# US 2024/0400491 A1 · New heterogeneous palladium-based catalyst, preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0400491 A1
- Document ID: US20240400491A1
- Status: Published application
- Kind: A1
- Application number: 18/690,809
- Filed: 2022-09-09
- Published: 2024-12-05
- Earliest claimed: 2021-09-10
- Assignees: Fairbrics
- Applicants: Fairbrics
- Inventors: Ibrahim ABDELLAH; Bidal YANNICK; Tawfiq NASR ALLAH
- Web page: https://patentgrep.com/patent/US20240400491A1

## CPC

- C07C 67/36: by reaction with carbon monoxide or formates (C07C67/02, C07C67/03, C07C67/10 take precedence)
- B01J 23/63: with rare earths or actinides
- B01J 23/6562: {Manganese}
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/45: Nanoparticles
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/657: {larger than 1000 nm}
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 35/77: Compounds characterised by their crystallite size
- B01J 37/0201: {Impregnation}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 35/30: characterised by their physical properties
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A new catalyst that includes palladium on a cerium dioxide support, of formula Pd—X/CeO2, in which X represents the empty set or a doping element, and its use in the implementation of a method for selectively preparing oxalates or oxamides from carbon monoxide, an oxidant, in particular molecular oxygen or air, and an alcohol or an amine respectively.

## Claims

### Claim at position 1

1-23. (canceled)

### Claim 24

A method for selectively preparing an oxalate compound or an oxamide compound comprising a step A of bringing an alcohol or an amine, respectively, into contact with:
carbon monoxide,
an oxidizing agent,
a catalyst of formula Pd—X/CeO2, wherein X represents an empty set or a dopant element, comprising Pd atoms on a CeO2 support, in which the catalyst has a surface area, analyzed by BET, from 100 to 250 m/g,2
to obtain a reaction medium which may be pressurized from 0.1 to 15 MPa, and
to obtain the oxalate compound or the oxamide compound.

### Claim 25 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, comprising a step A of bringing an alcohol or an amine, respectively, into contact with a promoter.

### Claim 26 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, comprising a step A of bringing an alcohol or an amine, respectively, into contact with a base.

### Claim 27 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, comprising a step A of bringing an alcohol or an amine, respectively, into contact with a solvent.

### Claim 28 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, further comprising a step B of heating the reaction medium.

### Claim 29 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, wherein the catalyst has a palladium content from 0.1 to 10%, in particular 2%, or 5%, by weight relative to the total weight of the catalyst.

### Claim 30 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, wherein a dopant is chosen from Mn, Mg, Ca, Fe, Ba, Sr, Y, Nb, Zn, Bi, Sn, La, Pr, Nb and Sm, in particular at a content from 0.5 to 10%, preferably 1%, by weight relative to the total weight of the catalyst.

### Claim 31 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, comprising a step A of bringing an alcohol or an amine, respectively, into contact with:
carbon monoxide, in particular used from 0.5 to 8.0 MPa, in particular at 6.5 MPa
oxygen or air, in particular oxygen used from 0.5 to 2.5 MPa, in particular at 1.5 MPa
a promoter, in particular an iodine compound, chosen in particular from tetramethylammonium iodide, potassium iodide or sodium iodide, preferably tetramethylammonium iodide, preferably in a proportion from 0.1 to 5 mol % relative to the alcohol or amine, in particular in a proportion of 0.2 mol %,
a Pd—X/CeO2 catalyst comprising Pd atoms on a CeO2 support of the formula Pd—X/CeO2 wherein X represents the void system or a dopant element, wherein the catalyst has a surface area, analyzed by BET, from 100 to 250 m2/g, preferably the palladium is from 0.01 to 10 mol % relative to the alcohol or amine,
optionally a base, in particular triethylamine, preferably used in a proportion from 0.1 to 5 mol % relative to the alcohol or amine, in particular in a proportion of 0.15 mol %,
optionally a solvent, in particular selected from acetonitrile, tetrahydrofuran, dioxane and toluene, preferably acetonitrile,
to obtain a reaction medium,
optionally a step B of heating the reaction medium,
to obtain the oxalate compound or the oxamide compound.

### Claim 32 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, wherein an oxalate compound is selectively prepared, and wherein the method comprises a step A of bringing an alcohol into contact with:
carbon monoxide,
oxygen or air,
a promoter,
a Pd—X/CeO2 catalyst, comprising Pd atoms on a CeO2 support, of the formula Pd—X/CeO2 wherein X represents the void system or a dopant element, wherein the catalyst has a surface area, analyzed by BET, from 100 to 250 m2/g, preferably in an amount from 0.01 to 10 mol % relative to the alcohol or amine,
to obtain a reaction medium,
a step B of heating said reaction medium, in particular at a temperature from 25 to 200° C., in particular from 60 to 110° C., preferably around 90° C., to obtain the oxalate compound.

### Claim 33 (depends on 32)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 32, wherein the method comprises a step A of bringing an alcohol, into contact with a base.

