# US 2024/0375395 A1 · Method for laminating a building panel core with a self-adhesive use layer and building panel core laminated with a self-adhesive use layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0375395 A1
- Document ID: US20240375395A1
- Status: Published application
- Kind: A1
- Application number: 18/690,493
- Filed: 2022-09-14
- Published: 2024-11-14
- Earliest claimed: 2021-09-15
- Assignees: wedi GmbH
- Applicants: Wedi GmbH
- Inventors: Stephan Wedi
- Web page: https://patentgrep.com/patent/US20240375395A1

## CPC

- B32B 37/0015: {to avoid warp or curl}
- B32B 37/26: with at least one layer which influences the bonding during the lamination process, e.g. release layers or pressure equalising layers
- B32B 37/0053: {Constructional details of laminating machines comprising rollers; Constructional features of the rollers}
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/12: characterised by using adhesives
- B32B 37/142: {Laminating of sheets, panels or inserts, e.g. stiffeners, by wrapping in at least one outer layer, or inserting into a preformed pocket}
- B32B 37/18: involving the assembly of discrete sheets or panels only
- B32B 37/226: {Laminating sheets, panels or inserts between two continuous plastic layers}
- B32B 38/0004: {Cutting, tearing or severing, e.g. bursting; Cutter details (cutting in general B26D; laminating combined with punching or perforating B32B38/04; removing all or part of the layers B32B38/10; cutting in combination with laying up and registration B32B38/185 takes precedence)}
- B32B 38/10: Removing layers, or parts of layers, mechanically or chemically
- B32B 38/1825: {characterised by the control or constructional features of devices for tensioning, stretching or registration}
- B32B 39/00: Layout of apparatus or plants, e.g. modular laminating systems
- B32B 41/00: Arrangements for controlling or monitoring lamination processes; Safety arrangements
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/06: as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a layer of a particular substance B32B9/045; next to a bituminous or tarry layer B32B11/046; next to a water setting substance layer B32B13/12; next to a metal layer B32B15/08; next to a glass layer B32B17/10; next to a layer formed of natural mineral fibres or particles B32B19/045; next to a wood layer B32B21/08; next to a cellulosic plastic layer B32B23/08; next to a natural or synthetic rubber layer B32B25/08)}
- B32B 2037/268: {Release layers}
- B32B 2250/03: 3 layers
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2307/554: Wear resistance
- B32B 2309/16: Tension
- B32B 2309/72: For measuring or regulating, e.g. systems with feedback loops
- B32B 2419/00: Buildings or parts thereof
- B32B 2471/00: Floor coverings (B32B2419/04 takes precedence)
- B32B 2479/00: Furniture
- B32B 2607/00: Walls, panels
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

A method and system for laminating a building board core with a use or wear layer, and a resultant board, in which the board core is provided with a lamination material on its top side and/or bottom side. A cover sheet that is provided as the lamination material has a wear layer provided with an adhesive layer and a peel-off film on the adhesive layer. To automate the manufacturing process and comply with predefined working conditions, the peel-off film is pulled off the adhesive layer with a predefined peel-off force and the wear layer is fixed to the top side or the bottom side of the board core by a pressure roller. Faults can occur if changing boundary conditions cause a change in the pull-off force, in which case a deviation between the relevant actual value and the predefined target value can lead to a fault in the process.

## Claims

### Claim 1

A method for laminating a building board core (10) with at least one wear layer (15), comprising the steps of:
cutting to size and providing at least the building board core (10), which has a top side (11) and a bottom side (12),
providing a lamination material (200) for forming the wear layer (15), whereby
a top layer web (13) is provided as the lamination material (200), the top layer web (13) comprising a wear layer (15) provided with an adhesive layer (14) and a peel-off film (16) arranged on the adhesive layer (14),
the top layer web (13) is provided on an unwinding roller (17) for laminating the top side (11) or the bottom side (12) of the building board core (10) on a lamination system (300),
the building board core (10) is fed to the lamination system (300),
the wear layer (15) and the peel-off film (16) are separated from one another by coupling a free end of the peel-off film (16) to a peel-off film roll-up roller (19) and bringing the wear layer (15) into contact with its adhesive layer (14) on the top side (11) or on the bottom side (12) of the supplied building board core (10),
the peel-off film (16) is peeled off the adhesive layer (14) with a predefined peel-off force (F1SOLL), and
the wear layer (15) is fixed to the top side (11) or the bottom side (12) of the building board core (10) by means of a pressure roller (20),
wherein
a sensor measures an actual value (F1IST) of the peel-off force acting on the adhesive bond between the wear layer (15) and the peel-off film (16),
a controller (25) compares the actual value (F1IST) of the pull-off force with the predefined setpoint value (F1SOLL), and
when a control deviation is detected, a controlled variable, preferably a torque (M) or a distance between the pressure roller (20) and the wear layer (15) is changed so that the actual value (F1IST) is adjusted to the setpoint value (F1SOLL).

### Claim 2 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein the wear layer (15) is applied on the top side (11) and on the bottom side (12) of the building board core (10), and the steps are preferably being carried out synchronously with one another.

### Claim 3 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein for adapting the actual value (F1IST) to the desired value of the predefined peel-off force (F1SOLL)
the drive torque (M1) of the unwinding roller (17), and/or
the drive torque (M2) of the peel-off film roll-up roller (19), and/or
the drive torque (M3) of the pressure roller (20) is adjusted.

