# US 2024/0384430 A1 · Functionally graded alloy coating and method for preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0384430 A1
- Document ID: US20240384430A1
- Status: Published application
- Kind: A1
- Application number: 18/637,817
- Filed: 2024-04-17
- Published: 2024-11-21
- Earliest claimed: 2023-05-17
- Assignees: Faraday Technology Corp.
- Applicants: Faraday Technology, Inc.
- Inventors: Timothy D. Hall; Rajeswaran Radhakrishnan; Holly Garich; Katherine Lee
- Web page: https://patentgrep.com/patent/US20240384430A1

## CPC

- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 3/562: {containing more than 50% by weight of iron or nickel or cobalt}
- C25D 5/36: of iron or steel
- C25D 5/38: of refractory metals or nickel
- C25D 5/50: by heat-treatment
- C25D 5/617: {Crystalline layers}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method, coated substrate, and coating wherein a metallic substrate is subject to an electrolytic deposition process including an electrolyte with an iron group element and a refractory group element. One or more electrolytic deposition waveform parameters are varied to deposit on the substrate a functionally graded coating with more of the iron group element and less of the refractory group element at an interface between the coating and the metallic substrate to better match the coefficient of thermal expansion of the coating and the metallic substrate and more of the refractory group element and less of the iron group element as the thickness of the coating increases for improving corrosion resistance to salts. The coating may be diffusion bonded to the substrate.

## Claims

### Claim 1

A method of coating a metallic substrate, the method comprising:
subjecting the metallic substrate to an electrolytic deposition process including an electrolyte with an iron group element and a refractory group element;
varying one or more electrolytic deposition waveform parameters to deposit on the substrate a functionally graded coating with more of the iron group element and less of the refractory group element at an interface between the coating and the metallic substrate to better match the coefficient of thermal expansion of the coating and the metallic substrate and more of the refractory group element and less of the iron group element as the thickness of the coating increases for improving corrosion resistance to salts; and
diffusion bonding the coating to the substrate.

### Claim 2 (depends on 1)

The method of claim 1 in which the waveform parameters vary from a waveform that preferentially influences the iron group element to transport to the substrate and to deposit on the substrate to a waveform that preferentially influences the refractory group element to transport to the substrate and to deposit on the substrate.

### Claim 3 (depends on 2)

The method of claim 2 in which varying the electrolytic waveform parameters includes varying the current density of the waveform, the length of time the waveform is applied, and the time between successive waveforms.

### Claim 4 (depends on 3)

The method of claim 3 in which varying the electrolytic waveform parameters further includes switching between cathodic and anodic waveforms.

### Claim 5 (depends on 1)

The method of claim 1 further including increasing the roughness of the substrate before deposition.

### Claim 6 (depends on 1)

The method of claim 1 further including activating the substrate.

### Claim 7 (depends on 6)

The method of claim 6 wherein the activation is accomplished by nickel strike, acid etch, or plasma treatment.

### Claim 8 (depends on 1)

The method of claim 1 wherein the substrate is a stainless steel material or tungsten.

### Claim 9 (depends on 1)

The method of claim 1 wherein the CTE of the functionally graded coating is lower than that of the substrate.

### Claim 10 (depends on 1)

The method of claim 1 wherein the iron group includes Fe, Co and/or Ni and the refractory group includes Mo, W, and/or Re.

### Claim 11 (depends on 1)

The method of claim 1 wherein the functionally graded coating adjacent the substrate interface comprises 90+% of the iron group and the functionally graded coating at its surface comprises between 25 and 60% of the refractory group.

### Claim 12 (depends on 1)

The method of claim 1 wherein the diffusion bonding is accomplished by hot isostatic pressing.

### Claim 13 (depends on 12)

The method of claim 12 wherein the hot isostatic pressing is conducted for about 3½ hours at about 1250 C and at about 22,000 psi pressure.

### Claim 14

A metallic substrate coated with a functionally graded diffusion bonded coating with more of an iron group element and less of a refractory group element at an interface between the metallic substrate and the coating to better match the coefficient of thermal expansion of the coating and the metallic substrate and more of the refractory group element and less of the iron group element as the thickness of the coating increases for improving corrosion resistance to salts.

### Claim 15

A coating for a metallic substrate comprising:
more of an iron group element and less of a refractory group element at a coating interface to better match the coefficient of thermal expansion of the coating and a metallic substrate and more of the refractory group element and less of the iron group element as the thickness of the coating increases for improving corrosion resistance to salts.

### Claim 16

A method of coating a metallic substrate, the method comprising:
subjecting the metallic substrate to an electrolytic deposition process including an electrolyte solution with an iron group element and a refractory group element; and
instead of changing the electrolyte solution, varying one or more electrolytic deposition waveform parameters to deposit on the substrate a functionally graded coating with more of the iron group element and less of the refractory group element at a first portion of the coating more of the refractory group element and less of the iron group element at a second portion of the coating.

### Claim 17 (depends on 16)

The method of claim 16 in which the first portion of the coating is at an interface between the coating and the substrate and the second portion of the coating is at the surface of the coating.

### Claim 18 (depends on 17)

The method of claim 17 in which the waveform parameters vary from a waveform that preferentially influences the iron group element to transport to the substrate and to deposit on the substrate to a waveform that preferentially influences the refractory group element to transport to the substrate and to deposit on the substrate.

### Claim 19 (depends on 18)

The method of claim 18 in which varying the electrolytic waveform parameters includes varying the current density of the waveform, the length of time the waveform is applied, and the time between successive waveforms.

### Claim 20 (depends on 19)

The method of claim 19 in which varying the electrolytic waveform parameters further includes switching between cathodic and anodic waveforms.

### Claim 21 (depends on 16)

The method of claim 16 further including increasing the roughness of the substrate before deposition.

### Claim 22 (depends on 16)

The method of claim 16 further including activating the substrate.

### Claim 23 (depends on 22)

The method of claim 22 wherein the activation is accomplished by nickel strike, acid etch, or plasma treatment.

### Claim 24 (depends on 16)

The method of claim 16 wherein the substrate is a stainless steel material or tungsten.

### Claim 25 (depends on 16)

The method of claim 16 wherein the CTE of the functionally graded coating is lower than that of the substrate.

### Claim 26 (depends on 16)

The method of claim 16 wherein the iron group includes Fe, Co and/or Ni and the refractory group includes Mo, W, and/or Re.

### Claim 27 (depends on 17)

The method of claim 17 wherein the functionally graded coating adjacent the substrate interface comprises 90+% of the iron group and the functionally graded coating at its surface comprises between 25 and 60% of the refractory group.

### Claim 28 (depends on 16)

The method of claim 16 further including diffusion bonding the coating to the substrate.

### Claim 29 (depends on 28)

The method of claim 28 wherein diffusion bonding includes hot isostatic pressing for about 3½ hours at about 1250 C and at about 22,000 psi pressure.

### Claim 30

A method of coating a metallic substrate, the method comprising:
subjecting the metallic substrate to an electrolytic deposition process including an electrolyte solution with an iron group element and a refractory group element; and
instead of changing the electrolyte solution, varying one or more electrolytic deposition waveform parameters to deposit on the substrate a functionally graded coating with more of the iron group element and less of the refractory group element at a first portion of the coating more of the refractory group element and less of the iron group element at a second portion of the coating in which the waveform parameters vary from a waveform that preferentially influences the iron group element to transport to the substrate and to deposit on the substrate to a waveform that preferentially influences the refractory group element to transport to the substrate and to deposit on the substrate.