# US 2024/0392109 A1 · Manufacturing method of low-shrinkage photocurable material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0392109 A1
- Document ID: US20240392109A1
- Status: Published application
- Kind: A1
- Application number: 18/791,956
- Filed: 2024-08-01
- Published: 2024-11-28
- Earliest claimed: 2020-06-02
- Assignees: Phrozen Tech Co., Ltd.
- Applicants: Phrozen Tech Co. Ltd.
- Inventors: Wei-Chun LIN; Yi-Jen WU; Chang-Hsien LI
- Web page: https://patentgrep.com/patent/US20240392109A1

## CPC

- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08J 3/2053: {the additives only being premixed with a liquid phase}
- C08K 3/04: Carbon
- C08K 5/09: Carboxylic acids; Metal salts thereof; Anhydrides thereof
- C08K 5/101: of monocarboxylic acids
- C08K 5/20: Carboxylic acid amides
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A low-shrinkage photocurable material is provided in the present disclosure. The low-shrinkage photocurable material includes an acrylonitrile butadiene styrene resin, a carbon black and a dispersant. The carbon black and the dispersant are mixed with the acrylonitrile butadiene styrene resin. The weight percentage of the acrylonitrile butadiene styrene resin is 85%-99.45%, the weight percentage of the carbon black is 0.05%-5%, and the weight percentage of the dispersant is 0.5%-10%.

## Claims

### Claim 1

A manufacturing method of a low-shrinkage photocurable material, comprising:
providing an acrylonitrile butadiene styrene resin;
providing a carbon black solution comprising a carbon black, a dispersant and a solvent; and
performing a mixing step to mix the acrylonitrile butadiene styrene resin and the carbon black solution, so as to obtain the low-shrinkage photocurable material;
wherein the weight percentage of the acrylonitrile butadiene styrene resin is 85%-99.45%, the weight percentage of the carbon black is 0.05%-5%, and the weight percentage of the dispersant is 0.5%-10%.

### Claim 2 (depends on 1)

The manufacturing method of the low-shrinkage photocurable material of claim 1, wherein the carbon black is a surface-modified carbon black material.

### Claim 3 (depends on 1)

The manufacturing method of the low-shrinkage photocurable material of claim 1, wherein the dispersant is a methyl methacrylate, a derivative of methyl methacrylate, a mixture with methyl methacrylate, a dimethylacetamide or a mixture with dimethylacetamide.

### Claim 4 (depends on 1)

The manufacturing method of the low-shrinkage photocurable material of claim 1, further comprising:
providing a solution of carbon black raw material, wherein the solution of carbon black raw material is prepared by mixing a carbon black raw material, a 2,4-diisocyanato-1-methyl-benzene, a dibutyltin dilaurate and a dimethylformide;
providing a polyethylene glycol-molecular sieve reactant by keeping a polyethylene glycol and a dimethylformide in a molecular sieve;
performing a carbon black pretreating step by mixing and stirring the solution of carbon black raw material, the polyethylene glycol-molecular sieve reactant and a dimethylol propionic acid, so as to obtain a substance for purification; and
performing a purifying step to purify the substance for purification, so as to obtain the carbon black.

### Claim 5 (depends on 4)

The manufacturing method of the low-shrinkage photocurable material of claim 4, wherein a weight ratio of the carbon black raw material, the 2,4-diisocyanato-1-methyl-benzene, the polyethylene glycol and the dimethylol propionic acid is 1:10:17:0.6 to 1:28:50:2.

### Claim 6 (depends on 4)

The manufacturing method of the low-shrinkage photocurable material of claim 4, wherein the solution of carbon black raw material and the polyethylene glycol-molecular sieve reactant are first mixed and stirred for a first reaction time, and then the dimethylol propionic acid is added and stirred for a second reaction time in the carbon black pretreating step.

### Claim 7 (depends on 6)

The manufacturing method of the low-shrinkage photocurable material of claim 6, wherein the first reaction time and the second reaction time are both 1 hour to 3 hours.