# US 2024/0391009 A1 · Solder-free joint and welding method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0391009 A1
- Document ID: US20240391009A1
- Status: Published application
- Kind: A1
- Application number: 18/694,422
- Filed: 2022-03-23
- Published: 2024-11-28
- Earliest claimed: 2021-09-24
- Assignees: Shanghai Jiao Tong University
- Applicants: Shanghai Jiao Tong University
- Inventors: Zhen HUANG
- Web page: https://patentgrep.com/patent/US20240391009A1

## CPC

- B23K 1/203: {Fluxing, i.e. applying flux onto surfaces}
- B23K 1/0016: {Soldering of electronic components}
- B23K 1/19: taking account of the properties of the materials to be soldered
- B23K 20/00: Non-electric welding by applying impact or other pressure, with or without the application of heat, e.g. cladding or plating
- B23K 2101/38: Conductors
- B23K 2103/12: Copper or alloys thereof
- Y02E 40/60: Superconducting electric elements or equipment; Power systems integrating superconducting elements or equipment
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A solder-free joint and a welding method thereof are provided. The welding method includes the following steps: S1: uniformly coating a flux on a surface of each of a plurality of materials to be soldered, thereby forming a flux layer; S2: performing binding according to the surface of the material, the flux layer, and the surface of the material; and S3: putting the materials into a hot-pressing device, and setting a desired pressure and temperature for soldering. In pretreatment before soldering, the welding method does not add any solder. The obtained solder-free joint has a desirable conductivity and desirable mechanical properties.

## Claims

### Claim 1

A welding method of a solder-free joint, comprising the following steps:
S1: coating a flux on a surface of each of a plurality of materials to be soldered, thereby forming a flux layer;
S2: performing face-to-face binding on the flux-coated surfaces of the materials; and
S3: setting a desired pressure and a desired temperature for hot-pressing soldering.

### Claim 2

A welding method of a solder-free joint, comprising the following steps:
step 1: cutting two superconducting tapes with an appropriate length;
step 2: uniformly coating a flux on a superconducting surface of each of the two superconducting tapes, wherein the superconducting surface is adjacent to a superconducting layer;
step 3: binding the superconducting surfaces of the two superconducting tapes;
step 4: putting the two superconducting tapes into a hot-pressing device; and
step 5: setting a desired pressure and a desired temperature.

### Claim 3 (depends on 2)

The welding method according to claim 2, wherein the superconducting surfaces are bound and aligned in step 3.

### Claim 4 (depends on 1)

The welding method according to claim 1, wherein pressurization is performed between pressure members of a hot-pressing device to obtain the desired pressure, and heating is performed to obtain the desired temperature; there is no chronological sequence between the pressurization and the heating; and the heating and the pressurization are also allowed to be performed simultaneously.

### Claim 5 (depends on 1)

The welding method according to claim 1, wherein the desired pressure is 10 MPa or above, and the desired temperature is 37° C. or above.

### Claim 6 (depends on 5)

The welding method according to claim 5, wherein the desired pressure is 84 MPa to 420 MPa, and the desired temperature is 190° C. to 260° C.

### Claim 7 (depends on 1)

The welding method according to claim 1, wherein the flux is used to remove an oxidation layer on the surface of each of the materials, such that an energy spectrum of Cu2p on the surface of each of the materials contains less than or equal to two peaks.

### Claim 8 (depends on 1)

The welding method according to claim 1, wherein each of the plurality of materials is a superconducting tape, a conductor with a metal surface and/or an alloy surface and/or a graphite surface, or a semiconductor material.

### Claim 9 (depends on 8)

The welding method according to claim 8, wherein the superconducting tape is a second-generation superconducting tape, with a surface being a copper layer.

### Claim 10 (depends on 1)

A solder-free joint obtained with the welding method according to claim 1.

### Claim 11 (depends on 2)

The welding method according to claim 2, wherein pressurization is performed between pressure members of the hot-pressing device to obtain the desired pressure, and heating is performed to obtain the desired temperature; there is no chronological sequence between the pressurization and the heating; and the heating and the pressurization are also allowed to be performed simultaneously.

### Claim 12 (depends on 2)

The welding method according to claim 2, wherein the desired pressure is 10 MPa or above, and the desired temperature is 37° C. or above.

### Claim 13 (depends on 2)

The welding method according to claim 2, wherein the flux is used to remove an oxidation layer on a surface of a material, such that an energy spectrum of Cu2p on the surface of the material contains less than or equal to two peaks.

### Claim 14 (depends on 2)

A solder-free joint obtained with the welding method according to claim 2.

### Claim 15 (depends on 14)

The solder-free joint according to claim 14, wherein the superconducting surfaces are bound and aligned in step 3.

### Claim 16 (depends on 10)

The solder-free joint according to claim 10, wherein pressurization is performed between pressure members of a hot-pressing device to obtain the desired pressure, and heating is performed to obtain the desired temperature; there is no chronological sequence between the pressurization and the heating; and the heating and the pressurization are also allowed to be performed simultaneously.

### Claim 17 (depends on 10)

The solder-free joint according to claim 10, wherein the desired pressure is 10 MPa or above, and the desired temperature is 37° C. or above.

### Claim 18 (depends on 17)

The solder-free joint according to claim 17, wherein the desired pressure is 84 MPa to 420 MPa, and the desired temperature is 190° C. to 260° C.

### Claim 19 (depends on 10)

The solder-free joint according to claim 10, wherein the flux is used to remove an oxidation layer on the surface of each of the materials, such that an energy spectrum of Cu2p on the surface of each of the materials contains less than or equal to two peaks.

### Claim 20 (depends on 10)

The solder-free joint according to claim 10, wherein each of the plurality of materials is a superconducting tape, a conductor with a metal surface and/or an alloy surface and/or a graphite surface, or a semiconductor material.