# US 2024/0375173 A1 · Process For In-Line Mechanically Scribing Of Amorphous Foil For Magnetic Domain Alignment And Core Loss Reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0375173 A1
- Document ID: US20240375173A1
- Status: Published application
- Kind: A1
- Application number: 18/668,352
- Filed: 2024-05-20
- Published: 2024-11-14
- Earliest claimed: 2020-09-25
- Assignees: Metglas, Inc.
- Applicants: Metglas, Inc.
- Inventors: Eric Alan THEISEN; Donald E. Granger, JR.; Thomas Joseph Hastie; Donald Robert Reed, JR.
- Web page: https://patentgrep.com/patent/US20240375173A1

## CPC

- B22D 11/114: by using agitating or vibrating means (B22D11/117 takes precedence)
- B22D 11/001: {of specific alloys}
- B22D 11/0611: {formed by a single casting wheel, e.g. for casting amorphous metal strips or wires}
- B22D 11/0642: {Nozzles (nozzles used in open-ended moulds B22D41/50)}
- B22D 11/0651: {Casting wheels (B22D11/0682 takes precedence)}
- H01F 1/14775: {in the form of sheets}
- H01F 1/15308: {based on Fe/Ni (H01F1/15325 takes precedence)}
- H01F 1/15341: {Preparation processes therefor}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The invention relates to the reduction of core losses in soft magnetic applications utilizing amorphous foil as the core material. Amorphous foil is known to have lower losses when compared to crystalline silicon steel laminations. It is found that a reduction of 10-40% of losses can be achieved over the current state of the art amorphous material by mechanical scribing of the surface of the soft magnetic laminations comprising the wound core in power conditioning devices such as a transformer. The scribing process introduces control of the magnetic domains causing ease of magnetic flux reversal.

## Claims

### Claim at position 1

-9. (canceled)

### Claim 10

An amorphous foil having a width of 75 to 260 mm and a scribed pattern with a wavelength of 0.5 to 10 mm.

### Claim 11 (depends on 10)

The amorphous foil of claim 10, wherein the scribed pattern covers more than 50% of a surface of the amorphous foil.

### Claim 12 (depends on 10)

The amorphous foil of claim 10, wherein the scribed pattern covers more than 75% of a surface of the amorphous foil.

### Claim 13 (depends on 10)

The amorphous foil of claim 10, wherein the scribed pattern covers more than 90% of a surface of the amorphous foil.

### Claim 14 (depends on 10)

The amorphous foil of claim 10, wherein the composition of the foil comprises of Fe100-v-w-x-y-zSivBwPxCyMz in atomic percentages and unavoidable impurities, wherein Si, B, P and C are nonmetals added to help forming the an amorphous structure and M is selected from the group consisting of metals from Groups IV to XI, and combinations thereof, wherein v=0-15.2, w=0-20.3, x=0-15.9, y=0-2, z=0-66.8 and 15<v+w+x+y<30.

### Claim 15 (depends on 14)

The amorphous foil of claim 14, wherein M is selected from the group consisting of Co, Nb, Cu, Mo, Cr, Ni and combinations thereof.

### Claim 16 (depends on 14)

The amorphous foil of claim 14, wherein the composition of the foil consists essentially of Fe100-v-w-x-y-zSivBwPxCyMz in atomic percentages, wherein Fe is from 78-84, Si is from 0-10, B is from 11-18, and C is from 0-0.5.

### Claim 17 (depends on 14)

The amorphous foil of claim 14, wherein the scribed foil has a saturation induction of 1.6 to 1.66 T.

### Claim 18 (depends on 14)

The amorphous foil of claim 14, wherein the scribed foil has a saturation induction of 1.4 to 1.6 T.

### Claim 19 (depends on 10)

The amorphous foil of claim 10, wherein the foil is 13 to 75 microns thick.

### Claim 20

An amorphous core comprising an amorphous foil having a width of 75 to 260 mm and a scribed pattern with a wavelength of 1 to 5 mm, wherein the amorphous foil is wound into a toroidal core or into a laced distribution transformer core, and wherein the amorphous core has reduced losses of core losses less than 0.2 W/kg when tested at 1.4 T, 60 Hz and less than 0.17 W/kg when tested at 1.3 T, 60 Hz.

### Claim 21

An amorphous foil having a width of 75 to 260 mm and a scribed pattern with a wavelength of 1 to 5 mm, wherein the amorphous foil is tested in the single sheet configuration, and wherein the amorphous foil has reduced losses of core losses less than 0.08 W/kg when tested at 1.4 T, 60 Hz and less than 0.06 W/kg when tested at 1.3 T, 60 Hz.

### Claim 22 (depends on 10)

The amorphous foil of claim 10, wherein the foil has a saturation induction of 1.63 T, and wherein the composition consists essentially of Fe81B14.7Si4C0.3.

### Claim 23 (depends on 10)

The amorphous foil of claim 10, wherein the foil has a saturation induction of 1.56 T, and wherein the composition consists essentially of Fe79B11.6Si9.3C0.1.

### Claim 24 (depends on 10)

The amorphous foil of claim 10, wherein the foil has a lamination factor between 0.87 and 0.92.