# US 2024/0343870 A1 · Stretched polyester film and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0343870 A1
- Document ID: US20240343870A1
- Status: Published application
- Kind: A1
- Application number: 18/233,566
- Filed: 2023-08-14
- Published: 2024-10-17
- Earliest claimed: 2023-04-12
- Assignees: SK Chemicals Co., Ltd.
- Applicants: SK Chemicals Co., Ltd.
- Inventors: Da-Young HWANG; Sangwoo Kim; Jiyeon Eom; Boo-Youn Lee
- Web page: https://patentgrep.com/patent/US20240343870A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- B29C 48/022: {characterised by the choice of material}
- B29C 48/305: having a wide opening, e.g. for forming sheets
- B29C 55/02: of plates or sheets
- B29C 55/045: {in a direction which is not parallel or transverse to the direction of feed, e.g. oblique}
- C08G 63/183: Terephthalic acids
- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G 63/672: Dicarboxylic acids and dihydroxy compounds
- C08G 63/85: Germanium, tin, lead, arsenic, antimony, bismuth, titanium, zirconium, hafnium, vanadium, niobium, tantalum, or compounds thereof {(C08G63/823 takes precedence)}
- C08G 63/863: {Germanium or compounds thereof}
- C08J 3/12: Powdering or granulating
- B29C 55/12: biaxial
- B29C 2948/92704: Temperature
- B29K 2067/003: {PET, i.e. poylethylene terephthalate}
- B29K 2995/0051: mono-axially
- B29K 2995/0097: Thickness
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A stretched polyester film and a method for preparing the stretched polyester film are disclosed. The stretched polyester film contains a polyester resin in which a diol component and a dicarboxylic acid component are polymerized, wherein the heat shrinkage rate of the film at 80° C. in the main shrinkage direction is 40% or more, and, upon a first thermal treatment and a second thermal treatment, a first melting temperature (Tm1) and a second melting temperature (Tm2) appear when the film is analyzed by differential scanning calorimetry (DSC). The stretched polyester film has excellent heat shrinkability, along with an increased efficiency of a recycling process of waste plastic containers.

## Claims

### Claim 1

A stretched polyester film, which comprises a single crystalline polyester resin in which a diol component and a dicarboxylic acid component are polymerized,
wherein the single crystalline polyester resin consists of a single polyester material,
wherein a heat shrinkage rate of the stretched polyester film at 80° C. in main shrinkage direction is 40% or more, and, upon a first thermal treatment and a second thermal treatment, a first melting temperature (Tm1) and a second melting temperature (Tm2) appear when the stretched polyester film is analyzed by differential scanning calorimetry (DSC),
wherein the first melting temperature (Tm1) is 150 to 230° C., the second melting temperature (Tm2) is 150 to 230° C., and the first melting temperature (Tm1) and the second melting temperature (Tm2) are different from each other,
wherein a difference (|Tm1−Tm2|) between the first melting temperature (Tm1) and the second melting temperature (Tm2) is in a range of 10 to 60° C.,
wherein the first thermal treatment temperature is 60 to 105° C.,
wherein the second thermal treatment temperature is 140 to 220° C., and
wherein a ratio (H1/H2) of a first heat of fusion (H1) at the first melting temperature (Tm1) to a second heat of fusion (H2) at the second melting temperature (Tm2) is 0.1 to 10.

### Claim at position 2

2-3. (canceled)

### Claim 4 (depends on 1)

The stretched polyester film of claim 1, wherein a sum (H1+H2) of the first heat of fusion (H1) at the first melting temperature (Tm1) and the second heat of fusion (H2) at the second melting temperature (Tm2) is 3 J/g or more.

