# US 2024/0383760 A1 · Surface-treated silica particle dispersion sol and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0383760 A1
- Document ID: US20240383760A1
- Status: Published application
- Kind: A1
- Application number: 18/694,009
- Filed: 2022-10-13
- Published: 2024-11-21
- Earliest claimed: 2021-10-18
- Assignees: Mitsubishi Materials Electronic Chemicals Co., Ltd.
- Applicants: Mitsubishi Materials Electronic Chemicals Co., Ltd.
- Inventors: Yuta Yamamoto
- Web page: https://patentgrep.com/patent/US20240383760A1

## CPC

- C01B 33/149: Coating
- C01B 33/12: Silica; Hydrates thereof, e.g. lepidoic silicic acid
- C01B 33/145: Preparation of hydroorganosols, organosols or dispersions in an organic medium
- C01B 33/146: After-treatment of sols ({preparation of hydrosols or aqueous dispersions from hydroorganosols, organosols or dispersions in an organic medium C01B33/141}; preparation of hydroorganosols, organosols or dispersions in an organic medium from hydrosols {or aqueous dispersions} C01B33/145)
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C09D 5/006: {Anti-reflective coatings}
- C09D 7/62: modified by treatment with other compounds
- C09D 7/67: {Particle size smaller than 100 nm}
- C09D 7/70: {characterised by shape, e.g. fibres, flakes or microspheres}
- C01B 33/18: Preparation of finely divided silica neither in sol nor in gel form; After-treatment thereof (preparation of aerogels by dehydrating gels C01B33/158; treatment to enhance the pigmenting or filling properties C09C)
- C01P 2004/03: obtained by SEM
- C01P 2004/32: Spheres
- C01P 2004/54: Particles characterised by their aspect ratio, i.e. the ratio of sizes in the longest to the shortest dimension
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/80: Compositional purity
- C08K 3/36: Silica
- C08K 9/06: with silicon-containing compounds
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

This surface-treated silica particle dispersion sol is formed by dispersing a group of colloidal silica particles in a hydrophobic solvent, the colloidal silica particles being composed of an average number of 4 to 300 spherical primary particles, chainly connected to have an average length of 35 nm to 1,800 nm, and the particle surfaces being coated with a silane coupling agent or the like having a functional group such as a vinyl group. The average particle diameter of the spherical primary particles is 6 nm to 20 nm and the average aspect ratio of the spherical primary particles is in the range of 1.0 to 1.3. The content ratio of impurities of K, Na, or NH3 per colloidal silica particle is 3,500 ppm by mass or less and the content ratio of impurities of alkaline earth metals or aluminum is less than 1 ppm by mass.

## Claims

### Claim 1

A surface-treated silica particle dispersion sol formed by dispersing a group of colloidal silica particles in a hydrophobic solvent, the colloidal silica particles being composed of an average number of 4 to 300 spherical primary particles, as observed with a field emission-type scanning electron microscope, chainly connected to have an average length of 35 nm to 1,800 nm, and the surfaces of the particles being coated with a silane coupling agent having a functional group which is a vinyl group, a methyl group, an epoxy group, a styryl group, or a methacrylic group, or coated with a titanate-based coupling agent or an aluminate-based coupling agent,
wherein an average particle diameter of the spherical primary particles is 6 nm to 20 nm,
an average aspect ratio of the spherical primary particles is in a range of 1.0 to 1.3,
a content ratio of each of impurities of K, Na, or NH3 per the colloidal silica particle is 3,500 ppm by mass or less, and
a content ratio of each of impurities of an alkaline earth metal or aluminum is less than 1 ppm by mass.

### Claim 2 (depends on 1)

A method for producing the surface-treated silica particle dispersion sol according to claim 1, the method comprising:
(a) a step of obtaining an alkyl silicate solution by mixing an alkyl silicate having an alkyl group having 1 to 2 carbon atoms in a mixed solvent of pure water and an organic solvent that is an alcohol having 1 to 4 carbon atoms or a water-soluble glycol compound having 2 to 4 carbon atoms;
(b) a step of obtaining a raw material liquid by adding and mixing an alkaline catalyst, which is an alkali metal hydroxide, ammonia, or an alkylamine, in the alkyl silicate solution;
(c) a step of obtaining a first precursor sol in which colloidal silica particles are dispersed by heating the raw material liquid at 40° C. to 100° C. for 24 hours to 100 hours;
(d) a step of obtaining an alcohol-diluted sol by adding and mixing an alcohol having 1 to 4 carbon atoms in the first precursor sol;
(e) a step of obtaining a second precursor sol in which surface-treated silica particles are dispersed by adding and mixing, in the alcohol-diluted sol, a surface treatment agent that is a silane coupling agent having a functional group which is a vinyl group, a methyl group, an epoxy group, a styryl group, or a methacrylic group, or a surface treatment agent that is a titanate-based coupling agent or an aluminate-based coupling agent, in a ratio of 10% by mass to 100% by mass, when the silica particles in the alcohol-diluted sol are set to 100% by mass, and carrying out heating at 40° C. to 100° C. for 3 hours to 24 hours; and
(f) a step of substituting the solvent by adding and mixing a hydrophobic solvent in the second precursor sol such that a silica concentration in the second precursor sol is set to 1% by mass to 25% by mass, and carrying out heating at 40° C. to 80° C. for 3 hours to 12 hours,
wherein the pure water is included in a ratio of 8 molar concentration to 23 molar concentration with respect to Si in the alkyl silicate,
the alkyl silicate is mixed at a ratio of 18% by mass to 44% by mass when the alkyl silicate solution is set to 100% by mass in the step (a), and
the alkaline catalyst is mixed at a ratio of 0.02% by mass to 0.40% by mass with respect to silica when converting the alkyl silicate into the silica in the step (b).

### Claim 3 (depends on 2)

The method for producing the surface-treated silica particle dispersion sol according to claim 2,
wherein spherical primary particles having an average aspect ratio of 1.0 to 1.1 and an average particle diameter of less than 5 nm are formed in an initial heating stage of the step (c) and, when the heating ends, the spherical primary particles in the initial heating stage have an average particle diameter of 6 nm to 20 nm and are linked in a chainlike shape having an average number of 4 to 300 particles to form a group of colloidal silica particles having an average length of 35 nm to 1,800 nm.

### Claim 4 (depends on 1)

A film obtained using the surface-treated silica particle dispersion sol according to claim 1,
wherein the film has a refractive index of 1.10 to 1.25.