### Claim 4 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein the predefined peel-off force (F1SOLL) is set on the basis of preset values stored in a data memory (23) of the lamination system (300), the setting preferably being carried out automatically by means of a system control (22).

### Claim 5 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein the peel-off force (F1SOLL) is kept constant by means of a control circuit.

### Claim 6 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein the top side (11) and/or bottom side (12) of the building board core (10) to be laminated is cleaned by means of a cleaning system (47) before gluing.

### Claim 7 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein at least two building board cores (10) are laminated directly one after the other on their top side (11) and/or on their bottom side (12) with the wear layer (15) and a gap sensor is used to check whether the at least two building board cores (10) are in contact with one another, wherein the wear layer (15) is a self-adhesive wear layer.

### Claim 8 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein the wear layer (15) is a self-adhesive wear layer that is pressed onto the top side (11) and/or the bottom side (12) of the building board core (10) by means of a pressure roller (20) which is flexible.

### Claim 9 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein:
the wear layer (15) is a self-adhesive wear layer that is provided with a width (B1) which does not exceed a width (B2) of the building board core (10) to be laminated, and
before gluing, the alignment of the self-adhesive wear layer with respect to the building board core (10) is controlled by means of a control circuit in such a way that the wear layer (15) does not protrude beyond the building board core (10) in the glued state.

### Claim 10 (depends on 1)

The method for laminating a building board core (10) according to claim 1, wherein a control loop is provided, by means of which the pressure force exerted by the pressure roller (20) on the wear layer (15) is kept constant at a predefined pressure value or a predefined pressure value range.

### Claim 11

A lamination system (300) for adhering a self-adhesive wear layer (15) to a building board core (10), the system comprising:
a conveyor system (27) for transporting the building board cores (10),
at least one unwinding roller (17) for receiving a top layer web (13), the top layer web (13) comprising a wear layer (15) provided with an adhesive layer (14) and a peel-off film (16) arranged on the adhesive layer (15),
at least one roll-up roller (19) for receiving the peel-off film (16) separated from the adhesive layer (14), and
at least one pressure roller (20) for pressing the wear layer (15) onto the building board core (10),
wherein the unwinding roller (17) and/or the roll-up roller (19) and/or the pressure roller (20) and/or the conveyor system (27) has an adjustable drive by means of which a peel-off force (F1IST) acting on the peel-off film (16) can be varied.

### Claim 12 (depends on 11)

The lamination system (300) according to claim 11, wherein the pressure roller (20) comprises a flexible pressure means which adapts to a building board core (10) with an uneven surface contour during the lamination of this surface contour.

### Claim 13 (depends on 11)

The lamination system (300) according to claim 11, wherein at least two pressure rollers (20) are provided, the pressure rollers preferably having flexible pressure means and pressing the wear layer (15) against the building board core (10) in different areas (B1, B2, B3).

### Claim 14 (depends on 11)

The lamination system (300) according to claim 11, wherein the pressure roller (20) comprises a support shaft (29) and at least two individual segments (30) which can be variably mounted on the support shaft (29) in the axial direction of the support shaft (29).

### Claim 15 (depends on 14)

The lamination system (300) according to claim 14, wherein one or more lamellar wheels (48) are provided as individual segments (30), which have a radius (R1) in the unloaded state and a reduced radius (R2) at the load point when the wear layer (15) is pressed against the building board core (10).

### Claim 16

A laminated building board (100) comprising a building board core (10), an adhesive layer (14) and a wear layer (15), wherein the laminated building board (100) is produced by a method for laminating a building board core (10) with at least one wear layer (15), comprising the steps of:
cutting to size and providing at least the building board core (10), which has a top side (11) and a bottom side (12),
providing a lamination material (200) for forming the wear layer (15),
whereby
a top layer web (13) is provided as the lamination material (200), the top layer web (13) comprising a wear layer (15) provided with an adhesive layer (14) and a peel-off film (16) arranged on the adhesive layer (14),
the top layer web (13) is provided on an unwinding roller (17) for laminating the top side (11) or the bottom side (12) of the building board core (10) on a lamination system (300),
the building board core (10) is fed to the lamination system (300),
the wear layer (15) and the peel-off film (16) are separated from one another by coupling a free end of the peel-off film (16) to a peel-off film roll-up roller (19) and bringing the wear layer (15) into contact with its adhesive layer (14) on the top side (11) or on the bottom side (12) of the supplied building board core (10),
the peel-off film (16) is peeled off the adhesive layer (14) with a predefined peel-off force (F1SOLL), and
the wear layer (15) is fixed to the top side (11) or the bottom side (12) of the building board core (10) by means of a pressure roller (20),
wherein
a sensor measures an actual value (F1IST) of the peel-off force acting on the adhesive bond between the wear layer (15) and the peel-off film (16),
a controller (25) compares the actual value (F1IST) of the pull-off force with the predefined setpoint value (F1SOLL), and
when a control deviation is detected, a controlled variable, preferably a torque (M) or a distance between the pressure roller (20) and the wear layer (15) is changed so that the actual value (F1IST) is adjusted to the setpoint value (F1SOLL).