### Claim 34 (depends on 32)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 32, wherein the method comprises a step A of bringing an alcohol, into contact with a solvent.

### Claim 35 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, wherein an oxalate compound of Formula 2 is selectively prepared, and wherein step A comprises contacting an alcohol of Formula 1:
wherein Ra represents:
a C1 to C20 linear or branched alkyl group,
a C3 to C10 cycloalkyl group,
a C5 to C20 alkyl-aryl or alkyl-heteroaryl group,
in particular the alcohol is chosen from methanol, ethanol and isopropanol.

### Claim 36 (depends on 24)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 24, wherein an oxamide compound is selectively prepared, and wherein the method comprises a step A of bringing an amine into contact with:
carbon monoxide,
oxygen or air,
a promoter,
a Pd—X/CeO2 catalyst comprising Pd atoms on a CeO2 support of the formula Pd—X/CeO2 wherein X represents the empty set or a dopant element, wherein the catalyst has a surface area, analyzed by BET, from 100 to 250 m2/g, preferably the palladium is from 0.01 to 10 mol % relative to the alcohol or amine,
a solvent,
to obtain a reaction medium comprising the oxamide compound.

### Claim 37 (depends on 36)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 36, wherein an oxamide compound is selectively prepared, and wherein the method comprises a step A of bringing an amine, into contact with a base.

### Claim 38 (depends on 36)

The method for selectively preparing an oxalate compound or an oxamide compound according to claim 36, wherein an oxamide compound of Formula 4 is selectively prepared, and wherein step A comprises contacting an amine of Formula 3:
wherein Rb and Rc independently of one another represent:
a hydrogen atom,
a C1 to C20 linear or branched alkyl group,
a C3 to C10 cycloalkyl group,
a C5 to C20 alkyl-aryl or alkyl-heteroaryl group,
at least one of the groups Rb or Rc being other than hydrogen,
Rb and Rc can form a cycle,
in particular the amine is chosen from piperidine, pyrrolidine, butylamine, benzylamine, furfurylamine and cyclohexylamine.

### Claim 39

A palladium/cerium dioxide catalyst, comprising palladium on a cerium dioxide support, of the formula Pd—X/CeO2, wherein X represents the void or a doping element,
wherein the catalyst has a surface area, analyzed by BET, from 100 to 250 m2/g, in particular from 100 and 200 m2/g,
and wherein the catalyst has a palladium content from 0.1 to 10%, in particular 2% or 5%, by weight relative to the total weight of the catalyst,
optionally the dopant being selected from the following group of elements: Mn, Mg, Ca, Fe, Ba, Sr, Y, Nb, Zn, Bi, Sn, La, Pr, Nb and Sm, preferably the dopant being Mn, in particular the said catalyst comprising a dopant content from 0.5 and 10%, in particular 1%, by weight relative to the total weight of the catalyst.

### Claim 40 (depends on 39)

The catalyst according to claim 39, wherein the catalyst has a fluorine-type structure by XRD and a crystallite size of less than 30 nanometers according to the Scherrer formula, in particular less than 20 nanometers, preferably less than 10 nanometers, or
wherein the catalyst has a crystallinity level from 0 to 50%, preferably from 0 to 20%.

### Claim 41 (depends on 39)

The catalyst according to claim 39, wherein said catalyst is in the form of particles of average micrometric size, in particular from 1 to 100 μm.

### Claim 42 (depends on 39)

The catalyst according to claim 39, wherein the surface of the said catalyst, analyzed by XPS, comprises from 90 to 100% palladium in the oxidation state (II), in particular in the form of Pd—O or a PdxCe1-xO2 solid solution, x varying from 0.01 to 1.

### Claim 43 (depends on 39)

A method for preparing a Pd—X/CeO2 catalyst according to claim 39, wherein the method comprises:
a step D of impregnating a palladium salt, in particular palladium nitrate, on a cerium dioxide support, to obtain a homogeneous material,
in particular said step D comprises:
the use of a support with a surface area from 100 to 300 m2/g, in particular from 150 to 160 m2/g or from 270 to 280 m2/g,
and using a palladium salt concentration calculated to obtain a palladium content of 0.1 to 10%, by weight relative to the total weight of the catalyst,
optionally using another salt selected from precursors of dopants from the following group of elements: Mn, Mg, Ca, Fe, Ba, Sr, Y, Nb, Zn, Bi, Sn, La, Pr, Nb and Sm, in particular the manganese salt, the dopant salt concentration is calculated to obtain a dopant content from 0.5 to 10% by weight relative to the total weight of the catalyst,
a step E for drying the material, in particular at a temperature from 60 to 100° C., in particular 80° C., preferably for a period from 10 to 24 hours, in particular 16 hours, and
a step F of palladium activation, in particular comprising calcination at a temperature from 200 to 1000° C., in particular 600° C., preferably for a period from 1 to 15 hours, in particular 2 hours, to obtain said catalyst.