# US 2024/0391779 A1 · Silicon carbon composite material and preparation method thereof, negative electrode material, negative electrode plate, electrode assembly, battery, electric equipment, and carbon substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0391779 A1
- Document ID: US20240391779A1
- Status: Published application
- Kind: A1
- Application number: 18/795,082
- Filed: 2024-08-05
- Published: 2024-11-28
- Earliest claimed: 2022-07-27
- Assignees: Contemporary Amperex Technology Co., Limited
- Applicants: Contemporary Amperex Technology Co., Limited
- Inventors: Yuan LI; Xiaobin DONG; Zijian LV; Liangbin LIU; Jiazheng WANG
- Web page: https://patentgrep.com/patent/US20240391779A1

## CPC

- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/364: {as mixtures}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- C01P 2002/08: Intercalated structures, i.e. with atoms or molecules intercalated in their structure
- C01P 2004/03: obtained by SEM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A silicon carbon composite material includes a carbon matrix and a silicon material, the carbon matrix has a cross-linked porous structure internally, and the silicon material is at least partially distributed in the cross-linked porous structure. A value of flexibility C1 of the silicon carbon composite material satisfies 0.4≤C1≤2. C1 is a factor by which a compression deformation variable of the silicon carbon composite material is scaled to be equal to its rebound deformation variable, representing flexibility of the silicon carbon composite material. When the C1 value satisfies 0.4≤C1≤2, the silicon carbon composite material has good flexibility, reducing overall impact of expansion stress of silicon on the silicon carbon composite material, and allowing for a certain degree of contractility of the carbon matrix framework, so that residual stress can be received and released, thereby maintaining overall stability of the silicon carbon composite material.

## Claims

### Claim 1

A silicon carbon composite material, comprising:
a carbon matrix having a cross-linked porous structure internally; and
a silicon material that is at least partially distributed in the cross-linked porous structure; and
wherein a value of flexibility C1 of the silicon carbon composite material satisfies 0.4≤C1≤2, the flexibility being measured by
applying a pressure of 2t to the silicon carbon composite material, holding the pressure for 10s and releasing the pressure for 100s, repeating until the pressure is held and released for 20 times, recording a compacted density P1 at the 1st pressure holding, a compacted density P2 at the 20th pressure holding, a compacted density P3 at the 1st pressure releasing, and a compacted density P4 at the 20th pressure releasing, and calculating C1=(P4−P3)/(P2−P1).

### Claim 2 (depends on 1)

The silicon carbon composite material according to claim 1, wherein 0.8≤C1≤2.

### Claim 3 (depends on 1)

The silicon carbon composite material according to claim 1, wherein P2−P1 is defined as M1 and P4−P3 is defined as N1, wherein 0.05≤M1≤0.18 and 0.08≤N1≤0.2; or wherein 0.08≤M1≤0.15 and 0.10≤N1≤0.18.

### Claim 4 (depends on 1)

The silicon carbon composite material according to claim 1, wherein the carbon matrix comprises a first region and a second region in sequence along a direction extending from a center to a surface, and the carbon matrix is composed of the first region and the second region, wherein a volume of the second region is twice a volume of the first region, and
a ratio of a number of pores with a pore size of 2 nm to 1000 nm in the first region to a number of pores with a pore size of 2 nm to 1000 nm in the second region is greater than 1; or
a ratio of a number of pores with a pore size of 2 nm to 500 nm in the first region to a number of pores with a pore size of 2 nm to 500 nm in the second region is greater than 1; or
a ratio of a number of pores with a pore size of 2 nm to 200 nm in the first region to a number of pores with a pore size of 2 nm to 200 nm in the second region is greater than 1.

### Claim 5 (depends on 1)

The silicon carbon composite material according to claim 1, wherein a specific surface area (SSA) value of the silicon carbon composite material satisfies 1 cm2/g≤SSA≤10 cm2/g; or
the SSA of the silicon carbon composite material satisfies 3 cm2/g≤SSA≤7 cm2/g.

### Claim 6 (depends on 1)

The silicon carbon composite material according to claim 1, wherein the silicon carbon composite material satisfies Dv10≤5 μm, Dv50≤8 μm, Dv90≤20 μm, and (Dv90−Dv10)/Dv50≥1.6.

### Claim 7 (depends on 1)

The silicon carbon composite material according to claim 1, wherein a powder compacted density PD of the silicon carbon composite material under a pressure of 5t is ≤1.1 g/cm3.

