# US 2024/0393546 A1 · Fiber Optic Ferrule and Method for Terminating a Fiber Optic Ferrule to Prevent Delamination

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0393546 A1
- Document ID: US20240393546A1
- Status: Published application
- Kind: A1
- Application number: 18/795,987
- Filed: 2024-08-06
- Published: 2024-11-28
- Earliest claimed: 2020-03-26
- Assignees: US Conec Ltd.
- Applicants: US Conec Ltd.
- Inventors: Dirk E. Schoellner; Darrell R. Childers
- Web page: https://patentgrep.com/patent/US20240393546A1

## CPC

- G02B 6/3861: {Adhesive bonding (adhesives in general C09J)}
- G02B 6/3825: {with an intermediate part, e.g. adapter, receptacle, linking two plugs}
- G02B 6/3849: {using mechanical protective elements, e.g. caps, hoods, sealing membranes (G02B6/3816 takes precedence; provisionally see H01R13/44)}
- G02B 6/3869: {Mounting ferrules to connector body, i.e. plugs}
- G02B 6/4471: {Terminating devices (demountable connectors G02B6/3807); Cable clamps}
- G02B 6/3885: {Multicore or multichannel optical connectors, i.e. one single ferrule containing more than one fibre, e.g. ribbon type (optical ribbon cable G02B6/4403, G02B6/448)}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for terminating a fiber optic ferrule included applying a force to a fiber optic ferrule while simultaneously holding the optical fibers. The fiber optic ferrule uses epoxy to hold the optical fibers, the epoxy can be either heat or light cured. The force is applied through a pusher that engages a cap on the front end of the fiber optic ferrule.

## Claims

### Claim 1

A method to prevent epoxy delamination in a fiber-optic ferrule made of an optically clear material, the fiber-optic ferrule configured to receive optical fibers, the method comprising:
inserting optical fibers into the fiber-optic ferrule;
pre-heating the fiber-optic ferrule;
adding an epoxy to the pre-heated fiber-optic ferrule, wherein the added epoxy covers the inserted optical fibers; and
applying light to the optically clear material for curing the epoxy in the pre-heated fiber-optic ferrule.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the applying light includes using ultraviolet light.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising applying an external force to the fiber-optic ferrule.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the applying the external force is carried out at an end face of the fiber-optic ferrule.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the applied external force causes a compressive force between the optical fibers and one or more fiber stop planes inside the fiber-optic ferrule.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the applying the light is carried out while applying the external force to the fiber-optic ferrule.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the applying the light is carried out while applying an external force to the fiber-optic ferrule.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the external force is applied to the fiber-optic ferrule through a cap to prevent any damage to the fiber-optic ferrule.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the cap has at least one projection to engage a guide pin hole on the fiber-optic ferrule.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the cap compressively engages a resilient member to provide the external force applied to the fiber-optic ferrule.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the applied external force is greater than 0.25 N per optical fiber inserted into the fiber-optic ferrule.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the applied external force is less than 1 N per optical fiber.

### Claim 13 (depends on 8)

The method according to claim 8, wherein the applied external force is greater than an internal force resulting from a thermal expansion of the fiber-optic ferrule, the optical fibers, and the epoxy.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the fiber-optic ferrule is a PRIZM® MT ferrule.

### Claim 15

A method to prevent epoxy delamination in a fiber-optic ferrule made of an optically clear material, the fiber-optic ferrule configured to receive optical fibers, the method comprising:
applying heat to the fiber-optic ferrule;
inserting epoxy into the fiber-optic ferrule via an opening of the fiber-optic ferrule;
inserting optical fibers into the fiber-optic ferrule, wherein the inserted epoxy covers respective ends of the inserted optical fibers; and
applying light from a source to the optically clear material of the fiber-optic ferrule, whereby the applied light cures the inserted epoxy to set the inserted optical fibers inside the fiber-optic ferrule without delamination of the epoxy.

### Claim 16 (depends on 15)

The method according to claim 15, wherein applying the heat is carried out before inserting of the optical fibers.

### Claim 17 (depends on 15)

The method according to claim 15, wherein applying the heat is carried out with the inserting of optical fibers.

### Claim 18 (depends on 15)

The method according to claim 15, wherein applying the heat is carried out prior to applying the light.

### Claim 19 (depends on 15)

The method according to claim 15, wherein the applying the light includes applying ultraviolet light.

### Claim 20 (depends on 15)

The method according to claim 15, further comprising applying an external force to the fiber-optic ferrule to overcome an internal force resulting from a thermal expansion of the fiber-optic ferrule, the inserted optical fibers, and the inserted epoxy.