of the Σ9 grain boundary is 5-8%, and the length fraction of the Σ27 grain boundary is 2.5-4.5%.

### Claim 3 (depends on 1)

The fine-grain tin-phosphor bronze alloy strip according to claim 1, wherein, the standard deviation is 0.6-0.9 μm.

### Claim 4 (depends on 1)

A preparation method of the fine-grain tin-phosphor bronze alloy strip according to claim 1, wherein, the preparation method comprises:
subjecting the pretreated tin-phosphor bronze alloy strip to cold rolling deformation and heat treatment steps sequentially so as to obtain the fine-grain tin-phosphor bronze alloy strip;
wherein, the average grain size of the pretreated tin-phosphor bronze alloy strip is 1-3 μm.

### Claim 5 (depends on 4)

The preparation method according to claim 4, wherein, the deformation amount of the cold rolling deformation step is 15-25%.

### Claim 6 (depends on 4)

The preparation method according to claim 4, wherein, the temperature of the heat treatment step is 600-750° C.

### Claim 7 (depends on 4)

The preparation method according to claim 4, wherein, the preparation method further comprises a preparation process flow of the pretreated tin-phosphor bronze alloy strip, which comprises a batching step, a horizontal continuous casting step, a homogenization annealing step, a face milling step, a cold rolling cogging step, a first recrystallization annealing step, an intermediate rolling deformation step, a second recrystallization annealing step, a finish rolling deformation step, a third recrystallization annealing step, a bottom reservation rolling step, and a fourth recrystallization annealing step carried out sequentially, wherein the temperature of the homogenization annealing step is 650-690° C.

### Claim 8 (depends on 7)

The preparation method according to claim 7, wherein, the temperature of the first recrystallization annealing step is 540-580° C., and the heat preservation time of the first recrystallization annealing step is preferably 4-6 h.

### Claim 9 (depends on 7)

The preparation method according to claim 7, wherein, the temperature of the third recrystallization annealing step is 430-460° C., and the heat preservation time of the third recrystallization annealing step is preferably 1-4 h.

### Claim 10 (depends on 8)

The preparation method according to claim 8, wherein, the atmosphere for the first recrystallization annealing step, the second recrystallization annealing step, the third recrystallization annealing step, and the fourth recrystallization annealing step is a mixed gas of nitrogen and hydrogen.

### Claim 11 (depends on 2)

The fine-grain tin-phosphor bronze alloy strip according to claim 2, wherein, the standard deviation is 0.6-0.9 μm.

### Claim 12 (depends on 4)

The preparation method according to claim 4, wherein, the heat preservation time of the heat treatment step is 40-120 s.

### Claim 13 (depends on 7)

The preparation method according to claim 7, wherein, the heat preservation time of the homogenization annealing step is 6-8 h.

### Claim 14 (depends on 7)

The preparation method according to claim 7, wherein, the deformation amount of the cold rolling cogging step is 80-90%.

### Claim 15 (depends on 7)

The preparation method according to claim 7, wherein, the deformation amount of the bottom reservation rolling step is 40-55%.

### Claim 16 (depends on 7)

The preparation method according to claim 7, wherein, the deformation amount of the intermediate rolling deformation step is 50-70%.

### Claim 17 (depends on 7)

The preparation method according to claim 7, wherein, the deformation amount of the finish rolling deformation step is 40-60%.

### Claim 18 (depends on 7)

The preparation method according to claim 7, wherein, the temperature of the second recrystallization annealing step is 460-500° C., and the heat preservation time of the second recrystallization annealing step is preferably 4-6 h.

### Claim 19 (depends on 7)

The preparation method according to claim 7, wherein, the temperature of the fourth recrystallization annealing step is 380-430° C., and the heat preservation time of the fourth recrystallization annealing step is preferably 1-4 h.

### Claim 20 (depends on 10)

The preparation method according to claim 10, wherein, the mixed gas comprises 15-30% of H2 and 70-85% of N2 in percentage by volume.