Zeolite and interferon coated disposable particulate respirator and air filtration media
OwnerWilliam L. Robinson, JR.inventor
Life of this patent
Estimating the term…
Abstract
A method and use of Zeolite, Polyethylenimine (PEI) and Benzalkonium Chloride Polymer coated air filtration media designed to absorb CH4 and CO2 and airborne bacterial and viral biological agents and a method and use of Polyacrylonitrile (PAN), Interferon, Vinegar and Zeolite coated disposable respirator media to absorb airborne deleterious pollutants such as PM2.5 and biological agents such as Influenza, SARS and COVID-19 viruses and respiratory bacteria and protect the wearer from inhalation of said pollutant and deleterious agents.
Claims3
A Method of producing mechanical air filtration media containing absorbent materials such as Clinoptilolite or Chabazite (Zeolite), Polyethyleneimine (PEI) and Benzalkonium Chloride (BAC) as CO2 air pollution absorbing/trapping agents dissolved in de-ionized water coated onto woven or nonwoven (polypropylene) fabric comprising:
- a) combining layers of Zeolites, Polyethyleneimine (PEI) and Benzalkonium Chloride polymer coated spunbond/meltblown polypropylene fabric for CO2 collection from an air stream.
- b) then adding a layer of the step of mixing radiation and air pollution absorbing materials ˜60-80% zeolite and correspondingly 40-20% boehmite (retention aid) binder in de-ionized water (5:1 ratio) at pH 8-9, specifically 8.5-8.9 at 28-30° C., specifically 28.8° C., and an organic polymer containing Hydroxypropylcellulose (HPC)+Ethoxylated Methyl Glucoside (EMG) ˜60%:40% (ratio) (Curie Formula sealant) (to minimize particle separation from the substrate creating dust), for two (2) 16 minutes,
- c) This Hazardous Emission Particulate Analysis (HEPA) tested (0.1-0.3 microns) air filtration media maybe coated with a Mayer rod. The bottom (first three layers) dry aim thicknesses are 1.8 mil and the top (or sealant) layer is 1.4 mil, air penetration is 0.001-0.003.
- then,
- d) the step of applying (spraying or dipping) or coating the absorbing material onto a woven or nonwoven (spunbond/meltblown polypropylene) fabric,
A method of producing disposable face masks and particulate respirator filtration media comprising the steps of:
- a) combining one (1) layer of Polyacrylonitrile (PAN) and one layer of acetic (Vinegar) or citric acid and Curie Formula coated spunbond polypropylene to form the top two (2) layers 1.4 mil thickness (each) with a third layer of spunbond coated with alpha interferon or iodine pH 6.0-6.5 and a fourth layer comprised of zeolite and Curie Formula coated absorbing materials ˜60-80% zeolite and correspondingly 40-20% boehmite (retention aid) binder in de-ionized water (5:1 ratio) at pH 8-9, specifically 8.5-8.9 at 28-30° C., specifically 28.8° C., spunbond material which acts to permanently seal the fabric,
- and
Alpha, Beta and Gamma Interferon and Zeolite adsorbent materials include but are not limited to zeolite type 13X, zeolite type Y, zeolite type 4A, 5A, ZSM-3, chabazite, clinoptilolite, naptolite, mordenite, Heu, brewsterite, SBN and ZON, mixtures of these can also be used.