# US 2024/0343913 A1 · Method for preparation of self-adhesive super-hydrophobic coatings from plastic waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0343913 A1
- Document ID: US20240343913A1
- Status: Published application
- Kind: A1
- Application number: 18/584,988
- Filed: 2024-02-22
- Published: 2024-10-17
- Earliest claimed: 2023-04-11
- Assignees: King Faisal University
- Applicants: King Faisal University
- Inventors: Junaid SALEEM; SAFDAR HOSSAIN SK; ZUBAIR KHALID BAIG MOGHAL; GORDAN MCKAY
- Web page: https://patentgrep.com/patent/US20240343913A1

## CPC

- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- B29B 17/02: Separating plastics from other materials
- B29C 39/003: {characterised by the choice of material}
- B29C 39/025: {for making multilayered articles}
- B29C 39/04: using movable moulds (B29C41/02 takes precedence){not applied}
- B29C 39/38: Heating or cooling
- C09D 123/04: Homopolymers or copolymers of ethene
- C09D 123/06: Polyethylene
- C09D 123/10: Homopolymers or copolymers of propene
- C09D 123/12: Polypropene
- B29B 2017/0203: {Separating plastics from plastics}
- B29B 2017/0293: {Dissolving the materials in gases or liquids}
- B29K 2223/0625: {LLDPE, i.e. linear low density polyethylene}
- B29K 2223/0633: {LDPE, i.e. low density polyethylene}
- B29K 2223/065: {HDPE, i.e. high density polyethylene}
- B29K 2223/12: {PP, i.e. polypropylene}
- B29K 2909/08: Glass
- B29K 2995/0093: hydrophobic
- C08L 2205/035: containing four or more polymers in a blend
- Y02P 20/582: Recycling of unreacted starting or intermediate materials
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Superhydrophobic films can be prepared from a stream of plastic waste (i.e., derived from post-consumer and/or industrial waste) by a method comprising: dissolving first semi-crystalline polymers in a solvent to form solution1; pre-heating a solid substrate to below a boiling point of the solvent; applying solution1 onto the substrate using spin-casting to obtain a porous blended-polymer layer with fragile structure; annealing the porous blended-polymer layer to above the melting point of the first semi-crystalline polymers to strengthen the porous blended-polymer layer's internal structure by closing pores and decreasing surface roughness, thereby obtaining a strong non-porous base support layer; and dissolving second semi-crystalline polymer in a solvent to form solution2; pre-heating the non-porous base layer to a temperature below a boiling point of the solvent; applying solution2 onto the non-porous base layer to obtain a top porous layer crosslinked with the non-porous base layer; and peeling off the freestanding superhydrophobic film.

## Claims

### Claim 1

A method of making a freestanding superhydrophobic film, the method comprising:
Step 1:
providing a first group of plastics consisting of semi-crystalline polymers comprising polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), or a combination thereof, and a second group of plastics comprising at least one semi-crystalline polymer(s) in common with the semi-crystalline polymers of the first group of plastics, or a combination thereof, in virgin, waste, or recycled form;
dissolving the first group of plastics in a solvent to form a solution 1;
pre-heating a solid substrate to a temperature below a boiling point of the solvent;
applying the solution 1 onto the solid substrate using spin casting to obtain a porous blended polymer layer with a fragile structure; and
annealing the porous blended polymer layer with a fragile structure to a temperature of the highest melting point of the first group of plastics to strengthen the porous blended polymer layer's internal structure by closing the porous blended polymer layers pores and decreasing surface roughness, thereby obtaining a strong non-porous base support layer having a thickness of about 10 μm to about 400 μm; and
Step 2:
dissolving the second group of plastics comprising the at least one semi-crystalline polymer(s) in common with the semi-crystalline polymers of the first group of plastics, or a combination thereof, in a solvent to form a solution 2;
pre-heating the strong non-porous base support layer prepared in step 1 to a temperature below a boiling point of the solvent;
applying the solution 2 onto the strong non-porous base support layer to obtain a top porous layer crosslinked with the strong non-porous base support layer; and
peeling off the top porous layer crosslinked with the strong non-porous base support layer to obtain the freestanding superhydrophobic film,
wherein the freestanding superhydrophobic film has a total thickness of about 20 μm to about 1 mm.

