# US 2024/0404925 A1 · Molded power semiconductor package

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0404925 A1
- Document ID: US20240404925A1
- Status: Published application
- Kind: A1
- Application number: 18/205,129
- Filed: 2023-06-02
- Published: 2024-12-05
- Earliest claimed: 2023-06-02
- Applicants: Infineon Technologies AG
- Inventors: Marco Bäßler; Martin Haller
- Web page: https://patentgrep.com/patent/US20240404925A1

## CPC

- H10W 70/464: {Additional interconnections in combination with leadframes}
- H01R 12/585: {Terminals having a press fit or a compliant portion and a shank passing through a hole in the printed circuit board}
- H10W 74/01: Manufacture or treatment
- H10W 74/111: {the semiconductor body being completely enclosed}
- H10W 74/114: {by a substrate and the encapsulations}
- H10W 90/811: {Multiple chips on leadframes}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H01R: ELECTRICALLY-CONDUCTIVE CONNECTIONS; STRUCTURAL ASSOCIATIONS OF A PLURALITY OF MUTUALLY-INSULATED ELECTRICAL CONNECTING ELEMENTS; COUPLING DEVICES; CURRENT COLLECTORS

## Abstract

A molded power semiconductor package includes a mold compound having first and second opposing main surfaces and an edge between the first and second main surfaces. Power semiconductor dies are embedded in the mold compound. A metallic frame embedded in the mold compound is electrically connected to the power semiconductor dies. Pins protrude from the first main surface of the mold compound, each pin being secured to a respective contact area of the metallic frame that is exposed by an opening in the mold compound at the first main surface. One or more of the openings extends to the edge of the mold compound to form an open channel from each contact area exposed by the one or more of the openings to the edge of the mold compound. Additional package embodiments and methods of production are also described.

## Claims

### Claim 1

A molded power semiconductor package, comprising:
a mold compound having a first main surface, a second main surface opposite the first main surface, and an edge between the first main surface and the second main surface;
a plurality of power semiconductor dies embedded in the mold compound;
a metallic frame embedded in the mold compound and electrically connected to the power semiconductor dies; and
a plurality of pins protruding from the first main surface of the mold compound,
wherein each pin is secured to a respective contact area of the metallic frame that is exposed by an opening in the mold compound at the first main surface,
wherein one or more of the openings has a first linear dimension (a) in a vertical direction generally perpendicular to the first main surface, a second linear dimension (l) in a first horizontal direction generally parallel to the first main surface, and a third linear dimension (b) in a second horizontal direction transverse to the first horizontal direction,
wherein b>a and l>2a.

### Claim 2 (depends on 1)

The molded power semiconductor package of claim 1, wherein each pin is a press-fit pin.

### Claim 3 (depends on 1)

The molded power semiconductor package of claim 1, wherein a proximal end of each pin is inserted into an opening in the respective contact area of the metallic frame.

### Claim 4 (depends on 1)

The molded power semiconductor package of claim 1, wherein two or more of the pins protrude from the first main surface of the mold compound through the same opening.

### Claim 5 (depends on 4)

The molded power semiconductor package of claim 4, wherein the opening through which the two or more of the pins protrude from the first main surface of the mold compound has an elliptical shape.

### Claim 6 (depends on 1)

The molded power semiconductor package of claim 1, wherein the power semiconductor dies are electrically interconnected, including by the metallic frame, to form a power electronics circuit.

### Claim 7 (depends on 6)

The molded power semiconductor package of claim 6, wherein the power electronics circuit is a half bridge.

### Claim 8 (depends on 1)

The molded power semiconductor package of claim 1, wherein one or more of the openings extends to the edge of the mold compound to form an open channel from the respective contact area to the edge of the mold compound.

### Claim 9

A molded power semiconductor package, comprising:
a mold compound having a first main surface, a second main surface opposite the first main surface, and an edge between the first main surface and the second main surface;
a plurality of power semiconductor dies embedded in the mold compound;
a metallic frame embedded in the mold compound and electrically connected to the power semiconductor dies; and
a plurality of pins protruding from the first main surface of the mold compound,
wherein each pin is secured to a respective contact area of the metallic frame that is exposed by an opening in the mold compound at the first main surface,
wherein one or more of the openings extends to the edge of the mold compound to form an open channel from each contact area exposed by the one or more of the openings to the edge of the mold compound.

### Claim 10 (depends on 9)

The molded power semiconductor package of claim 9, wherein each pin is a press-fit pin.

### Claim 11 (depends on 9)

The molded power semiconductor package of claim 9, wherein a proximal end of each pin is inserted into an opening in the respective contact area of the metallic frame.

### Claim 12 (depends on 9)

The molded power semiconductor package of claim 9, wherein two or more of the pins protrude from the first main surface of the mold compound through the same opening.

### Claim 13 (depends on 12)

The molded power semiconductor package of claim 12, wherein the opening through which the two or more of the pins protrude from the first main surface of the mold compound has an elliptical shape.

### Claim 14 (depends on 9)

The molded power semiconductor package of claim 9, wherein the power semiconductor dies are electrically interconnected, including by the metallic frame, to form a power electronics circuit.

### Claim 15 (depends on 14)

The molded power semiconductor package of claim 14, wherein the power electronics circuit is a half bridge.

### Claim 16 (depends on 9)

The molded power semiconductor package of claim 9, wherein one or more of the openings has a first linear dimension (a) in a vertical direction generally perpendicular to the first main surface, a second linear dimension (l) in a first horizontal direction generally parallel to the first main surface, and a third linear dimension (b) in a second horizontal direction transverse to the first horizontal direction, and wherein b>a and l>2a.

### Claim 17

A method of producing a molded power semiconductor package, the method comprising:
embedding a plurality of power semiconductor dies and a metallic frame electrically connected to the power semiconductor dies in a mold compound, the mold compound having a first main surface, a second main surface opposite the first main surface, and an edge between the first main surface and the second main surface;
during the embedding, forming a plurality of openings in the first main surface of the mold compound and aligned with respective contact areas of the metallic frame, wherein one or more of the openings extends to the edge of the mold compound to form an open channel from each contact area aligned with the one or more of the openings to the edge of the mold compound;
after the embedding, performing a de-flashing process to remove mold compound flash from the contact areas of the metallic frame, wherein each open channel provides an ingress or egress path for a chemical de-flashing agent of the de-flashing process; and
after the de-flashing process, securing a plurality of pins to the contact areas of the metallic frame.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
directing a pressurized fluid at the openings in the first main surface of the mold compound to remove mold compound flash loosened by the chemical de-flashing agent from the contact areas of the metallic frame,
wherein the pressurized fluid is directed at an angle with respect to the first main surface of the mold compound.

### Claim 19 (depends on 17)

The method of claim 17, wherein the pins are secured to the contact areas of the metallic frame by press-fitting a proximal end of each pin into an opening in the respective contact area of the metallic frame.

### Claim 20 (depends on 17)

The method of claim 17, wherein one or more of the openings has a first linear dimension (a) in a vertical direction generally perpendicular to the first main surface, a second linear dimension (l) in a first horizontal direction generally parallel to the first main surface, and a third linear dimension (b) in a second horizontal direction transverse to the first horizontal direction, and wherein b>a and l>2a.