### Claim at position 4

5-7. (canceled)

### Claim 8 (depends on 1)

The stretched polyester film of claim 1, wherein the diol component comprises one or more selected from the group consisting of bis(2-hydroxyethyl) terephthalate, isosorbide, neopentyl glycol, ethylene glycol, cyclohexanedimethanol, 1,2-propanediol, 1,3-propanediol, 2-methyl-1,3-propanediol, 2-methylene-1,3-propanediol, 2-ethyl-1,3-propanediol, 2-isopropyl-1,3-propanediol, 2,2-dimethyl-1,3-propanediol, 1,4-butanediol, 2,3-butanediol, 3-methyl-1,5-pentanediol, 3-methyl-2,4-pentanediol, 1,6-hexanediol, 1,2-cyclohexanediol, 1,4-cyclohexanediol, diethylene glycol, 4-(hydroxymethyl)cyclohexylmethyl-4-(hydroxymethyl)cyclohexanecarboxylate, 4-(4-(hydroxymethyl)cyclohexylmethoxymethyl)cyclohexylmethanol, recycled cyclohexanedimethanol, recycled ethylene glycol, recycled bis(2-hydroxyethyl) terephthalate, and recycled diethylene glycol.

### Claim 9 (depends on 1)

The stretched polyester film of claim 1, wherein the dicarboxylic acid component comprises one or more selected from the group consisting of isophthalic acid, terephthalic acid, dimethyl isophthalate, phthalic acid, dimethyl phthalate, phthalic anhydride, 2,6-naphthalenedicarboxylic acid, dimethyl 2,6-naphthalenedicarboxylate, diphenyl dicarboxylic acid, 1,4-cyclohexanedicarboxylic acid, 1,3-cyclohexanedicarboxylic acid, dimethyl 1,4-cyclohexanedicarboxylate, dimethyl 1,3-cyclohexanedicarboxylate, sebacic acid, succinic acid, isodecylsuccinic acid, maleic acid, maleic anhydride, fumaric acid, adipic acid, glutaric acid, azelaic acid, recycled isophthalic acid, recycled terephthalic acid, recycled dimethyl isophthalate, and recycled dimethyl phthalate.

### Claim 10 (depends on 1)

The stretched polyester film of claim 1, which has a heat shrinkage rate at 90° C. in the main shrinkage direction of 50% or more.

### Claim 11 (depends on 1)

The stretched polyester film of claim 1, wherein the polyester resin has an intrinsic viscosity (IV) of 0.5 dl/g to 1.2 dl/g.

### Claim 12 (depends on 1)

The stretched polyester film of claim 1, wherein, when the stretched polyester film is heated to 195° C. after the first thermal treatment and the second thermal treatment, the stretched polyester film has a deformation rate of 10% or less according to the following Equation 1:
Deformation
⁢
rate
⁢
(
%
)
=
(
F
m
/
F
T
)
×
100
[
Equation
⁢
1
]
in Equation 1, Fm is a total number of stretched polyester film samples that are melted when heated to 195° C., FT is a total number of stretched polyester film samples before being heated to 195° C., and a size of the stretched polyester film samples is 1 cm in width and 1 cm in length.

### Claim 13 (depends on 1)

A method for preparing a stretched polyester film according to claim 1, which comprises:
polymerizing a diol component and a dicarboxylic acid component to prepare a crystalline polyester resin;
preparing a stretched sheet from the polyester resin; and
heat-setting the stretched sheet,
wherein a heat shrinkage rate of the stretched polyester film at 80° C. in main shrinkage direction is 40% or more, and, upon a first thermal treatment and a second thermal treatment, a first melting temperature (Tm1) and a second melting temperature (Tm2) appear when the stretched polyester film is analyzed by differential scanning calorimetry (DSC),
wherein the first melting temperature (Tm1) is 150 to 230° C., the second melting temperature (Tm2) is 150 to 230° C., and the first melting temperature (Tm1) and the second melting temperature (Tm2) are different from each other,
wherein a difference (|Tm1−Tm2|) between the first melting temperature (Tm1) and the second melting temperature (Tm2) is in a range of 10 to 60° C.,
wherein the first thermal treatment temperature is 60 to 105° C.,
wherein the second thermal treatment temperature is 140 to 220° C., and
wherein a ratio (H1/H2) of a first heat of fusion (H1) at the first melting temperature (Tm1) to a second heat of fusion (H2) at the second melting temperature (Tm2) is 0.1 to 10.

### Claim 14 (depends on 13)

The method for preparing a stretched polyester film of claim 13, wherein the first thermal treatment temperature is 60 to 105° C.

### Claim 15 (depends on 13)

The method for preparing a stretched polyester film of claim 13, wherein the second thermal treatment temperature is 140 to 220° C.