# US 2024/0352555 A1 · Method for melting a charge of aluminium using an induction furnace

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0352555 A1
- Document ID: US20240352555A1
- Status: Published application
- Kind: A1
- Application number: 18/683,614
- Filed: 2022-08-29
- Published: 2024-10-24
- Earliest claimed: 2021-08-31
- Assignees: Constellium Issoire; Constellium Neuf-Brisach; Constellium Muscle Shoals LLC
- Applicants: Constellium Issoire; Constellium Neuf-Brisach; Constellium Muscle Shoals LLC
- Inventors: Marc BERTHERAT; Anne PICHAT; Emmanuel WAZ; Alain VASSEL
- Web page: https://patentgrep.com/patent/US20240352555A1

## CPC

- C22B 21/0092: {Remelting scrap, skimmings or any secondary source aluminium}
- C22B 7/003: {only remelting, e.g. of chips, borings, turnings; apparatus used therefor}
- C22B 9/003: {by induction}
- F27B 14/061: {Induction furnaces}
- F27B 14/0806: {Charging or discharging devices}
- F27D 3/0024: {of metallic workpieces}
- F27D 3/0025: {Charging or loading melting furnaces with material in the solid state}
- F27D 11/06: Induction heating, i.e. in which the material being heated, or its container or elements embodied therein, form the secondary of a transformer
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

The invention relates to a method for melting an aluminum load, comprising: supplying an aluminum load (11, 12, 13) of which at least 15% by weight is in the form of a sow of essentially cylindrical shape (11) of height h and maximum diameter d; loading said load into a cylindrical induction furnace (10) of height H and maximum internal diameter D in which the height direction of said sow is substantially parallel to the height direction of the furnace; melting said load by induction to obtain a liquid metal bath (2); optionally adjusting content of said liquid metal in which d is in the range from 0.7 D to 0.97 D and preferably in the range from 0.84 D to 0.92 D.

## Claims

### Claim 1

A method for melting an aluminum load, characterized in that it comprises:
supplying an aluminum load (11, 12, 13) of which at least 15% by weight is in the form of a sow of essentially cylindrical shape (11) with a height h and maximum diameter d;
loading said load into a cylindrical induction furnace (10) with a height H and maximum internal diameter D in which the height direction of said sow is substantially parallel to the height direction of the furnace;
melting said load by induction to obtain a liquid metal bath (2);
optionally adjusting the content of said liquid metal, wherein d is in the range from 0.7 D to 0.97 D and preferably in the range from 0.84 D to 0.92 D.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the diameter positioned at mid-height h/2 of the sow of essentially cylindrical shape is located at a distance from the bottom of the furnace between H/2−H/4 and H/2+H/4.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the sow of essentially cylindrical shape has an opening in its center (111).

### Claim 4 (depends on 3)

The method according to claim 3, wherein the sow of essentially cylindrical shape is handled during the loading step by a handling tool (3) inserted through said opening (111).

### Claim 5 (depends on 1)

A method for manufacturing an intermediate product (100, 101), such as a rolling plate, extrusion billet, forging block or ingot or sow, characterized in that it comprises:
obtaining a liquid metal bath optionally content adjusted by the melting method according to claim 1;
optionally filtering and/or treating said liquid metal (2);
forming said intermediate product (100, 101) by casting said liquid metal.

### Claim 6 (depends on 5)

The method for manufacturing an intermediate product according to claim 5, wherein at least 60% of the load is derived from remelt metal.

### Claim 7

An essentially cylindrical aluminum sow with a height h and a maximum diameter d suitable for melting.

### Claim 8 (depends on 7)

The sow according to claim 7, provided with at least two legs (113).

### Claim 9 (depends on 7)

The sow according to claim 7, wherein the sow of essentially cylindrical shape is truncated at the ends by at least one diameter (114).

### Claim 10

A mold (4) for casting an aluminum sow of essentially cylindrical shape with a height h and a maximum diameter d.

### Claim 11 (depends on 10)

The mold according to claim 10, comprising a recessed central tip (411) for making the opening (111).

### Claim 12 (depends on 11)

The mold according to claim 11, wherein the central tip (411) for making the opening (111) is removable.