### Claim 2 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprises polypropylene (PP), in virgin, waste, or recycled form.

### Claim 3 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprises high-density polyethylene (HDPE), in virgin, waste, or recycled form.

### Claim 4 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprises low-density polyethylene (LDPE), in virgin, waste, or recycled form.

### Claim 5 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprises linear low-density polyethylene (LLDPE), in virgin, waste, or recycled form.

### Claim 6 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprises a combination of polypropylene (PP), high density polyethylene (HDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), in virgin, waste, or recycled form.

### Claim 7 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise high density polyethylene (HDPE), and the second group of plastics in step 2 comprise high density polyethylene (HDPE), in virgin, waste, or recycled form.

### Claim 8 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise low-density polyethylene (LDPE), and the second group of plastics in step 2 comprise low-density polyethylene (LDPE), in virgin, waste, or recycled form.

### Claim 9 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the first group of plastics in step 1 comprise linear low-density polyethylene (LLDPE), and the second group of plastics in step 2 comprise linear low-density polyethylene (LLDPE), in virgin, waste, or recycled form.

### Claim 10 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1 wherein the solvent is selected from the group consisting of p-xylene, m-xylene, o-xylene, an isomeric mixture of xylenes, toluene, decalin, mesitylene, other compatible hydrocarbons, and mixtures thereof.

### Claim 11 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1 wherein the step 1 of dissolving the first group of plastics in a solvent to form a solution 1 and the step 2 of dissolving the second group of plastics in a solvent to form a solution 2 is conducted at a temperature ranging from about 100° C. to about 180° C., but below a boiling point of the solvent.

### Claim 12 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein a ratio of the first group of plastics in step 1 and the second group of plastics in step 2 to the solvent is about 1 mg/ml to about 400 mg/ml.

### Claim 13 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the solid substrate is selected from the group consisting of glass, copper, silica, alumina, and another metal, and is preheated to a temperature of about 0° C. to 190° C., but below the boiling point of the solvent.

### Claim 14

(canceled)

### Claim 15 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the step of applying solutions 1 and 2 in steps 1 and step 2, respectively, is conducted by spin casting at a speed ranging from about 100 to about 6000 rpm for a period of about 1 minute to about 15 minutes, or until the solvent is removed and a film is formed.

### Claim 16 (depends on 15)

The method of making the freestanding superhydrophobic film of claim 15, wherein the step of applying the solution 1 onto the solid substrate is conducted by spin casting and comprises:
a first spin casting step at a first speed for about 20 seconds;
a second spin casting step at a second speed which is higher than the first speed for about 60-120 seconds to ensure complete removal of the solvent.

### Claim 17 (depends on 16)

The method of making the freestanding superhydrophobic film of claim 16, wherein the first speed is about 500 rpm, the second speed is about 2500 rpm, and the annealing is conducted at a temperature above the melting point of the first group of plastics ranging from 105° C. to 180° C.

### Claim 18 (depends on 15)

The method of making the freestanding superhydrophobic film of claim 15, wherein the step of applying the solution 2 onto the strong non-porous base support layer is conducted by spin casting and results in formation of the top porous layer crosslinked with the strong non-porous base support layer having a thickness of about 10 μm to about 400 μm.

### Claim 19 (depends on 18)

The method of making the freestanding superhydrophobic film of claim 18, wherein the step of applying the solution 2 onto the strong non-porous base support layer is conducted by spin casting and comprises:
a first spin casting step at a first speed for about 20 seconds;
a second spin casting step at a second speed which is higher than the first speed for about 60-120 seconds to ensure complete removal of the solvent to achieve a porous superhydrophobic layer having a thickness of about 10 μm to about 400 μm; and
peeling off the bi-layered superhydrophobic film from the substrate.

### Claim 20 (depends on 1)

The method of making the freestanding superhydrophobic film of claim 1, wherein the superhydrophobic film has a thickness of about 20 μm to about 1 mm.