A binder component for a feedstock compound for use in a shaping and sintering process, comprising, based on the total volume of the binder component,
- b-i) 3 to 70% by volume of at least one first thermoplastic and/or wax-type material,
- b-ii) 30 to 97% by volume of at least one second thermoplastic and/or wax-type material or a plasticized thermoplastic and/or wax-type material,
- wherein the first thermoplastic and/or wax-type material and the second thermoplastic and/or wax-type material differ in at least one property which property is selected from
- (1) solubility in a solvent,
- (2) degradability induced by heat and/or a reactant, and
- (3) volatility,
- wherein the first thermoplastic and/or wax-type material is less soluble, less degradable or less volatile than the second thermoplastic and/or wax-type material,
- wherein Tcross is below 120° C. wherein Tcross is the temperature at the intersection between the storage modulus G′ curve and the loss modulus G″ curve in a dynamic viscoelasticity measurement of the binder component.