# US 2024/0361260 A1 · Method of analyzing crystal structure, crystal morphology, or crystal distribution of rubber material in stretching

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0361260 A1
- Document ID: US20240361260A1
- Status: Published application
- Kind: A1
- Application number: 18/619,796
- Filed: 2024-03-28
- Published: 2024-10-31
- Earliest claimed: 2023-04-25
- Assignees: Tohoku University; Sumitomo Rubber Industries, Ltd.
- Applicants: Tohoku University; Sumitomo Rubber Industries, Ltd.
- Inventors: Hiroshi JINNAI; Tomohiro MIYATA; Daisuke WATANABE; Wakana ITO; Takehiro KITAURA
- Web page: https://patentgrep.com/patent/US20240361260A1

## CPC

- G01N 23/20058: Measuring diffraction of electrons, e.g. low energy electron diffraction [LEED] method or reflection high energy electron diffraction [RHEED] method
- G01N 23/2055: Analysing diffraction patterns
- G01N 2223/0566: analysing diffraction pattern
- G01N 2223/418: electron microscope
- G01N 2223/602: crystal growth
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

To provide an analysis method that can analyze a crystal structure, a crystal morphology, a crystal distribution of a rubber material in stretching even in a local portion of the rubber material. The present disclosure relates to a method of analyzing a crystal structure, a crystal morphology, or a crystal distribution of a rubber material in stretching using a nanodiffraction imaging technique that analyzes an electron diffraction pattern acquired by scanning electron beams converged to a diameter of 100 nm or less on a surface of the rubber material while a behavior of stretching deformation of the rubber material and/or a state of the rubber material in stretching are observed using a transmission electron microscope.

## Claims

### Claim 1

A method of analyzing a crystal structure, a crystal morphology, or a crystal distribution of a rubber material in stretching using a nanodiffraction imaging technique that analyzes an electron diffraction pattern acquired by scanning electron beams converged to a diameter of 100 nm or less on a surface of the rubber material while a behavior of stretching deformation of the rubber material and/or a state of the rubber material in stretching are observed using a transmission electron microscope.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the nanodiffraction imaging technique is performed under measurement conditions described below:
(measurement conditions)
probe size: ϕ1 to ϕ150 nm
total dose: 1.0×10−6 to 1.0×103 e−/Å2.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein when a diffraction pattern obtained by performing a further electron diffraction is analyzed, an integrated region of the diffraction pattern is a region of 1×1 to 1000×1000 nm2.

### Claim 4 (depends on 1)

The method according to claim 1,
wherein a local strain in an observation visual field of a transmission electron microscopic image is 1 to 40.