# US 2024/0407107 A1 · Method for selective metallisation of inorganic dielectrics or semiconductors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0407107 A1
- Document ID: US20240407107A1
- Status: Published application
- Kind: A1
- Application number: 18/340,111
- Filed: 2023-06-23
- Published: 2024-12-05
- Earliest claimed: 2023-06-01
- Assignees: Valstybinis Moksliniu Tyrimu Institutas Fiziniu Ir Technologijos Mokslu Centras
- Applicants: Valstybinis Moksliniu Tyrimu Institutas Fiziniu Ir Technologijos Mokslu Centras
- Inventors: Karolis RATAUTAS; Gediminas RACIUKAITIS; Aldona JAGMINIENE; Ina STANKEVICIENE; Eugenijus NORKUS
- Web page: https://patentgrep.com/patent/US20240407107A1

## CPC

- H05K 3/187: {means therefor, e.g. baths, apparatus}
- C03C 17/10: by deposition from the liquid phase
- C03C 23/0025: {by a laser beam}
- C23C 18/1608: {from pretreatment step, i.e. selective pre-treatment}
- C23C 18/1868: {Radiation, e.g. UV, laser}
- C23C 18/1893: {with use of organic or inorganic compounds other than metals, first}
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H05K 3/0026: {by laser ablation}
- C03C 2217/253: Cu
- C03C 2218/31: Pre-treatment
- C23C 18/405: {Formaldehyde}
- H05K 2203/072: Electroless plating, e.g. finish plating or initial plating
- H05K 2203/107: Using laser light
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

This invention describes a process for selectively depositing metal on the surfaces of inorganic dielectric materials such as glass, ceramics, or semiconductor materials. The method enables the rapid and precise formation of electric circuits on both flat and three-dimensional surfaces. The production method includes steps: firstly, treatment of an item surface with an ultrashort pulse laser of the areas for metallisation, seconds step pre-treatment with the R—OH solution followed by metal salt catalyst activation in a bath and finally electroless metal plating. During immersion in the metal salt catalyst activation bath, localized R—OH molecules on the item's surface act as reducing agents, facilitating the reduction of metal ions from the activation bath. This results in the formation of catalytic seeds exclusively at the laser-modified areas. The metal layers exhibit high adhesion to the dielectric surface due to the formation of chemical bonds.

## Claims

### Claim 1

A method for selective metal plating on an item surface of an item made of an inorganic dielectric or semiconductor material, comprising steps of:
surface modification with a pulse laser on the item surface areas to be plated by the metal;
bringing the item with the laser-modified surface in contact with a pre-treatment solution;
immersing the item in a catalyst activation bath, and
metal plating in an electroless metal plating bath,
wherein the surface modification is performed with an ultrashort pulse laser leading to a static electrical charge formation on the item surface to be plated;
wherein parameters of the ultrashort laser pulses are chosen such that the static electrical charge formed on the item surface initiates formation of hydroxy groups on the laser-modified surface areas by adsorbing water molecules from ambient;
wherein the pre-treatment solution contains a mixture of a compound described by a formula of: R—OH and water, where R is a radical molecule, which does not dissociate in water;
wherein upon bringing the item with the laser-modified surface in contact with the pre-treatment solution, R—OH molecules are adsorbed and localised in the laser-modified areas;
wherein the catalyst activation bath is a metal salt activation bath;
wherein upon immersing the item in the metal salt catalyst activation bath the localised R—OH molecules on the surface of the item act as reducing agents to facilitate a reduction of metal ions from the catalyst activation bath, thereby forming catalytic seeds exclusively at the laser-modified areas.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the parameters of the ultrashort laser pulses are chosen such that when laser pulse radiation interacts with the material to be plated, a static electric charge occurs on the laser-modified surface of the material due to a Coulomb explosion.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the parameters of the ultrashort laser pulses are chosen such that when laser pulse radiation interacts with the material to be plated, a static electric charge occurs on the laser-modified surface of the material due to photochemical ablation including breaking of chemical bonds.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the ultrashort pulse laser has a pulse duration in a range of 0.005-500 picoseconds.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a wavelength of the ultrashort pulse laser comprises infrared, visible and ultraviolet range, wherein said irradiation dose is in a range of 0.01-200 J/cm2 and a laser scanning speed is in a range of 0.1-20 m/s. and said irradiation dose and scanning speed are chosen such that the laser-irradiated areas become active for hydroxy groups formation and adsorption of R—OH molecule in the pre-treatment solution.

### Claim 6 (depends on 5)

The method according to claim 5, wherein irradiation carried out by the ultrashort pulse laser is performed in a burst mode of laser pulses.

### Claim 7 (depends on 5)

The method according to claim 5, wherein a laser beam translation is performed with a galvanometric scanner.

### Claim 8 (depends on 5)

The method according to claim 5, wherein the laser beam of the ultra-pulse laser is a Bessel beam, shaped with an axicon optical element.

### Claim 9 (depends on 1)

The method according to claim 1, wherein humidity of the ambient during the method of selective metal plating is maintained within a range of 15% to 95%.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the pre-treatment solution is a mixture of water and alcohol at a concentration rate from 1% to 99.998% alcohol.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the item after pre-treatment with a pre-treatment solution is brought into contact with the catalyst activation bath at a time scale from 0.2 s to 10 min.

### Claim 12 (depends on 1)

The method according to claim 1, wherein an activation solution of the catalyst activation bath used for chemical activation is an aqueous solution of a metal salt selected from the group of the salts comprising silver (Ag) salt, copper (Cu) salt, nickel (Ni) salt, cobalt (Co) salt, zinc (Zn) salt, chromium (Cr) salt, or tin (Sn) salt.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the pre-treatment solution is an alkaline alcohol-containing bath with a pH value higher than 7.0.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the pre-treatment solution is an alcohol-containing bath and consists of mono-hydroxyl and/or poly-hydroxyl alcohols.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the pre-treatment solution consists of an ethanol and water mixture, or isopropanol and water mixture or pentanol and water mixture, or their mixture thereof.

### Claim 16 (depends on 1)

The method according to claim 1, wherein after immersion in the catalyst activation bath, the item is rinsed in water.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the item surface to be plated is glass selected from a group consisting of: silicate glass, soda-lime glass, borosilicate glass, fused silica, float glass, aluminosilicate glass, lead glass, borate glass fluorine glass, and phosphate glass.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the item surface to be plated is ceramics selected from a group consisting of: alumina, zirconia, SiC, AlN, Al2O3, silicon nitride, boron nitride, barium titanate, and ferrite ceramics.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the item surface to be plated is silicon or germanium.

### Claim 20 (depends on 1)

The method according to claim 1, wherein the reduction of metal ions takes place due to formation of a metal oxide and during reaction of metal ions with OH-ions produced after surface modification by the ultrashort pulse laser or after contact with a preparation solution or by reaction with OH ions in an alkaline electroless metal plating bath, and subsequently reducing metal oxide with the alcohol molecule formed after contact with the preparation solution.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the reduction of metal ions is due to metal ion or metal oxide reaction with a reducer in the electroless plating bath.