### Claim 8 (depends on 1)

The silicon carbon composite material according to claim 1, wherein the silicon material comprises any one or more of a silicon-oxygen compound, elemental silicon, or a silicon alloy.

### Claim 9 (depends on 1)

A preparation method for the silicon carbon composite material according to claim 1, wherein the preparation method for silicon carbon composite material comprises: subjecting raw materials to first heat treatment to produce a solid resin, subjecting the solid resin to second heat treatment to volatilize a neutral solvent and produce a carbon precursor, subjecting the carbon precursor to pyrolysis and carbonization treatment to produce the carbon matrix, and incorporating the silicon material into the cross-linked porous structure of the carbon matrix; and
wherein the raw materials comprise a resin, a porogen, and the neutral solvent.

### Claim 10 (depends on 9)

The preparation method for silicon carbon composite material according to claim 9, wherein the second heat treatment is conducted at a treatment temperature of 150° C. to 400° C. for a treatment time of at least 10 hours.

### Claim 11 (depends on 9)

The preparation method for silicon carbon composite material according to claim 9, wherein a mass ratio of the resin to the neutral solvent ranges from 1:10 to 10:1, and a mass ratio of the resin to the porogen ranges from 1:5 to 10:1;
the resin comprises any one or more of phenolic resin, epoxy resin, or polyurethane;
the neutral solvent comprises any one or more of methanol, ethanol, ethylene glycol, polyethylene glycol, glycerol, or isopropanol; and
the porogen comprises any one or more of potassium chloride, sodium chloride, zinc chloride, sodium hydroxide, potassium hydroxide, sodium carbonate, potassium carbonate, sodium bicarbonate, phosphoric acid, sodium acetate, zinc acetate, nickel acetate, or ammonium acetate.

### Claim 12 (depends on 9)

The preparation method for silicon carbon composite material according to claim 9, wherein the first heat treatment comprises standing at 60° C. to 150° C. for at least 10 hours.

### Claim 13 (depends on 9)

The preparation method for silicon carbon composite material according to claim 9, wherein the pyrolysis and carbonization treatment comprises sintering at 600° C. to 1600° C. for 1 to 3 hours; and
the pyrolysis and carbonization treatment is conducted at a temperature of 800° C. to 1000° C.

### Claim 14 (depends on 1)

A negative electrode material, wherein the negative electrode material comprises the silicon carbon composite material according to claim 1.

### Claim 15 (depends on 14)

A negative electrode plate, wherein the negative electrode plate comprises the negative electrode material according to claim 14.

### Claim 16 (depends on 15)

An electrode assembly, wherein the electrode assembly comprises the negative electrode plate according to claim 15.

### Claim 17 (depends on 16)

A battery cell, wherein the battery cell comprises the electrode assembly according to claim 16.

### Claim 18 (depends on 17)

A battery, wherein the battery comprises the battery cell according to claim 17.

### Claim 19 (depends on 18)

An electric apparatus, wherein the electric apparatus comprises the battery according to claim 18, wherein the battery is configured to supply electric energy.

### Claim 20

A carbon matrix, wherein the carbon matrix has a cross-linked porous structure internally, and a value of flexibility C2 of the carbon matrix satisfies 0.8≤C2≤2 or 1.2≤C2≤1.8, the flexibility being measured by applying a pressure of 2t to the carbon matrix, holding the pressure for 10s and releasing the pressure for 100s, repeating until the pressure is held and released for 20 times, recording a compacted density P5 at the 1st pressure holding, a compacted density P6 at the 20th pressure holding, a compacted density P7 at the 1st pressure releasing, and a compacted density P8 at the 20th pressure releasing, and calculating C2=(P8−P7)/(P6−P5),
wherein M2 is defined as P6−P5, and N2 is defined as P8−P7, wherein 0.04≤M2≤0.18 and 0.04≤N2≤0.08; or wherein the carbon matrix comprises a first region and a second region in sequence along a direction extending from a center to a surface, wherein a volume of the second region is twice a volume of the first region, and a ratio of a number of pores with a pore size of 2 nm to 1000 nm in the first region to a number of pores with a pore size of 2 nm to 1000 nm in the second region is greater than 1;
or wherein a ratio of a number of pores with a pore size of 2 nm to 500 nm in the first region to a number of pores with a pore size of 2 nm to 500 nm in the second region is greater than 1;
or wherein a ratio of a number of pores with a pore size of 2 nm to 200 nm in the first region to a number of pores with a pore size of 2 nm to 200 nm in the second region is greater than 1.