# US 2024/0391822 A1 · Thermochromic film and method for manufacturing thermochromic film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0391822 A1
- Document ID: US20240391822A1
- Status: Published application
- Kind: A1
- Application number: 18/685,672
- Filed: 2022-08-23
- Published: 2024-11-28
- Earliest claimed: 2021-08-23
- Assignees: Korea Institute of Industrial Technology
- Applicants: Korea Institute of Industrial Technology
- Inventors: Kwang Seok KIM; Jung Pil KIM; Myoung Hun KIM
- Web page: https://patentgrep.com/patent/US20240391822A1

## CPC

- C03C 17/25: by deposition from the liquid phase
- B29D 11/00: Producing optical elements, e.g. lenses or prisms (grinding or polishing of optical elements B24B; constructional form of optical elements G02B; {optical parts of spectacles G02C7/00})
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C09D 5/26: Thermosensitive paints
- C09D 11/50: Sympathetic, colour changing or similar inks
- G02F 1/00: Devices or arrangements for the control of the intensity, colour, phase, polarisation or direction of light arriving from an independent light source, e.g. switching, gating or modulating; Non-linear optics
- G02F 1/01: for the control of the intensity, phase, polarisation or colour (G02F1/29, G02F1/35 take precedence)
- G02F 1/0147: {based on thermo-optic effects (G02F1/132 takes precedence)}
- C03C 2217/218: V2O5, Nb2O5, Ta2O5
- C03C 2218/11: from solutions or suspensions
- C03C 2218/116: by spin-coating, centrifugation
- C03C 2218/32: After-treatment
- G02F 2201/56: Substrates having a particular shape, e.g. non-rectangular
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

The present invention provides a thermochromic film in which vanadium dioxide can be used without a doping process after the phase transition temperature thereof is reduced, and thus, there are economic and environmental advantages, and a method for manufacturing a thermochromic film, the method comprising: a formation step of forming a coating layer by applying a solution including untreated vanadium oxide onto a substrate; and a formation step of forming a thermochromic layer by phase change of untreated vanadium oxide to vanadium dioxide through annealing using intense pulsed light (IPL).

## Claims

### Claim 1

A thermochromic film comprising:
a substrate having heat shrinkability; and
a thermochromic layer whose phase transition temperature changes due to heat shrinkage of the substrate and which is formed on the substrate.

### Claim 2 (depends on 1)

The thermochromic film of claim 1, wherein the phase transition temperature of the thermochromic layer decreases during heat shrinkage of the substrate.

### Claim 3 (depends on 1)

The thermochromic film of claim 1, wherein the substrate has a curved surface, wherein the curvature of the curved surface is gently deformed during the heat shrinkage.

### Claim 4 (depends on 1)

The thermochromic film of claim 1, wherein the substrate includes a shape memory polymer (SMP).

### Claim 5 (depends on 4)

The thermochromic film of claim 4, wherein the shape memory polymer has a glass transition temperature of 30° C. or more.

### Claim 6 (depends on 4)

The thermochromic film of claim 4, wherein the shape memory polymer is a urethane-based shape memory polymer.

### Claim 7 (depends on 1)

The thermochromic film of claim 1, wherein the thermochromic layer includes vanadium oxide.

### Claim 8 (depends on 1)

The thermochromic film of claim 1, wherein the substrate has a thickness ranging from 50 to 200 μm.

### Claim 9 (depends on 1)

The thermochromic film of claim 1, wherein a layered product has a maximum transmittance of 50% or more in the range of 400 to 800 nm.

### Claim 10 (depends on 1)

The thermochromic film of claim 1, wherein the layered product has a minimum transmittance of 70% or less in the range of 2,000 to 3,000 nm at any temperature greater than or equal to the critical temperature.

### Claim 11 (depends on 1)

The thermochromic film of claim 1, wherein the layered product satisfies the conditions of the following General Expression 1:
ΔIR=BPmin−Opmin≥10% [General Expression 1]
wherein BPmin represents the minimum transmittance in the range of 2,000 to 3,000 nm at any temperature less than or equal to the critical temperature, and OPmin represents the minimum transmittance in the range of 2,000 to 3,000 nm at any temperature greater than or equal to the critical temperature.

### Claim 12

A method of manufacturing a thermochromic film, comprising:
a formation step of forming a coating layer by applying a solution including untreated vanadium oxide (VOx) onto a substrate; and
a preparation step of preparing a thermochromic layer by phase-changing the untreated vanadium oxide (VOx) to vanadium dioxide (VO2) through annealing using intense pulsed light (IPL).

### Claim 13 (depends on 12)

The method of claim 12, wherein the untreated vanadium oxide (VOx) is vanadium pentoxide (V2O5).

### Claim 14 (depends on 12)

The method of claim 12, wherein the annealing is performed in a vacuum or air atmosphere.

### Claim 15 (depends on 14)

The method of claim 14, wherein the output voltage of the intense pulsed light in a vacuum atmosphere ranges from 1,500 to 1,900 V.

### Claim 16 (depends on 14)

The method of claim 14, wherein the output voltage of the intense pulsed light in an air atmosphere ranges from 1,700 to 2,000 V.

### Claim 17 (depends on 14)

The method of claim 14, wherein the annealing is performed by repetitive light irradiation with a constant pulse interval and pulse width.

### Claim 18 (depends on 16)

The method of claim 16, wherein the pulse width in a vacuum atmosphere ranges from 1 to 4 ms.

### Claim 19 (depends on 16)

The method of claim 16, wherein the pulse interval in a vacuum atmosphere ranges from 0.2 to 1 Hz.

### Claim 20 (depends on 16)

The method of claim 16, wherein the number of repetitions in a vacuum atmosphere ranges from 20 to 200.

### Claim 21 (depends on 16)

The method of claim 16, wherein the pulse width in an air atmosphere ranges from 0.1 to 1 ms or less.

### Claim 22 (depends on 16)

The method of claim 16, wherein the pulse interval in an air atmosphere ranges from 1.0 to 3.0 Hz.

### Claim 23 (depends on 16)

The method of claim 16, wherein the number of repetitions in an air atmosphere ranges from 200 to 400.

### Claim 24 (depends on 12)

The method of claim 12, wherein the substrate is a glass, quartz, or polymer film.

### Claim 25 (depends on 24)

The method of claim 24, wherein the polymer film includes a polymer having a glass transition temperature of 70° C. or more.

### Claim 26 (depends on 12)

The method of claim 12, wherein the coating layer has a thickness of 10 to 300 nm or less.

### Claim 27 (depends on 12)

The method of claim 12, wherein the untreated vanadium oxide (VOx) has an average particle size of 1 to 40 nm or less.