Process
AssigneeCycladex Inc
InventorRoger B. PETTMAN
Life of this patent
Estimating the term…
Abstract
Disclosed herein is a method of extracting lithium from a lithium bearing material comprising the steps of: a) providing an aqueous oxidant mixture comprising water, an oxidising means, and a source of halide ion; b) contacting the aqueous oxidant mixture with the lithium bearing material to extract the lithium from the lithium bearing material and form a lithium halide solution.
Claims26
A method of extracting lithium from a lithium bearing material comprising the steps of:
- a) providing an aqueous oxidant mixture comprising water, an oxidising means, and a source of halide ion,
- b) contacting the aqueous oxidant mixture with the lithium bearing material to extract the lithium from the lithium bearing material and form a lithium halide solution.
The method of any preceding claim wherein the oxidising means is hydrogen peroxide, oxygen, ozone, chlorine, hypochlorous acid, hypobromous acid, a hypochlorite salt, a hypobromite salt, a hypoiodite salt, a permanganate salt, or a combination thereof.
The method of any preceding claim, wherein the oxidising means is hydrogen peroxide.
The method of any preceding claim, wherein the source of halide ion is a source of bromide ion, a source of chloride ion, a source of iodide ion, or a combination thereof.
The method of any preceding claim, wherein the source of halide ion is a source of bromide ion, a source of chloride ion, or a combination thereof.
The method of any preceding claim, wherein the source of halide ion is at least one metal halide, said metal being lithium, potassium, sodium, calcium, or a combination thereof.
The method of any preceding claim, wherein the source of halide ion is at least one alkali metal halide, said alkali metal being lithium, potassium, sodium, or a combination thereof.
The method of any preceding claim, wherein the aqueous oxidant mixture has a pH of 0-7, preferably 0-6, more preferably 0.8 to 6.
The method of any preceding claim, wherein the aqueous oxidant mixture has a pH of 0.1 to 5.
The method of any preceding claim, wherein the aqueous oxidant mixture further comprises an acid, said acid preferably being sulphuric acid, nitric acid, hydrochloric acid, acetic acid, carbonic acid, formic acid, or a combination thereof.
The method of any preceding claim, wherein the aqueous oxidant mixture has a pH of 7-14, preferably 8-14.
The method of any preceding claim, wherein the aqueous oxidant mixture further comprises an alkaline material, said alkaline material preferably being sodium hydroxide, potassium hydroxide, calcium carbonate, calcium bicarbonate, sodium carbonate, sodium bicarbonate, potassium carbonate, potassium bicarbonate, calcium oxide, sodium hypochlorite, potassium hypochlorite, or a combination thereof.
The method of any preceding claim, further comprising the step of:
- c) converting the lithium halide to lithium metal, lithium carbonate, and/or lithium hydroxide.
The method of any preceding claim, wherein step b further comprises contacting the aqueous oxidant mixture with a resin, said resin being an ion exchange resin comprised of an organic polymer backbone to which a series of functional groups are attached, said functional groups containing at least one heteroatom.
The method of any preceding claim, wherein step c further comprises contacting the lithium halide solution with a resin, said resin being an ion exchange resin comprised of an organic polymer backbone to which a series of functional groups are attached, said functional groups containing at least one heteroatom.
The method of any preceding claim, wherein the lithium bearing material is an ore, a subsurface brine, a lithium battery, or a combination thereof.
The method of any preceding claim, wherein the lithium bearing material is an ore.
The method of any preceding claim, wherein the lithium bearing material is a lithium battery.