# US 2024/0360024 A1 · Cleaning step to remove metals or metal oxides from porous glass body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0360024 A1
- Document ID: US20240360024A1
- Status: Published application
- Kind: A1
- Application number: 18/637,553
- Filed: 2024-04-17
- Published: 2024-10-31
- Earliest claimed: 2023-04-28
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Steven Treavis Arndt; Raymond David Groh; Ashley Anne Holman; Spencer Thomas Kingsbury
- Web page: https://patentgrep.com/patent/US20240360024A1

## CPC

- C03B 37/01446: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering (C03B37/01853 takes precedence)}
- C03B 37/01846: {Means for after-treatment or catching of worked reactant gases}
- C03B 37/01853: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering}
- C03B 37/032: {for glass optical fibres}
- C03B 2201/07: Impurity concentration specified
- C03B 2201/10: doped with boron (C03B2201/14 takes precedence)
- C03B 2201/28: doped with phosphorus
- C03B 2201/31: doped with germanium
- C03B 2201/32: doped with aluminium (C03B2201/36 takes precedence)
- C03B 2201/34: doped with rare earth metals, i.e. with Sc, Y or lanthanides, e.g. for laser-amplifiers
- C03B 2201/42: doped with titanium
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of manufacturing including: (a) a first vapor deposition step comprising vapor depositing a first porous glass body of a glass former and a doping constituent onto a substrate; (b) a cleaning step after the first vapor deposition step, the cleaning step comprising exposing the first porous glass body to a cleaning gas at a cleaning temperature for a cleaning period of time, the cleaning gas (i) removing a metal or metal oxide from the first porous glass body, (ii) changing an oxidation state of a metal or metal oxide within the first porous glass body, or (iii) a combination of (i) and (ii); and (c) a second vapor deposition step after the cleaning step, the second vapor deposition step comprising vapor depositing a second porous glass body of the glass former onto the first porous glass body resulting in a porous preform for an optical fiber.

## Claims

### Claim 1

A method of manufacturing comprising:
a first vapor deposition step comprising vapor depositing a first porous glass body of a glass former and a doping constituent onto a substrate;
a cleaning step after the first vapor deposition step, the cleaning step comprising exposing the first porous glass body to a cleaning gas at a cleaning temperature for a cleaning period of time, the cleaning gas (i) removing a metal or metal oxide from the first porous glass body, (ii) changing an oxidation state of a metal or metal oxide within the first porous glass body, or (iii) a combination of (i) and (ii); and
a second vapor deposition step after the cleaning step, the second vapor deposition step comprising vapor depositing a second porous glass body of the glass former onto the first porous glass body resulting in a porous preform for an optical fiber.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the first vapor deposition step utilizes a burner that causes a first source material for the glass former and a first source material for the doping constituent to react and form layers of the first porous glass body onto the substrate.

### Claim 3 (depends on 2)

The method of claim 2, wherein
the first source material for the glass former comprises SiCl4; and
the first source material for the doping constituent comprises GeCl4.

### Claim 4 (depends on 1)

The method of claim 1, wherein
the first porous glass body that is vapor deposited onto the substrate comprises SiO2 doped with GeO2; and
the second porous glass body that is vapor deposited onto the first porous glass body comprises SiO2.

### Claim 5 (depends on 1)

The method of claim 1 further comprising:
a substrate removal step comprising removing the substrate from the first porous glass body before the cleaning step.

### Claim 6 (depends on 1)

The method of claim 1, wherein
the first porous glass body comprises a greater amount of the metal or metal oxide before the cleaning step than after the cleaning step.

### Claim 7 (depends on 1)

The method of claim 1, wherein
the cleaning gas comprises a halogen gas, a hydrogen halide gas, or carbon monoxide;
the cleaning temperature is greater than or equal to 800° C.; and
the cleaning period of time is greater than or equal to 30 minutes.

### Claim 8 (depends on 7)

The method of claim 7, wherein
the cleaning gas comprises the halogen gas or the hydrogen halide gas;
the hydrogen gas or hydrogen halide gas of the cleaning gas comprises a partial pressure that is greater than or equal to 7 torr;
the cleaning temperature is within a range of from 1000° C. to 1200° C.; and
the cleaning period of time is within a range of from 1.0 hour to 8.0 hours.

### Claim 9 (depends on 8)

The method of claim 8, wherein
the cleaning gas comprises Cl2.

### Claim 10 (depends on 7)

The method of claim 7, wherein
the cleaning gas comprises carbon monoxide;
the carbon monoxide of the cleaning gas comprises a partial pressure that is within a range of from 1 torr to 10 torr;
the cleaning temperature is within a range of from 1000° C. to 1200° C.; and
the cleaning period of time is within a range of from 1.0 hour to 8.0 hours.

### Claim 11 (depends on 7)

The method of claim 7, wherein
the cleaning gas further comprises O2 for at least a portion of the cleaning period of time.

### Claim 12 (depends on 7)

The method of claim 7, wherein
the cleaning period of time is within a range of from about 2 hours to about 4 hours.

### Claim 13 (depends on 1)

The method of claim 1, wherein
the second vapor deposition step utilizes a burner that causes a second source material for the glass former to react and forms layers of the second porous glass body on the first porous glass body.

### Claim 14 (depends on 13)

The method of claim 13, wherein
the second source material for the glass former comprises one or more of SiCl4 and octamethylcyclotetrasiloxane.

### Claim 15 (depends on 1)

The method of claim 1, wherein
the first vapor deposition step, the cleaning step, and the second vapor deposition step each occur in a different furnace.

### Claim 16 (depends on 1)

The method of claim 1 further comprising:
after the second vapor deposition step, a second cleaning step comprising exposing the porous preform to a cleaning gas at a cleaning temperature for a cleaning period of time, the cleaning gas (i) removing a metal or metal oxide from the porous preform, (ii) changing an oxidation state of a metal or metal oxide within the porous preform, or (iii) a combination of (i) and (ii).

### Claim 17 (depends on 1)

The method of claim 1, wherein
the first porous glass body comprises a greater weight percentage of the doping constituent than the second porous glass body.

### Claim 18 (depends on 1)

The method of claim 1 further comprising:
a core sintering step comprising sintering the porous preform to form a sintered preform;
a redraw step comprising redrawing the sintered preform into a core cane;
an outer cladding step comprising forming a porous outer cladding layer over the core cane; and
a sintering step comprising sintering the porous outer cladding layer, resulting in an optical fiber preform.

### Claim 19 (depends on 1)

The method of claim 1 further comprising:
an optical fiber draw step comprising drawing an optical fiber from an optical fiber preform made from the porous preform.

### Claim 20 (depends on 1)

The method of claim 1, wherein
the optical fiber exhibits an attenuation of electromagnetic radiation having a wavelength of 1310 nm of less than or equal to 0.324 dB/km as measured with an optical time-domain reflectometer; and
the optical fiber exhibits an attenuation of electromagnetic radiation having a wavelength of 1550 nm of less than or equal 0.185 dB/km as measured with an optical time-domain reflectometer.