# US 2024/0407270 A1 · Electro-formed metal foils

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0407270 A1
- Document ID: US20240407270A1
- Status: Published application
- Kind: A1
- Application number: 18/657,367
- Filed: 2024-05-07
- Published: 2024-12-05
- Earliest claimed: 2020-08-06
- Assignees: American Superconductor Corporation
- Applicants: American Superconductor Corporation
- Inventors: Cornelis Leo Hans Thieme
- Web page: https://patentgrep.com/patent/US20240407270A1

## CPC

- C25D 1/003: {3D structures, e.g. superposed patterned layers}
- H10N 60/0604: {Monocrystalline substrates, e.g. epitaxial growth}
- C25D 1/04: Wires; Strips; Foils
- C25D 1/20: Separation of the formed objects from the electrodes {with no destruction of said electrodes}
- C25D 3/56: of alloys
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/617: {Crystalline layers}
- C25D 7/0614: {Strips or foils}
- C30B 19/00: Liquid-phase epitaxial-layer growth
- C30B 30/02: using electric fields, e.g. electrolysis
- H10N 60/0241: {of devices comprising nitrides or carbonitrides}
- H10N 60/0324: {from a solution}
- C25D 5/611: {Smooth layers}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A process for producing a cube textured foil is described. The process includes providing a cube textured metal foil M. The process further includes electroplating an epitaxial layer of an alloy on the foil M, whereby the epitaxial layer substantially replicates the cube texture of the metal foil M. The process further includes electroplating a non-epitaxial layer of an alloy on the epitaxial layer. The process further includes separating the electroplated alloy from the cube textured metal foil M to obtain an electro-formed alloy with one cube textured surface.

## Claims

### Claim 1

A foil comprising an alloy of Ni(1-X-Y)BXCY, the foil having an epitaxial, non-magnetic layer of the alloy having a cube texture overlying a non-epitaxial, non-textured, non-magnetic layer of the alloy, wherein B and C are selected from the group consisting of W, Mo, and Cr; and wherein X is 0.02-0.14 and Y is 0-0.14.

### Claim 2 (depends on 1)

The foil of claim 1 wherein the non-epitaxial, non-textured, non-magnetic layer comprises a texture chosen from the group consisting of a random texture, a fiber texture, and a combination thereof.

### Claim 3 (depends on 1)

The foil of claim 1, wherein the epitaxial, non-magnetic layer has a thickness of 0.5 to 80 microns and the non-epitaxial, non-magnetic layer has a thickness of 0.5 to 150 microns.

### Claim 4 (depends on 1)

The foil of claim 1, wherein the epitaxial, non-magnetic layer has a thickness of 2 to 6 microns and the non-epitaxial, non-magnetic layer has a thickness of 56 to 78 microns.

### Claim 5 (depends on 1)

The foil of claim 1, wherein the foil has a length of 10 meters to 2000 meters.

### Claim 6 (depends on 1)

The foil of claim 1, wherein the alloy is selected from the group consisting of Ni(1-X-Y)WX, Ni(1-X-Y) MoX, Ni(1-X-Y)CrX, Ni(1-X-Y)WXMoY, and Ni(1-X-Y)WXCrY.

### Claim 7 (depends on 1)

The foil of claim 1, wherein the epitaxial, non-magnetic layer and the non-epitaxial, non-magnetic layer each comprise Ni(1-X-Y)WX wherein X is 0.08-0.10 and Y is 0.

### Claim 8 (depends on 1)

The foil of claim 1, wherein the non-epitaxial layer has an average grain size of between about 1 μm to about 5 μm.

### Claim 9 (depends on 1)

The foil of claim 1 wherein the epitaxial layer has a Ra surface roughness of between about 12 to about 20 nm.