# US 2024/0401247 A1 · Resorbable and biocompatible glass fiber bundle having a well-defined diameter and process for making such

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0401247 A1
- Document ID: US20240401247A1
- Status: Published application
- Kind: A1
- Application number: 18/806,670
- Filed: 2024-08-15
- Published: 2024-12-05
- Earliest claimed: 2022-02-16
- Applicants: Purac Biochem B.V
- Inventors: Jenq LIU; Judit CANADELL-AYATS; Muhammed Sami HASAN; Shawn James PENISTON
- Web page: https://patentgrep.com/patent/US20240401247A1

## CPC

- D02G 3/18: from glass or the like
- C03B 37/02: by drawing or extruding, {e.g. direct drawing of molten glass from nozzles; Cooling fins therefor (C03B37/04 takes precedence; sizing of the fibres C03C25/00)}
- C03B 37/083: Nozzles; Bushing nozzle plates (C03B37/095 takes precedence)
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/0014: {Biodegradable glass}
- C03C 13/00: Fibre or filament compositions (manufacture of fibres or filaments C03B37/00)
- C03C 25/26: Macromolecular compounds or prepolymers
- C03C 25/323: Polyesters, e.g. alkyd resins
- C08K 7/14: Glass
- D02G 3/447: {Yarns or threads for specific use in general industrial applications, e.g. as filters or reinforcement}
- D02G 3/448: {Yarns or threads for use in medical applications (D02G3/449 takes precedence; surgical suture materials A61L17/00)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C 2213/02: Biodegradable glass fibres
- C08K 2201/003: Additives being defined by their diameter
- D10B 2401/063: high strength
- D10B 2401/12: biodegradable
- D10B 2505/02: Reinforcing materials; Prepregs
- D10B 2509/00: Medical; Hygiene
- D02G: CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, OR YARNS; YARNS OR THREADS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

The invention relates to a resorbable and biocompatible glass fiber bundle characterized in that the glass fibers of the bundle have an average diameter in the range of 5-30 μm, as measured according to ASTM D1577-01 C, the glass fiber bundle having a coefficient of variation at most 15%. The invention also pertains to, and a method of obtaining this glass fiber bundle. Also, the invention relates to composites and medical devices produced with said glass fiber bundle.

## Claims

### Claim 1

A resorbable and biocompatible glass fiber bundle, wherein the glass fibers of the glass fiber bundle have an average diameter in the range of 5-30 μm, wherein the coefficient of variation of the diameter is at most 15%, and wherein the number of fibers in the glass fiber bundle is at least 50.

### Claim 2 (depends on 1)

The glass fiber bundle according to claim 1, wherein the glass fibers in the glass fiber bundle comprise:
50 to 75 wt. % of SiO2,
0 to 15 wt. % of B2O3,
0.5 to 5 wt. % of P2O5,
5 to 20 wt. % of Na2O,
5 to 25 wt. % of CaO,
0 to 10 wt. % of MgO,
0 to 1 wt. % of Li2O,
0 to 15 wt. % of K2O,
0 to 4 wt. % of SrO,
0 to 5 wt. % of Al2O3, and
0 to 5 wt. % of Fe2O3.

### Claim 3 (depends on 1)

The glass fiber bundle according to claim 1, wherein the glass fibers have a tensile strength of 1000-3000 MPa as measured according to DIN EN ISO 5079, and/or wherein the glass fibers have an elastic modulus between 20 GPa and 100 GPa as measured according to DIN EN ISO 5079.

### Claim 4

A method for obtaining a glass fiber bundle, comprising the steps of:
a) providing a resorbable and biocompatible glass composition melt,
b) providing the glass composition melt to a first bushing having a plurality of orifices,
c) allowing or forcing the glass composition melt to flow through orifices of the first bushing, producing an intermediate glass melt stream,
d) collecting the intermediate glass melt stream in a second bushing having a plurality of orifices, and allowing or forcing the intermediate glass melt stream through the orifices of the second bushing to obtain a second glass melt stream, and
e) attenuating the second glass melt stream from the orifices of the second bushing to obtain fibers and letting the glass melt stream solidify to obtain a glass fiber bundle.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the temperature in the first bushing is in the range of 1000 to 1500° C., and wherein the temperature in the second bushing is in the range of from 1100 to 1250° C.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the second bushing is operated at a temperature which is lower than the temperature of the first bushing, wherein the difference between the temperature of the second bushing and the temperature of the first bushing is at least 50° C.

### Claim 7 (depends on 4)

The method according to claim 4, wherein viscosity of the melt in the first bushing is at least 50 poise below viscosity of the melt in the second bushing.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the intermediate glass melt stream resulting from the orifices of the first bushing is passed in a thin film over a plate before being provided to the second bushing.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the temperature of the glass in the thin film is higher than the temperature of the glass in the first bushing.

### Claim 10 (depends on 4)

The method according to claim 4, further comprising splitting the glass bundle into at least two bundles, and/or applying a sizing onto the glass fiber bundle(s), and/or collecting the glass fiber bundle(s).

### Claim 11 (depends on 4)

A composite comprising the glass fiber bundle obtained by the method of claim 4, or glass fibers from said bundle, in a polymer matrix compatible with the glass fibers, wherein the glass fibers and the polymer matrix are (i) biocompatible and resorbable, (ii) bioactive, or (i) and (ii).

### Claim 12 (depends on 11)

The composite according to claim 11, wherein the composite in the form of a unidirectional composite tape, tape, strand, (cannulated) rod, tube, pellet, or granule.

### Claim 13 (depends on 11)

A medical device comprising the composite of claim 11.

### Claim 14 (depends on 1)

A composite comprising the glass fiber bundle according to claim 1, or glass fibers from said bundle, in a polymer matrix compatible with the glass fibers, wherein the glass fibers and the polymer matrix are (i) biocompatible and resorbable, (ii) bioactive, or (i) and (ii).

### Claim 15 (depends on 14)

The composite according to claim 14, wherein the composite in the form of a unidirectional composite tape, tape, strand, (cannulated) rod, tube, pellet, or granule.

### Claim 16 (depends on 14)

A medical device comprising the composite of claim 14.

### Claim 17 (depends on 1)

The glass fiber bundle according to claim 1, wherein the glass fibers are composed of a glass formulation comprising network formers and network modifiers, wherein the weight or molar ratio between the network formers and network modifiers is between 1 and 4, and wherein the network former comprises an oxide of Si, B, P, Na, Mg, or Ca.

### Claim 18 (depends on 1)

The glass fiber bundle according to claim 1, wherein the glass fibers are sized glass fibers, wherein the glass fibers are made of a glass with a liquidus temperature of at least 800° C. as measured according to ASTM C829-81 (2015), and/or wherein the bundle has a linear density of between 50 and 500 tex as measured according to ASTM D1577-01 A.

### Claim 19 (depends on 1)

The glass fiber bundle according to claim 1, wherein the glass fibers are bioactive glass fibers.

### Claim 20 (depends on 4)

The method according to claim 4, wherein the glass composition melt exhibits a working window ΔT=TF−TL<330° C., wherein TF is the fiber forming temperature at log(η) of 3.0 dPas and TL is the liquidus temperature of the glass composition.